Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shelf Life = 9.00 Month Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Shelf Life 9.00 Month
9.00 Month
Parker Chomerics CHO-BOND 589-29 Conductive Epoxy
Low cost, highly conductive adhesive system which combines the strong adhesion characteristics of an epoxy with the superior conductivity of silver. CHO-BOND 589-29 adhesive meets the most exacting ..
Shelf Life 9.00 Month
9.00 Month
Bulk
Parker Chomerics CHO-SHIELD® 4900 Conductive Coating
CHO-SHIELD® 4900 silver-filled acrylic coating provides the highest levels of EMI shielding, as well as anti-static protection and grounding surfaces. It offers convenient fast tack and drying. Fil..
Shelf Life 9.00 Month
9.00 Month
@ 70°F
Parker Chomerics CHO-SHIELD® 4904 Conductive Coating
Conductive Nickel-Filled Acrylic Coating. This is the lowest coast in the family of nickel-filled, electrically conductive acrylic coatings. CHO-SHIELD® 4904 is resistant to solvent attack and to f..
Shelf Life 9.00 Month
9.00 Month
Parker Chomerics CHO-SHIELD® 4914 Conductive Coating
Conductive Solvent-Resistant Acrylic Coating. Formulated for high resistance to solvent attack, CHO-SHIELD® 4914 is an electrically conductive, one-component acrylic coating. Compared to zinc arc s..
Shelf Life 9.00 Month
9.00 Month
Parker Chomerics CHO-SHIELD® 576 Platable Silver Epoxy Coating
Description: CHO-SHIELD® 576 coating is a two component, silver filled, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric plastic substrate. This coating ..
Shelf Life 9.00 Month
9.00 Month
Unopened Container
Parker Chomerics Tecknit® 73-00008 Electrically Conductive Acrylic and Polyurethane Paint
Description: TECKNIT manufactures a highly conductive acrylic and polyurethane paints filled with silver. These coatings provide a cost effective method for shielding and grounding plastic enclosure..
Shelf Life 9.00 Month
9.00 Month
Unopened Container
Parker Chomerics Tecknit CON/RTV-II 2 Part Silver Filled RTV
Description: TECKNIT electrically conductive, medium viscosity adhesive- sealant system. It is formulated with a special conductive material producing its own unique advantages. After full cure, the..
Shelf Life 9.00 Month
9.00 Month
Unopened Container
Parker Chomerics Tecknit TeckBond™-C Silver-Plated Copper-Filled Adhesive
Description: TECKBOND-C is a silicone rubber base filled with silver-plated copper particles to produce a highly conductive one-component adhesive sealant. The system is an RTV moisture-cured compou..
Shelf Life 9.00 Month
9.00 Month
Unopened Container
Parker Chomerics Tecknit TeckBond™-NC Nickel Coated Graphite-Filled Adhesive
Description: TECKBOND-NC is a silicone rubber base filled with nickel coated graphite particles to produce a highly conductive one-component adhesive sealant. The system is an RTV moisture-cured com..
Shelf Life 9.00 Month
9.00 Month
unopened
Parker Chomerics CHO-BOND 2165 Polyurethane Sealant
Conductive sealant is a stabilized copper filled, two component polyurethane. It has excellent electrical and physical properties for aerospace and military applications. CHO-BOND® 2165 sealant is ..
Shelf Life 9.00 Month
9.00 Month
Parker Chomerics CHO-FLEX 4430 Conductive Ink
CHO-FLEX polyester inks were developed for the membrane keyboard and sensor industries. The ink bond to Mylar films, and can be creased, heat-formed or scratched without affecting their performance...
Shelf Life 9.00 Month
9.00 Month
Parker Chomerics CHO-FLEX 4432 Conductive Ink
CHO-FLEX polyester inks were developed for the membrane keyboard and sensor industries. The ink bond to Mylar films, and can be creased, heat-formed or scratched without affecting their performance...
Shelf Life 9.00 Month
9.00 Month
Parker Chomerics CHO-SHIELD® 579 Low VOC Silver Epoxy Coating
Description: CHO-SHIELD® 579 coating is a two component, silver-filled, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric substrate. This coating was spec..
Shelf Life 9.00 Month
<br>@Temperature 25.0 °C
9.00 Month
<br>@Temperature 77.0 °F
Lord Adhesives Thermosetâ„¢ SC-303 Silicone Encapsulant, Flame Retardant
Lord SC-303 is a two component silicone elastomer that provides excellent thermal conductivity, while retaining the other desirable properties associated with silicones. It is a low viscosity, easil..
Shelf Life 9.00 Month
<br>@Temperature 20.0 °C
9.00 Month
<br>@Temperature 68.0 °F
in unopened original container
Heraeus Cleviosâ„¢ P Conductive Sulfonate Polymer for Antistatic Coatings
Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P is an antistatic material based on PEDOT:PSS..
Shelf Life 9.00 Month
<br>@Temperature 20.0 °C
9.00 Month
<br>@Temperature 68.0 °F
in unopened original container
Heraeus Cleviosâ„¢ P HC V4 Conductive Sulfonate Polymer for Antistatic Coatings
Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P HC V4 is an antistatic material based on PED..
Shelf Life 9.00 Month
9.00 Month
shelf life at 5ºC
Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive
Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or..
Shelf Life 9.00 Month
9.00 Month
Dow Corning SM 8715 EX
A reactive epoxyfunctional silicone emulsion; imparts very good water repellency, very good stability, high whiteness retention and improves fabric physical properties.Information provided by Dow Co..
Shelf Life 9.00 Month
9.00 Month
Dow Corning SYL-OFF® PMCPEM 7974 Emulsion Coating
Syl-Off® EM 7974 is an emulsion based silicone release coating, excellent for bakery release performance and is specifically developed for application during the paper making process.Information pr..
Shelf Life 9.00 Month
9.00 Month
Dow Corning 3559 NEUTRAL ADHESIVE SEALANT BLACK
DOW CORNING 3559 is a black, 1- component, non-flowing, silicone adhesive with fast deep section cure. It forms high strength, medium modulus flexible bonds to metal, glass, ceramic substrates and m..
Shelf Life 9.00 Month
<br>@Temperature <=26.7 °C
9.00 Month
<br>@Temperature <=80.1 °F
3M AC-236 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t..
Shelf Life 9.00 Month
<br>@Temperature <=26.7 °C
9.00 Month
<br>@Temperature <=80.1 °F
3M AC-236 Class C-20 Aerospace Sealant
3M Aerospace Sealant AC-236 Class C are two-component, manganese dioxide cured, liquid polysulfide polymer systems providing excellent fuel tank and fuselage seals. They have outstanding resistance ..
Shelf Life 9.00 Month
<br>@Temperature <=26.7 °C
9.00 Month
<br>@Temperature <=80.1 °F
3M AC-240 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan..
Shelf Life 9.00 Month
<br>@Temperature <=26.7 °C
9.00 Month
<br>@Temperature <=80.1 °F
3M AC-251 Black Class B-1 Aerospace Sealant
3M Aerospace Sealant AC-251 Black Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate ai..
Shelf Life 9.00 Month
<br>@Temperature <=26.7 °C
9.00 Month
<br>@Temperature <=80.1 °F
3M AC-251 Gray Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-251 Gray Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate air..
Shelf Life 9.00 Month
<br>@Temperature <=26.7 °C
9.00 Month
<br>@Temperature <=80.1 °F
3M AC-350 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are..
Shelf Life 9.00 Month
<br>@Temperature <=26.7 °C
9.00 Month
<br>@Temperature <=80.1 °F
3M AC-350 Class B-12 Aerospace Sealant
3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are..
Shelf Life 9.00 Month
<br>@Temperature <=26.7 °C
9.00 Month
<br>@Temperature <=80.1 °F
3M AC-730 Class C-4 (168) Aerospace Sealant
3M Aerospace Sealant AC-730 Class C are two-part, manganese-cured, non-chromate corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corrosion on a..
Shelf Life 9.00 Month
<br>@Temperature <=26.7 °C
9.00 Month
<br>@Temperature <=80.1 °F
3M AC-370 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-370 Class B are fast cure, low density polysulfide sealants suitable for fuel tank and fuselage applications. These two-component, manganese dioxide cured sealants are solven..
Shelf Life 9.00 Month
9.00 Month
Parker Chomerics CHO-SHIELD® 2044 Nickel-Filled Acrylic Coating for EMI Shielding
Description: CHO-SHIELD® 2044 is an electrically conductive, one-component nickel-filled acrylic coating that is especially formulated for application on plastics to provide modest EMI shielding. C..