Polymer Property : Cure Time = 0.00417 hour Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Buna N Rubber, handling time
Permabond 2010 Cyanoacrylate, gap filling
PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Steel, handling time
Permabond 2010 Cyanoacrylate, gap filling
PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Phenolic, handling time
Permabond 2011 Cyanoacrylate, gel
PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Steel, handling time
Permabond 2050 Cyanoacrylate, flexible
PERMABOND® 2050 is a flexible cyanoacrylate adhesive, exhibiting improved peel strengths when compared to other grades. It has excellent impact and vibration resistance, and is suitable for bonding..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Buna N Rubber, handling time
Permabond 735 Cyanoacrylate, toughened
PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Buna Rubber, set time, cured
Permabond 738 Cyanoacrylate, toughened
PERMABOND 738 is a toughened cyanoacrylate with improved impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable over..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Steel, handling time
Permabond 940 Cyanoacrylate, low odor
PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Aluminum, handling time
Permabond 940 Cyanoacrylate, low odor
PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
PVC, handling time
Permabond 940 Cyanoacrylate, low odor
PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
ABS, handling time
Permabond 940 Cyanoacrylate, low odor
PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Steel, handling time
Permabond 102 Cyanoacrylate, General purpose
PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Steel, handling time
Permabond 801 Cyanoacrylate, High Temperature
PERMABOND® 801 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Buna N Rubber, handling time
Permabond 801 Cyanoacrylate, High Temperature
PERMABOND® 801 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Steel, handling time
Permabond 802 Cyanoacrylate, High Temperature
PERMABOND® 802 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Phenolic, handling time
Permabond 802 Cyanoacrylate, High Temperature
PERMABOND® 802 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Steel, handling time
Permabond 820 Cyanoacrylate, High Temperature
PERMABOND® 820 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Phenolic, handling time
Permabond 820 Cyanoacrylate, High Temperature
PERMABOND® 820 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Phenolic, handling time
Permabond 920 Cyanoacrylate, High temperature
PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Buna N Rubber, handling time
Permabond 920 Cyanoacrylate, High temperature
PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Phenolic, set time
Permabond 930 Cyanoacrylate
PERMABOND 930 is a low odor, non­fogging, non­frosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The ..
Cure Time 0.0833 - 0.250 min
0.00139 - 0.00417 hour
10-20 mil thick layers cured with Dymax 5000-EC at 2 inches. Thicker layers may require more cure time.
Dymax 9003v2.0 Hard Clear Microencapsulant
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9003v2.0 Hard Clear MicroencapsulantGlob top for photosensing devices Cure Type: UV/Visible Typical Use: Optical p..
Cure Time 0.0833 - 0.250 min
0.00139 - 0.00417 hour
10-20 mil thick layers cured with Dymax 5000-EC at 2 inches. Thicker layers may require more cure time.
Dymax 9003v3.0 Flexible Clear Microencapsulant
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9003v3.0 Flexible Clear MicroencapsulantGlob top for photosensing devices Cure Type: UV/Visible Typical Use: Optic..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Aluminum, handling time
Permabond 941 Cyanoacrylate, low odor
PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
PVC, handling time
Permabond 941 Cyanoacrylate, low odor
PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Phenolic resin, handling time
Permabond 941 Cyanoacrylate, low odor
PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
ABS, handling time
Permabond 941 Cyanoacrylate, low odor
PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Steel, handling time
Permabond 943 Cyanoacrylate, low odor
PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Aluminum, handling time
Permabond 947 Cyanoacrylate, low odor
PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
PVC, handling time
Permabond 947 Cyanoacrylate, low odor
PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Phenolic resin, handling time
Permabond 947 Cyanoacrylate, low odor
PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Copyright © lookpolymers.com All Rights Reserved