Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 149 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 149 - 171 °C
300 - 340 °F
ASTM D789
Niche Polymer PPCG20BK Copolymer PP, 20% Glass Fiber Filled
Information provided by Niche Polymer
Melt Temperature 149 - 171 °C
300 - 340 °F
ASTM D789
Niche Polymer PPCM15BK Copolymer PP
Information provided by Niche Polymer
Melt Temperature 149 - 171 °C
300 - 340 °F
ASTM D789
Niche Polymer PPCM6BK Copolymer PP
Information provided by Niche Polymer
Melt Temperature 149 - 232 °C
300 - 450 °F
DuPont Nucrel® 535 Ethylene-Methacrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 535 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Melt Temperature 149 - 232 °C
300 - 450 °F
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for..
Melt Temperature 149 - 232 °C
300 - 450 °F
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Melt Temperature 149 - 279 °C
300 - 534 °F
Average value: 219 °C Grade Count:177
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Melt Temperature 149 °C
300 °F
Spartech E65050 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
Melt Temperature 149 - 232 °C
300 - 450 °F
DuPont Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin
Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC1390AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC1390 is used primarily in extrusion-coating applications that require fast line speeds and relatively low coating weights. When compared with other low-density po..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC1924AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC1924 is a resin that is widely used in the boardstock coating industry. This material has an excellent combination of low neck-in, ease of processing, good chill-..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC4042AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC4042 is a low density resin designed for applications, such as sugar pouches and freezer wrap, where high coating speeds and good drawdown are required. The combi..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC4056AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC4056 is a natural low density material with an 80 melt index.FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All in..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC800AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC800 is a general-purpose low-density formulation used for extrusion coating applications.Application/UsesGeneral extrusion coatingFDA: This material complies with..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC812AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC812 is a natural low-density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a backing to carpet to bin..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EM1550AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM1550 is a low-density formulation used for injection molding applications.Application/UsesFlexible medicalLidsMedicalFDA: This material complies with FDA regulati..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EM182AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM182 is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easi..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EM184AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM184 is a low density injection-molding formulation suggested for the production of closures where a high melt index is needed to meet shrinkage requirements and f..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EM800AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM800 is a general-purpose low-density formulation used for injection molding applications that require good stress-crack resistance.Application/UsesCosmetics/perso..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EM808AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM808 is a general-purpose low-density formulation used for injection molding applications and general purpose extrusion.Application/UsesFood packagingMedicalFDA: T..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EM811AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM811 is a low-density polyethylene used for injection molding. It is characterized by high flow and low stiffness.Application/UsesFlexible medicalMedicalFDA: This ..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EM812AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM812 is a low-density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easi..
Melt Temperature 149 - 232 °C
300 - 450 °F
DuPont Nucrel® 599 Ethylene-Methacrylic Acid Copolymer Resin
Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Melt Temperature 149 °C
300 °F
Axiall 47551 Flexible PVC
Injection molding compound designed for automotive encapsulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 149 °C
300 °F
Axiall 7540 Moldings & Extrusions Flexible PVC
A high quality clear outdoor grade PVC molding and extrusion compound formulated for good UV light resistance and excellent low temperature properties.Information provided by Georgia GulfGeorgia Gul..
Melt Temperature 149 - 327 °C
300 - 620 °F
Average value: 214 °C Grade Count:42
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and..
Melt Temperature 149 - 232 °C
300 - 450 °F
Average value: 193 °C Grade Count:3
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min..
Melt Temperature 149 - 310 °C
300 - 590 °F
Average value: 221 °C Grade Count:81
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..
Melt Temperature 149 °C
300 °F
Axiall 46234B Flexible PVC
Injection molding compound designed for automotive encapsulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 149 - 240 °C
300 - 464 °F
Average value: 184 °C Grade Count:40
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..
Copyright © lookpolymers.com All Rights Reserved