| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Shelf Life | 5.00 Month | 5.00 Month | shelf life at 4ºC |
|
Loctite® Output™ 5404 Heat Cure Silicone
Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or..
|
|||
| Shelf Life | 5.00 Month | 5.00 Month | |
|
Dow Corning SYL-OFF® 292 COATING
Syl-Off® 292 Coating is one of several alternative base polymers for use in Syl-Off solvent-based, tin-catalyzed release coatings. It is a 30 percent solids dispersion of a blend of reactive siloxa..
|
|||
| Shelf Life | <= 5.00 Month | <= 5.00 Month | |
|
Abatron AboWeld 8708-8 One-Component Structural/Dielectric Epoxy
AboWeld 8708-8 is a highly filled, class H (180°C) structural, heat-conductive adhesive paste for FAST high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating;..
|
|||
| Shelf Life | 5.00 - 8.00 Month | 5.00 - 8.00 Month | |
|
Abatron AboCast 8103-13 One-Component Epoxy
AboCast 8103-13 is the low-viscosity one-component clear epoxy system with deep impregnation that offers high performance at relatively high temperatures. It is best for thin-wall casting. Suggested..
|
|||
| Shelf Life | 5.00 - 8.00 Month | 5.00 - 8.00 Month | |
|
Abatron AboCast 8103-14 One-Component Epoxy
AboCast 8103-14 is the lowest-viscosity one-component epoxy system with heavy-duty structural and dielectric properties. It is clear and has maximum wetting and penetration. Suggested Uses: Casting..
|
|||
| Shelf Life | 5.00 - 8.00 Month | 5.00 - 8.00 Month | |
|
Abatron AboCast 8501-6 One-Component Epoxy
AboCast 8501-6 is a clear, high-temperature one-component epoxy system for very high-temperature uses. It offers the highest heat resistance of the clear resins. Suggested Uses: Casting; Potting; E..
|
|||
| Shelf Life | 5.00 - 8.00 Month | 5.00 - 8.00 Month | |
|
Abatron AboCast 8504-1 One-Component Epoxy
AboCast 8504-1 is a clear, all-purpose one-component epoxy system, with an optimum balance of properties for most casting, adhesive, impregnation, and coating applications.
|
|||
| Shelf Life | 5.00 - 8.00 Month | 5.00 - 8.00 Month | |
|
Abatron AboCast 8504-5 One-Component Epoxy
AboCast 8504-5 is a clear, plasticized one-component epoxy system with very high strength and impact. It provides exceptional physical properties and thermal shock resistance from sub-zero to modera..
|
|||
| Shelf Life | <= 5.00 Month | <= 5.00 Month | |
|
Abatron AboCast 8708-10 One-Component Structural/Dielectric Epoxy
AboCast 8708-10 is a highly filled, class H (180°C) structural, castable adhesive compound for FAST high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating; Em..
|
|||
| Shelf Life |
5.00
Month @Temperature 17.0 - 27.0 °C |
5.00
Month @Temperature 62.6 - 80.6 °F |
|
|
Parker Chomerics CHO-FORM 5538 Conductive Form-In-Place Gaskets
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..
|
|||