Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Cure Time = 4320 min Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Cure Time 30.0 - 4320 min
0.500 - 72.0 hour
Average value: 854 min Grade Count:23
Overview of materials for Epoxy, High Temperature
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val..
Cure Time 180 - 4320 min
3.00 - 72.0 hour
Average value: 1890 min Grade Count:5
Overview of materials for Silicone, RTV, Encapsulation Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value..
Cure Time 1440 - 4320 min

@Temperature 23.9 °C
24.0 - 72.0 hour

@Temperature 75.0 °F
Master Bond EP37-3FLSP Optically Clear Epoxy Has Low Exotherm
Description: Master Bond EP37-3FLSP is a very flexible, low viscosity, optically clear two component epoxy resin system designed for high performance bonding, coating and casting applications. It fe..
Cure Time 1440 - 4320 min
24.0 - 72.0 hour
(1-3 Days)
Abatron AboWeld 8104-12 Polysulfide-Epoxy Sealant and Caulk
AboWeld 8104-12 is a 2-part, 100% solids, liquid or filled polysulfide-epoxy. It is available in many colors. It is often used with sand and gravel to mix grouts for filling and resurfacing. It is p..
Cure Time 1440 - 4320 min
24.0 - 72.0 hour
(1-3 Days)
Abatron AboWeld 8104-13 Polysulfide-Epoxy Sealant and Caulk
AboWeld 8104-13 is a 2-part, 100% solids, liquid or filled polysulfide-epoxy. It is available in many colors. It has high hardness and rigidity, very low elongation, and is often used with sand or o..
Cure Time 1440 - 4320 min

@Temperature 25.0 °C
24.0 - 72.0 hour

@Temperature 77.0 °F
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System
Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru..
Cure Time 2880 - 4320 min
48.0 - 72.0 hour
ambient temperatures
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System
Master Bond Polymer System EP39MHT is a low viscosity, two component, epoxy resin system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to..
Cure Time 1.50 - 4320 min
0.0250 - 72.0 hour
Average value: 324 min Grade Count:27
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..