| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time |
10.0
-
30.0
min @Temperature -65.0 - 300 °C |
0.167
-
0.500
hour @Temperature -85.0 - 572 °F |
Handling |
|
Palm Labs Adhesives TURBO SEAL SERIES 55 BROWN FINE THREADS THREAD SEALANT
TURBO SEAL SERIES 55 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures quickly in the absence of air between..
|
|||
| Cure Time |
10.0
min @Temperature 155 °C |
0.167
hour @Temperature 311 °F |
|
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR TCP Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
|
|||
| Cure Time |
10.0
min @Temperature 155 °C |
0.167
hour @Temperature 311 °F |
|
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR TP-95 Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
|
|||
| Cure Time |
10.0
min @Temperature 155 °C |
0.167
hour @Temperature 311 °F |
|
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Aerosil 200
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
|
|||
| Cure Time |
10.0
min @Temperature 160 °C |
0.167
hour @Temperature 320 °F |
|
|
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 95A
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
|
|||
| Cure Time |
10.0
min @Temperature 68.3 °C |
0.167
hour @Temperature 155 °F |
Press cured |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N990 (MT) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
|
|||
| Cure Time | 10.0 - 15 min | 0.167 - 0.25 hour | |
|
Gwent Electronic Materials C2000107P3 Silver Ink
Silver Ink C2000107P3 is designed as a termination for single layer PZT ceramics. After firing the film has good adhesion and solderability.The ink is in a ready to use form at a viscosity suitable..
|
|||
| Cure Time | 10.0 min | 0.167 hour | Tack free |
|
Momentive Performance Materials TSE397 One Component RTV Adhesive Sealant/Coating, Clear/White
TSE392, TSE397 and TSE399 adhesive sealants/coatings are one component RTV’s that cure quickly by reacting with atmospheric moisture forming a soft dielectric silicone rubber. These materials i..
|
|||
| Cure Time | 10.0 - 15 min | 0.167 - 0.25 hour | |
|
Gwent Electronic Materials C2010515D4 Silver Ink
Silver Ink C2010515D4 is designed as an internal electrode ink for LTCC applications. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the mark..
|
|||
| Cure Time | 10.0 - 15 min | 0.167 - 0.25 hour | |
|
Gwent Electronic Materials C2031105D2 Palladium Ink
Palladium Ink C2031105D2 is an ink formulated for screen printing for use on Fuel Cells. It is suitable for application onto Solid Oxide Fuel Cells.The ink has been made at a ready to use viscosity..
|
|||
| Cure Time | 10.0 min | 0.167 hour | |
|
Shin-Etsu Silicones SV-13500U Silicone Rubber
SV13500U is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendaring. Product F..
|
|||
| Cure Time | 10.0 - 15.0 min | 0.167 - 0.250 hour | Tack-free time |
|
Master Bond MasterSil 708FR One Part, Flame Resistant Silicone
Description: MasterSil 708FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V.1 for thicknesses of ..
|
|||
| Cure Time |
10.0
min @Temperature 171 °C |
0.167
hour @Temperature 340 °F |
|
|
Uniseal BETABRACE™ 85002 Epoxy
BETABRACE™ 85002 is a composite used for reinforcing sheet metal. It is composed of a high temperature curing tacky polymer, woven glass fabric, and release paper. BETABRACE™ 85002 provides adhe..
|
|||
| Cure Time |
10.0
min @Temperature 171 °C |
0.167
hour @Temperature 340 °F |
|
|
Uniseal BETABRACE™ 85076 Epoxy
BETABRACE™ 85076 is an expandable composite used for reinforcing sheet metal. It is composed of a high temperature curing tacky polymer, woven glass fabric, and release paper. BETABRACE™ 85076 p..
|
|||
| Cure Time |
10.0
min @Temperature 68.3 °C |
0.167
hour @Temperature 155 °F |
|
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR MBT
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
|
|||
| Cure Time |
10.0
min @Temperature 68.3 °C |
0.167
hour @Temperature 155 °F |
Press cured |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Fumed Silica - Wacker HK N20
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
|
|||
| Cure Time |
10.0
min @Temperature 68.3 °C |
0.167
hour @Temperature 155 °F |
Press cured |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N220 (ISAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
|
|||
| Cure Time |
10.0
min @Temperature 68.3 °C |
0.167
hour @Temperature 155 °F |
Press cured |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Talc-Mistron Vapor
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
|
|||
| Cure Time |
10.0
min @Temperature 68.3 °C |
0.167
hour @Temperature 155 °F |
Press cured |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N550 (FEF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
|
|||
| Cure Time | 10.0 min | 0.167 hour | |
|
Loctite® 243 Oil Resistant/Medium Strength Threadlocker
ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from..
|
|||
| Cure Time | 10.0 - 30.0 min | 0.167 - 0.500 hour | Tack-Free, 50% RH |
|
3M 760 Hybrid Adhesive Sealant
3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp..
|
|||
| Cure Time | 10.0 min | 0.167 hour | Tack free |
|
3M Scotch-Weld™ DP-105 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s..
|
|||
| Cure Time | 10.0 - 20.0 min | 0.167 - 0.333 hour | Time to Handling Strength |
|
3M Scotch-Weld™ DP810 Tan Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
|
|||
| Cure Time |
10.0
min @Temperature 154 °C |
0.167
hour @Temperature 309 °F |
|
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-550 (FEF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
|
|||
| Cure Time |
10.0
min @Temperature 155 °C |
0.167
hour @Temperature 311 °F |
|
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-330 (HAF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
|
|||
| Cure Time | 10.0 min | 0.167 hour | Fixture |
|
Resinlab® RC8003 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
|
|||
| Cure Time | 10.0 min | 0.167 hour | Fixture |
|
Resinlab® RC8035 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
|
|||
| Cure Time |
10.0
min @Temperature 149 °C |
0.167
hour @Temperature 300 °F |
|
|
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 46A
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
|
|||