| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
|
PTS Tristar® PC-10R-CL(15) 15 MFI Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 111-64 Thermoplastic Elastomer
(discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 221-55 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 241-80 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 241-87 Thermoplastic Elastomer
(discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 261-87 Thermoplastic Elastomer
(discontinued **)
A hard, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance for use in wet electrical wire and cable applications. This gra..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Vyram™ 9101-55 Thermoplastic Elastomer
(discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Vyram™ 9101-85 Thermoplastic Elastomer
(discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
|
|||
| Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
|
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
|
PTS Tristar® PC-10FR-(8) 8 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
|
PTS Tristar® PC-10FR-(V8) 8 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
|
PTS Tristar® PC-10R 10 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
|
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
|
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
|
Mitsubishi Iupilon® H2001R 23 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
|
Samyang Trirex® PC-3025N2 10 MFI Flame Retardant Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 103-50 Thermoplastic Elastomer
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 121-62M100 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult ..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer
A hard, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer
(discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer
(discontinued **)
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Vyram™ 9201-65 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 221-80 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
|
|||
| Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
|
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
|
|||