| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 0.500 - 1.00 min | 0.00833 - 0.0167 hour | On Steel (Fixture) |
|
ND Industries 388 Toughened Instant Superglue
Black toughened Cyanoacrylate for metal, rubber, and plastic
|
|||
| Cure Time | 0.500 - 1.17 min | 0.00833 - 0.0194 hour | On Steel (Fixture) |
|
ND Industries SuperGlue Ethyl 309
Non-running gel for porous surfaces, general purpose
|
|||
| Cure Time | <= 0.500 min | <= 0.00833 hour | Phenolic, handling time |
|
Permabond 731 Cyanoacrylate, toughened
PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
|
|||
| Cure Time | 0.500 - 0.750 min | 0.00833 - 0.0125 hour | ABS, handling time |
|
Permabond 731 Cyanoacrylate, toughened
PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
|
|||
| Cure Time | 0.500 - 0.833 min | 0.00833 - 0.0139 hour | Steel, handling time |
|
Permabond 735 Cyanoacrylate, toughened
PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
|
|||
| Cure Time | 0.500 - 0.583 min | 0.00833 - 0.00972 hour | Aluminum, set time, cured |
|
Permabond 738 Cyanoacrylate, toughened
PERMABOND 738 is a toughened cyanoacrylate with improved impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable over..
|
|||
| Cure Time | 0.500 - 0.750 min | 0.00833 - 0.0125 hour | handling time with initiator 41 |
|
Permabond TA437 Toughened Acrylic Adhesive
PERMABOND TA437 is a single component structural acrylic adhesive designed primarily for bonding metals, ferrites and ceramics. The typical fixture time of TA437 when used with Initiator 41 is 30 –..
|
|||
| Cure Time | <= 0.500 min | <= 0.00833 hour | Handling time |
|
Permabond TA440 Toughened Acrylic Adhesive
PERMABOND TA440 is a two component structural acrylic adhesive suitable for bonding metals, glass, wood, ferrites, ceramics and some rigid plastics. This adhesive may be used in a variety of structu..
|
|||
| Cure Time | 0.500 - 1.00 min | 0.00833 - 0.0167 hour | Per 1 mm of wall thickness, compression molding |
|
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
(dis
Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l..
|
|||
| Cure Time | 0.500 - 0.667 min | 0.00833 - 0.0111 hour | Metal set time |
|
Lord Adhesives 9900 Normal Setting, High Viscosity, Odorless, Non-Frosting Methyl Cyanoacrylate Adhesive
Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal..
|
|||
| Cure Time | 0.500 min | 0.00833 hour | |
|
Loctite® 493 General Purpose Methyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
|
|||
| Cure Time | 0.500 min | 0.00833 hour | |
|
Loctite® 496 General Purpose Methyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
|
|||
| Cure Time | <= 0.500 min | <= 0.00833 hour | Dry Time |
|
Loctite® 712 Isopropanol Base Surface Primer
Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the ..
|
|||
| Cure Time | <= 0.500 min | <= 0.00833 hour | Dry Time |
|
Loctite® 7453 Acetone (electronic grade) Base Surface Primer
Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the ..
|
|||
| Cure Time | 0.500 - 1.17 min | 0.00833 - 0.0195 hour | Dry Time |
|
Loctite® 7649 Acetone Base Primer N
Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the ..
|
|||
| Cure Time | 0.500 min | 0.00833 hour | Tack-free; 120 mW/cm^2; varies with substrates |
|
Loctite® FASTGASKET® 5950 Flange Sealant
Silicone Gasketing and Gasketing and Wire TackersLoctite® Silicone Gasketing materials include unique products with excellent resistance, formulations for high operating temperatures, and UV-curing..
|
|||
| Cure Time | 0.500 min | 0.00833 hour | at 120 mW/cm^2 |
|
Loctite® FASTGASKET® 5950 Flange Sealant
Silicone Gasketing and Gasketing and Wire TackersLoctite® Silicone Gasketing materials include unique products with excellent resistance, formulations for high operating temperatures, and UV-curing..
|
|||
| Cure Time | 0.500 min | 0.00833 hour | |
|
Loctite® PRISM® 411 Clear Instant Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
|
|||
| Cure Time | 0.500 min | 0.00833 hour | Dry Time |
|
Loctite® Prism® 770 Primer
Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the ..
|
|||
| Cure Time | 0.500 min | 0.00833 hour | |
|
Loctite® Tak Pak® 382 Instant Adhesive
Cyanoacrylate Bonding Adhesives and Gasketing and Wire TackingLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of..
|
|||
| Cure Time | 0.500 min | 0.00833 hour | |
|
Loctite® Tak Pak® 444 Instant Adhesive
Cyanoacrylate Bonding Adhesives and Gasketing and Wire TackersLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of..
|
|||
| Cure Time | 0.500 min | 0.00833 hour | Set Time |
|
3M Scotch-Weld™ EZ250030 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th..
|
|||
| Cure Time | 0.500 - 1.00 min | 0.00833 - 0.0167 hour | |
|
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material
Product Introduction: Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC t..
|
|||
| Cure Time | 0.500 min | 0.00833 hour | Set Time |
|
3M Scotch-Weld™ TE031 Black Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
|
|||
| Cure Time | 0.500 - 1.00 min | 0.00833 - 0.0167 hour | |
|
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material
Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC thermosets are the most ..
|
|||
| Cure Time | 0.500 - 0.667 min | 0.00833 - 0.0111 hour | Zinc, handling time |
|
Permabond 941 Cyanoacrylate, low odor
PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
|
|||
| Cure Time | 0.500 min | 0.00833 hour | Tack-free; 120 mW/cm^2; varies with substrates |
|
Loctite® FASTGASKET® 5960 Flange Sealant
Silicone Gasketing and Gasketing and Wire TackersLoctite® Silicone Gasketing materials include unique products with excellent resistance, formulations for high operating temperatures, and UV-curing..
|
|||
| Cure Time | 0.500 - 1.00 min | 0.00833 - 0.0167 hour | Per 1 mm of wall thickness, compression molding |
|
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U..
|
|||
| Cure Time | 0.500 - 1.17 min | 0.00833 - 0.0195 hour | Dry Time |
|
Loctite® 7471 Acetone/Isopropanol Base Primer T
Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the ..
|
|||