Polymer Property : Cure Time = 48.0 hour Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Cure Time 1440 - 2880 min
24.0 - 48.0 hour
hard dry (return to service)
Industrial Nanotech Nansulateâ„¢ GP Translucent Insulation Coating
Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology. This grade is for general purpose insulation.NANSULATEâ„¢ liquid applied insulation is a prem..
Cure Time 1440 - 2880 min
24.0 - 48.0 hour
hard dry (return to service)
Industrial Nanotech Nansulateâ„¢ High Heat Translucent Insulation Coating
Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology.NANSULATEâ„¢ liquid applied insulation is a premium industrial grade rust proofing protective ..
Cure Time 1440 - 2880 min
24.0 - 48.0 hour
hard dry (return to service)
Industrial Nanotech Nansulateâ„¢ PT Translucent Insulation Coating
Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology. This grade is for general insulation use for pipes, tanks, and metallic surfaces.NANSULATEâ„¢..
Cure Time 1440 - 2880 min
<br>@Temperature >=18.0 °C
24.0 - 48.0 hour
<br>@Temperature >=64.4 °F
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive
Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh..
Cure Time 2160 - 2880 min
36.0 - 48.0 hour
90% of maximum strength developed within
Master Bond EP21TDCN Two Component Nickel Conductive Epoxy Adhesive
Product Description: Master Bond Polymer System EP21TDCN is a two component, nickel filled, electrically conductive, adhesive for high performance bonding, formulated to cure at room temperature or ..
Cure Time 1440 - 2880 min
<br>@Temperature 23.0 °C
24.0 - 48.0 hour
<br>@Temperature 73.4 °F
Master Bond Mastersil 150 Two Part, Condensation Cured, Flexible Silicone
Master Sil 150 is a 2 part condensation cured liquid silicone which, after the addition of curing agent 150, cures at room temperature to a tough, resilient silicone rubber potting and encapsulation..
Cure Time 1440 - 2880 min
<br>@Temperature 23.0 °C
24.0 - 48.0 hour
<br>@Temperature 73.4 °F
Master Bond Mastersil 700 One Component High Temperature Resistant Silicon
Master Bond MasterSil 700 is a ready-to-use, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. It remains flexible and..
Cure Time 1440 - 2880 min
<br>@Temperature 23.0 °C
24.0 - 48.0 hour
<br>@Temperature 73.4 °F
Master Bond Mastersil 701 One Component, Room Temperature Curing Silicone Elastomer
Master Bond Master Sil 701 is a ready-to-use, one component, high performance silicone elastomer compound for bonding, and sealing protective coatings and formed-in-place gaskets. It cures at ambien..
Cure Time 1440 - 2880 min
<br>@Temperature 23.0 °C
24.0 - 48.0 hour
<br>@Temperature 73.4 °F
Master Bond Mastersil 702 One Component, Room Temperature Curing Silicone Elastomer
Master Bond Master Sil 702 is ready-to-use, one component high performance silicone elastomer compound for bonding and sealing. Master Sil 702 is heat resistant to 450°F. It is supplied as an easy ..
Cure Time 1440 - 2880 min
<br>@Temperature 23.0 °C
24.0 - 48.0 hour
<br>@Temperature 73.4 °F
Master Bond Mastersil 705 One Component Room Temperature Curing Silicon Elastomer
Master Bond Master Sil 705 is a one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. This material is a translucent nonco..
Cure Time 1440 - 2880 min
<br>@Temperature 23.0 °C
24.0 - 48.0 hour
<br>@Temperature 73.4 °F
Master Bond Mastersil 800 One Component, Room Temperature Curing Silicone
MasterSil 800 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed-in-place gaskets. This specialty system features ultra high temp..
Cure Time 1440 - 2880 min
<br>@Temperature 23.0 °C
24.0 - 48.0 hour
<br>@Temperature 73.4 °F
Master Bond Mastersil 801 One Component, Room Temperature Curing, Silicone System
MasterSil 801 is an easy to use, one component, high performance silicone elastomer compound. MasterSil 801 features non-corrosive cure and serviceability up to 300°C; it exhibits good stability at..
Cure Time 360 - 2880 min
6.00 - 48.0 hour
Full Cure; Unprimed
Loctite® Gasket Eliminator® 509 Flange Sealant
Anaerobic GasketingLoctite® 509 Flexible Cure Gasket Eliminator® Flange SealantProduct withstands minor flange movements caused by vibrations. It will not run when applied to vertical surfaces. F..
Cure Time 1440 - 2880 min
24.0 - 48.0 hour
3M Scotch-Weld™ DP-100NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP-100NS is a two-part adhesives offering fast cure and machinability.Information provided by 3M
Cure Time 1440 - 2880 min
24.0 - 48.0 hour
3M Scotch-Weld™ DP-100 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP-100 is a two-part adhesives offering fast cure and machinability.Information provided by 3M
Cure Time 1440 - 2880 min
24.0 - 48.0 hour
3M Scotch-Weld™ DP100 FR Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP100 FR is a two-part flame retardant (self-extinguishing) version of Scotch-Weld DP100. It meets the UL94 V-O Burn Test requirements and has a work life of 4-8 mi..
Cure Time 1440 - 2880 min
24.0 - 48.0 hour
Full cure
3M Scotch-Weld™ DP820 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Cure Time 360 - 2880 min
6.00 - 48.0 hour
Full Cure; Unprimed
Loctite® 573 Semi-rigid Cure Anaerobic Sealant
Anaerobic GasketingLoctite® 573 Semi-rigid Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Slow curing for extended assembly operations