| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
|
Gromax PBT 4130-104D 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
|
|||
| Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
|
Gromax PBT 1100-211XG
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
|
Gromax PBT 1200-211L
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Screw Speed | 60 - 100 rpm | 60 - 100 rpm | |
|
Techmer ES Electrafil® PS-31/EC BK Polystyrene, Electrically Conductive Carbon Black |
|||
| Screw Speed | 60 - 100 rpm | 60 - 100 rpm | Extrusion |
|
Stellarchem GP-785A TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Screw Speed | 60 - 100 rpm | 60 - 100 rpm | Extrusion |
|
Stellarchem GP-975B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Screw Speed | 60 - 100 rpm | 60 - 100 rpm | Extrusion |
|
Stellarchem MP-8001 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Screw Speed | 60 - 100 rpm | 60 - 100 rpm | Extrusion |
|
Stellarchem MP-950NC TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Screw Speed | 60 - 80 rpm | 60 - 80 rpm | |
|
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Screw Speed | 60 - 80 rpm | 60 - 80 rpm | |
|
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Screw Speed | 60 - 100 rpm | 60 - 100 rpm | Extrusion |
|
Stellarchem MP-860Q TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Screw Speed | 60 - 120 rpm | 60 - 120 rpm | |
|
Teknor Apex Chemlon® 233 GH Nylon, 6, 30% Short Glass Fiber Reinforced
Features: Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Processing Method: Injection Molding Forms: Pellets Addi..
|
|||
| Screw Speed | 60 - 120 rpm | 60 - 120 rpm | |
|
Wellman Wellamid® GS25-66 22LH-N 25% Glass Sphere Filled Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
|
|||
| Screw Speed | 60 - 120 rpm | 60 - 120 rpm | |
|
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
|
|||
| Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
|
Alliance Polymers Zythane™ 4060D Thermoplastic Polyurethane Elastomer
Zythane™ 4060D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
|
Alliance Polymers Zythane™ 4080A Thermoplastic Polyurethane Elastomer
Zythane™ 4080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
|
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer
Zythane™ 4085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
|
Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer
Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
|
Alliance Polymers Zythane™ 6045D Thermoplastic Polyurethane Elastomer
Zythane™ 6045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
|
Alliance Polymers Zythane™ 6070A Thermoplastic Polyurethane Elastomer
Zythane™ 6070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
|
Alliance Polymers Zythane™ 7055D Thermoplastic Polyurethane Elastomer
Zythane™ 7055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
|
Alliance Polymers Zythane™ 7085AF Thermoplastic Polyurethane Elastomer
Zythane™ 7085AF is a FR polyether-based TPU specifically formulated with non-halogenated flame retardants for extrusion applications with ease of processing. It exhibits excellent abrasion resistan..
|
|||
| Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
|
Alliance Polymers Zythane™ 5085A Thermoplastic Polyurethane Elastomer
Zythane™ 5085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
|
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer
Zythane™ 7085UF is a UV stabilized polyether-based TPU specifically formulated for extrusion applications. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability,..
|
|||
| Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
|
Gromax CCP PBT 1200-211E
Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle..
|
|||
| Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
|
Gromax CCP PBT 3040-201 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
|
|||
| Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
|
Gromax CCP PBT 6730-104F Glass/Mineral Filled
Product Description: PBT glass/mineral reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent w..
|
|||
| Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
|
Gromax PBT 3015-104 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
|
|||
| Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
|
Gromax CCP PBT 5630-200C 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
|
|||
| Screw Speed | 60 - 100 rpm | 60 - 100 rpm | Injection |
|
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol.
|
|||