| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Shelf Life |
14.0
Month @Temperature -18.0 °C |
14.0
Month @Temperature -0.400 °F |
|
|
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Modulus 12k carbon UD tape 110 g/m2
Information provided by HexCel
|
|||
| Shelf Life |
14.0
Month @Temperature -18.0 °C |
14.0
Month @Temperature -0.400 °F |
|
|
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Strength 12k carbon UD tape Not Supported 150 g/m2
Information provided by HexCel
|
|||
| Shelf Life |
14.0
Month @Temperature -18.0 °C |
14.0
Month @Temperature -0.400 °F |
|
|
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, Intermediate Modulus 12k carbon UD tape 150 g/m2
Information provided by HexCel
|
|||
| Shelf Life |
14.0
Month @Temperature -18.0 °C |
14.0
Month @Temperature -0.400 °F |
|
|
Hexcel® HexPly® EH25 180°C Curing Epoxy Matrix
HexPly® EH25 is a high performance, tough 180°C curing matrix for us in aerospace primary structures. HexPly® EH25 is a self-extinguishing epoxy resin with controlled flow. HexPly® EH25 prepregs..
|
|||
| Shelf Life |
14.0
Month @Temperature -18.0 °C |
14.0
Month @Temperature -0.400 °F |
|
|
Hexcel® HexPly® ES 84 120°C Curing Epoxy Matrix, Aramid Balanced fabric 175 g/m2
Information provided by HexCel
|
|||
| Shelf Life |
14.0
Month @Temperature -18.0 °C |
14.0
Month @Temperature -0.400 °F |
|
|
Hexcel® HexPly® ES 84 120°C Curing Epoxy Matrix, E-glass Balanced fabric 390 g/m2
Information provided by HexCel
|
|||
| Shelf Life |
14.0
Month @Temperature -18.0 °C |
14.0
Month @Temperature -0.400 °F |
|
|
Hexcel® HexPly® ES/EH 84 120°C Curing Epoxy Matrix
HexPly® ES/EH 84 matrix is a structural epoxy resin for tubular parts designed for low pressure curing in the manufacture of sports goods and for industrial applications. It is ideal for the follow..
|
|||
| Shelf Life |
14.0
Month @Temperature -18.0 °C |
14.0
Month @Temperature -0.400 °F |
|
|
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Strength 12k carbon UD tape supported S25 150 g/m2
Information provided by HexCel
|
|||
| Shelf Life |
14.0
Month @Temperature -18.0 °C |
14.0
Month @Temperature -0.400 °F |
|
|
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix
HexPly® M12 is a good performance, self extinguishing, tough epoxy matrix for use in helicopter blades. It exhibits good fatigue life and hot/wet performances up to 100ºC. HexPly® M12 is supplied..
|
|||
| Shelf Life |
14.0
Month @Temperature -18.0 °C |
14.0
Month @Temperature -0.400 °F |
|
|
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber
Information provided by HexCel
|
|||
| Shelf Life |
14.0
Month @Temperature -18.0 °C |
14.0
Month @Temperature -0.400 °F |
|
|
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber
Information provided by HexCel
|
|||
| Shelf Life |
14.0
Month @Temperature -18.0 °C |
14.0
Month @Temperature -0.400 °F |
|
|
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Information provided by HexCel
|
|||