| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Shelf Life | 3.00 Month | 3.00 Month | |
|
Gwent Electronic Materials C2000215D4 Silver / Silver Chloride Paste
C2000215D4 has a ratio of Silver to Silver Chloride of 50/50. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a ..
|
|||
| Shelf Life | 3.00 Month | 3.00 Month | |
|
Gwent Electronic Materials C2040308D2 Silver/Silver Chloride Paste
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 40/60. The paste is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing. The paste..
|
|||
| Shelf Life | 3.00 Month | 3.00 Month | |
|
Lucite International Colacryl ® TS1778 Acrylic Solution Resin
Colacryl TS 1778 is a self cross-linking acrylic copolymer designed for adhesive applications. Once dried, a film cast from this product remains permanently tacky.Suggested Uses: Pressure-sensitiv..
|
|||
| Shelf Life |
3.00
-
6.00
Month @Temperature 23.9 °C |
3.00
-
6.00
Month @Temperature 75.0 °F |
in unopened containers |
|
Master Bond EP21TDCNFL Two Component Nickel Conductive Epoxy Adhesive
Master Bond Polymer System EP21TDCNFL is a two component, nickel filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl..
|
|||
| Shelf Life | 3.00 - 6.00 Month | 3.00 - 6.00 Month | |
|
Master Bond EP21TDCSMed Two Component, Silver Conductive USP Class VI Epoxy
Master Bond Polymer System EP21TDCS MED is a two component, silver filled, electrically conductive adhesive/sealant that meets USP Class VI specifications for medical applications. The high strength..
|
|||
| Shelf Life |
3.00
-
6.00
Month @Temperature 23.9 °C |
3.00
-
6.00
Month @Temperature 75.0 °F |
in original unopened containers |
|
Master Bond Supreme 10AOHT-LO High Shear and Peel Strength Epoxy
Description: Master Bond Supreme 10AOHT-LO has a combination of properties consisting of excellent thermal conductivity, superior electrical insulation, great adhesion to a wide variety of substrate..
|
|||
| Shelf Life |
3.00
-
6.00
Month @Temperature 4.44 - 10.0 °C |
3.00
-
6.00
Month @Temperature 40.0 - 50.0 °F |
in original unopened containers |
|
Master Bond Supreme 3HT-80 One Component, Toughened, Heat Curing Epoxy
Master Bond Polymer System Supreme 3HT-80 is a one component, heat curing epoxy adhesive/sealant featuring excellent physical and chemical resistance properties and a minimal curing temperature of 1..
|
|||
| Shelf Life | 3.00 Month | 3.00 Month | At 5°C |
|
Tra-Con Tra-Bond 77-1S One Component SMD Adhesive
TRA-BOND 77-1S one component, solvent-free, insulating epoxy adhesive is designed specifically for attaching surface mounted devices (SMDs) to printed circuit boards prior to wave solder. TRA-BOND 7..
|
|||
| Shelf Life |
3.00
Month @Temperature -40.0 °C |
3.00
Month @Temperature -40.0 °F |
|
|
Loctite® 3533 Low viscosity fill encapsulant Fill Encapsulant
COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp..
|
|||
| Shelf Life |
3.00
Month @Temperature -40.0 °C |
3.00
Month @Temperature -40.0 °F |
|
|
Loctite® 3564 Fast flow epoxy, moderate CTE and Tg Fast Flow Underfill
COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp..
|
|||
| Shelf Life |
3.00
Month @Temperature -40.0 °C |
3.00
Month @Temperature -40.0 °F |
|
|
Loctite® 3566 Rapid Flow Low Profile Underfill
COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp..
|
|||
| Shelf Life |
3.00
-
6.00
Month @Temperature 23.9 °C |
3.00
-
6.00
Month @Temperature 75.0 °F |
in original unopened container |
|
Master Bond EP36AN One Part, Toughened, B-Stage Epoxy
Description: Master Bond EP36AN is a unique one component, high performance epoxy for bonding, encapsulation, potting and coating featuring thermal conductivity, electrical insulation and high tempe..
|
|||
| Shelf Life | >= 3.00 Month | >= 3.00 Month | Plastic syringes |
|
Master Bond Supreme 10HTFS Silver Conductive Microelectronic Epoxy
Description: Master Bond Polymer System Supreme 10HTFS “snap cure” epoxy is a formulated system featuring a combination of high performance properties including high shear and peel strength, outst..
|
|||
| Shelf Life | 3.00 Month | 3.00 Month | At 5°C |
|
Tra-Con Tra-Bond 968-5 High Dielectric Constant Epoxy Adhesive
TRA-BOND 968-5 is a high dielectric constant epoxy adhesive. This one component, electrically insulating epoxy adhesive is designed for chip bonding.Information provided by Tra-Con Inc.
|
|||
| Shelf Life | 3.00 Month | 3.00 Month | Moisture absorption after extended storage |
|
Fainplast Compounds EVAtech 801S Ethylene Vinyl Acetate Foam
EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds
|
|||
| Shelf Life |
3.00
Month @Temperature 30.0 °C |
3.00
Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
|
Fainplast Compounds Hax™ HFC 0108/4 Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding, designed to meet BS 7846Information provided by Fainplast Compounds
|
|||
| Shelf Life |
3.00
Month @Temperature 30.0 °C |
3.00
Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
|
Fainplast Compounds Hax™ HFX 507 Crosslinkable HFFR Cable Compound
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing; Insulation; easy processingInformation provided..
|
|||
| Shelf Life |
3.00
Month @Temperature 30.0 °C |
3.00
Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
|
Fainplast Compounds Hax™ HFX 509 Crosslinkable HFFR Cable Compound
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Insulation for solar cablesInformation provided by Fainpla..
|
|||
| Shelf Life |
3.00
Month @Temperature 30.0 °C |
3.00
Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
|
Fainplast Compounds Hax™ HFX 515 Crosslinkable HFFR Cable Compound
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing, InsulationInformation provided by Fainplast Com..
|
|||
| Shelf Life |
3.00
Month @Temperature 30.0 °C |
3.00
Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
|
Fainplast Compounds Hax™ HFC 0108 Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding, designed to meet BS 6724Information provided by Fainplast Compounds
|
|||
| Shelf Life |
3.00
Month @Temperature 4.44 °C |
3.00
Month @Temperature 40.0 °F |
|
|
Arlon 30400R060 0.06" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should..
|
|||
| Shelf Life |
3.00
Month @Temperature 23.9 °C |
3.00
Month @Temperature 75.0 °F |
From date of manufacture |
|
Arlon P29514R020P 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassThis data represents typical values for the production material. The data should..
|
|||
| Shelf Life |
3.00
Month @Temperature 7.22 °C |
3.00
Month @Temperature 45.0 °F |
From date of manufacture |
|
Arlon P30670R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassAppearance: Red silicone gum on fiberglass with polymer release linersThis data represents typical values for the..
|
|||
| Shelf Life |
3.00
Month @Temperature 23.9 °C |
3.00
Month @Temperature 75.0 °F |
From date of manufacture |
|
Arlon R36029R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass This data represents typical values for the production ..
|
|||
| Shelf Life |
3.00
Month @Temperature 4.44 °C |
3.00
Month @Temperature 40.0 °F |
|
|
Arlon 30850S125 0.125" Uncured, Unsupported Silicone Rubber on a Kodacel Carrier
Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should..
|
|||
| Shelf Life |
3.00
Month @Temperature 21.1 °C |
3.00
Month @Temperature 70.0 °F |
From date of manufacture |
|
Arlon 32400R040 0.040" (1.02 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material..
|
|||
| Shelf Life |
3.00
Month @Temperature 1.67 - 7.22 °C |
3.00
Month @Temperature 35.0 - 45.0 °F |
From date of manufacture |
|
Arlon R34260N005 0.005" (0.127 mm) Unsupported/Uncured Rubber with Fiberglass Substrate
Design/Construction:Side 1: Unsupported/Uncured Rubber Appearance: Clear gum on release linersThis data Represents typical values for the production material. The data should not be used to write, o..
|
|||
| Shelf Life |
3.00
Month @Temperature 7.22 °C |
3.00
Month @Temperature 45.0 °F |
From date of manufacture |
|
Arlon R38020B020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material. The data should not be used to wr..
|
|||
| Shelf Life | 3.00 Month | 3.00 Month | |
|
Gwent Electronic Materials C2010809D3 Silver Ink
Silver Ink C2010809D3 is designed for printing via, when screen printed onto LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the ma..
|
|||
| Shelf Life |
3.00
-
6.00
Month @Temperature 23.9 °C |
3.00
-
6.00
Month @Temperature 75.0 °F |
in original unopened containers |
|
Master Bond Supreme 10HTFL One Part Epoxy Cures at 250°F
Description: Master Bond Polymer System Supreme 10HTFL features a blend of physical properties including outstanding peel strength, very high shear strength and a wide service temperature range of 4..
|
|||