| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 20.0 min | 0.333 hour | On steel (fixture) |
|
ND Industries NutGrade® 121 Removable Threadlocker
A medium strength threadlocker. Seals most types of nuts and bolts allowing disassembly using standard tools.Typical Usesstuds and bolts, threaded pipe fittings, and locking nuts or bolts larger th..
|
|||
| Cure Time | 20.0 min | 0.333 hour | On steel (fixture) |
|
ND Industries StudGrade® 140 Permanent Threadlocker
General DescriptionHigh strength threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical Usesstuds and bolts, and threaded pipe fittings.Meets m..
|
|||
| Cure Time | 20.0 - 25.0 min | 0.333 - 0.417 hour | working strength |
|
Permabond TA4202 Toughened Acrylic Adhesive
PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni..
|
|||
| Cure Time | 20.0 min | 0.333 hour | handling time, .5 mm gap |
|
Permabond TA435 Toughened Acrylic Adhesive & Initiator
PERMABOND TA435 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This adhesive may be used in a variety of structural bonding appli..
|
|||
| Cure Time | 20.0 - 40.0 min | 0.333 - 0.667 hour | working strength |
|
Permabond TA439 Toughened Acrylic Adhesive
Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f..
|
|||
| Cure Time |
20.0
min @Temperature 149 °C |
0.333
hour @Temperature 300 °F |
|
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N550 (FEF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time |
20.0
min @Temperature 149 °C |
0.333
hour @Temperature 300 °F |
|
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N990 (MT) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time |
20.0
min @Temperature 149 °C |
0.333
hour @Temperature 300 °F |
|
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N774 (SRF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time |
20.0
min @Temperature 149 °C |
0.333
hour @Temperature 300 °F |
|
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N220 (ISAF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time |
20.0
min @Temperature 149 °C |
0.333
hour @Temperature 300 °F |
|
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N774 (SRF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time |
20.0
-
3600
min @Temperature 50.0 - 204 °C |
0.333
-
60.0
hour @Temperature 122 - 400 °F |
Average value: 198 min Grade Count:40 |
|
Overview of materials for Epoxy, Cast, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr..
|
|||
| Cure Time | 20.0 min | 0.333 hour | Dry Time to Handling; Fed Std 141 4061 |
|
Humiseal 1B31LSE Acrylic Conformal Coating
Humiseal 1B31LSE Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C Approval PendingPasses thermal sho..
|
|||
| Cure Time | 20.0 min | 0.333 hour | Tack-free |
|
Momentive Performance Materials RTV103 One Component Acetoxy Adhesive Sealant, Black
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
|
|||
| Cure Time | 20.0 min | 0.333 hour | Tack Free Time |
|
Shin-Etsu Silicones KE-445 Silicone, RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
|
|||
| Cure Time |
20.0
min @Temperature 149 °C |
0.333
hour @Temperature 300 °F |
|
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N774 (SRF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time |
20.0
min @Temperature 149 °C |
0.333
hour @Temperature 300 °F |
|
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N990 (MT) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time |
20.0
min @Temperature 149 °C |
0.333
hour @Temperature 300 °F |
|
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR N550 (FEF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time |
20.0
min @Temperature 154 °C |
0.333
hour @Temperature 310 °F |
|
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Control Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time |
20.0
min @Temperature 154 °C |
0.333
hour @Temperature 310 °F |
|
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Sundex 790 Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time |
20.0
min @Temperature 149 °C |
0.333
hour @Temperature 300 °F |
|
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N990 (MT) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time | 20.0 min | 0.333 hour | |
|
Loctite® 222 Threadlocker
ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from..
|
|||
| Cure Time | 20.0 min | 0.333 hour | Tack-free |
|
Loctite® 5910 Form-in-place RTV Silicone Flange Sealant
Silicone GasketingLoctite® Silicone Gasketing materials include unique products with excellent resistance, formulations for high operating temperatures, and UV-curing formulations for cure-in-place..
|
|||
| Cure Time |
20.0
min @Temperature 149 °C |
0.333
hour @Temperature 300 °F |
|
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N220 (ISAF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time | 20.0 min | 0.333 hour | Handling Strength |
|
3M Scotch-Weld™ DP-105 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s..
|
|||
| Cure Time |
20.0
min @Temperature 149 °C |
0.333
hour @Temperature 300 °F |
|
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 70 PHR N330 (HAF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time | <= 20.0 min | <= 0.333 hour | Tack-Free, 50% RH |
|
3M 230 Crystal Clear Sealant
3M™ Crystal Clear Sealant 230 is a one component thermoplastic elastomer which forms permanent elastic bonds when used in surface sealing applications. 3M Crystal Clear Sealant 230 bonds to a wide ..
|
|||
| Cure Time |
20.0
min @Temperature 154 °C |
0.333
hour @Temperature 310 °F |
Press cured |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Laminar Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time |
20.0
min @Temperature 154 °C |
0.333
hour @Temperature 310 °F |
Press cured |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 80 PHR Mistron Vapor Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Cure Time |
20.0
min @Temperature 149 °C |
0.333
hour @Temperature 300 °F |
|
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N330 (HAF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||