Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 182 - 199 °C | 360 - 390 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L7703 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 185 - 199 °C | 365 - 390 °F | |
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE) Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough.. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | |
Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Cellular E2010 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Physical Properties were measured on flat cellular profiles with a 0.59 specific gravity natural compound.Information provided by PolyOne |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible A65M0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible B85B0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible R100AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible R130AE White 41 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible SL60 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible XV3878G Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible C6502 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 199 °C | 379 - 390 °F | |
PolyOne Geon™ Vinyl Flexible C7000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 199 °C | 379 - 390 °F | |
PolyOne Geon™ Vinyl Flexible C70U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | |
PolyOne Geon™ Vinyl Flexible R5145A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | with BUR of 1.5:1 or higher |
Westlake EF378 Low Density Polyethylene WESTLAKE EF378 is suggested for cast film applications. It has excellent haze and gloss, good strength, good processability, and good heat sealability.Application/UsesDiaper linersGeneral purpose cl.. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | with BUR of 1.5:1 or higher |
Westlake EF403 Low Density Polyethylene WESTLAKE polyethylene EF403 is a fractional melt low-density formulation suggested for use in clarity shrink applications. This LDPE formula exhibits excellent skrinkability, and has very good optic.. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | with BUR of 1.5:1 or higher |
Westlake EF418 Low Density Polyethylene WESTLAKE polyethylene EF418 is a LDPE formula with excellent optical properties suggested by light and medium duty packaging.Application/UsesLight and medium duty produce bagsClarity packagingGenera.. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | with BUR of 1.5:1 or higher |
Westlake Elevate™ EF439 4.0% Ethylene Vinyl Acetate Copolymer Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio.. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | with BUR of 1.5:1 or higher |
Westlake Elevate™ EF561 6.5% Ethylene Vinyl Acetate Copolymer Westlake EF 561 resin is a fractional melt index 6.5% EVA copolymer designed for ice bags, frozen food bags, and other films that require excellent toughness and good heat sealing characteristics. T.. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | Extrusion |
Lubrizol Estane® 2103-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | Extrusion |
Lubrizol Estane® 2103-80AEN Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: NSF Standard 61 certified, FDA complianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane produ.. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | Extrusion |
Lubrizol Estane® 2103-80PF Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
Axiall HHW-191 Rigid PVC, Extrusion Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemic.. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Walled Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |