| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 204 - 260 °C | 399 - 500 °F | Air purge at equilibrium conditions |
|
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade
High heat resistance, Sparking water-white clarity, Good chemical resistance, High modulus, for superior shear and torque resistanceApplications: Light pipes and lighting, High heat microwave packag..
|
|||
| Melt Temperature | 204 °C | 400 °F | |
|
ExxonMobil Vyram™ 9101-65 Thermoplastic Elastomer
(discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
|
|||
| Melt Temperature | 204 °C | 400 °F | |
|
ExxonMobil Vyram™ 9201-85 Thermoplastic Elastomer
(discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
|
|||
| Melt Temperature | 204 - 232 °C | 400 - 450 °F | Molding |
|
PolyOne Edgetek® AS-20GB/000 Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
(discontinued **)
Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Melt Temperature | 204 °C | 399 °F | |
|
Eastman 5254 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations
(discontinued **)
Resin Type: VA CopolymerCharacteristics: Good adhesion, Good processability and bubble stability, Low slip, Medium antiblock, Good optical properties, Good impact strengthApplications:Laminations, H..
|
|||
| Melt Temperature | <= 204 °C | <= 399 °F | |
|
Kleerdex Kydex® P54 Acrylic/PVC Extrusion Compound
(discontinued **)
High impact profile extrusion compoundApplications: Extruded profiles requiring high impact, good chemical resistance, weatherability, and excellent flammability resistance.Features: P54 is extremel..
|
|||
| Melt Temperature | 204 - 218 °C | 400 - 425 °F | |
|
LyondellBasell Petrothene® NA951080 Low Density Polyethylene
ApplicationsPETROTHENE NA 951-080 is designed for use as a base resin for compounding material including gas-injected or chemically expanded insulation. NA 951-080 is a natural, low density, medium..
|
|||
| Melt Temperature | 204 - 238 °C | 400 - 460 °F | |
|
Styrolution Zylar 650 MBS
Zylar® 650 is an impact modified styrene acrylic copolymer that provides a balance of clarity and toughness, with outstanding strength and rigidity. Zylar 650 also has superior processing charact..
|
|||
| Melt Temperature | 204 - 238 °C | 400 - 460 °F | |
|
Styrolution Zylar 960 MBS
ZYLAR 960 is an impact modified styrene acrylic copolymer that provides toughness equivalent to some grades of polycarbonate, good clarity and superior processing characteristics for demanding injec..
|
|||
| Melt Temperature | <= 204 °C | <= 399 °F | Cast Film |
|
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ EF529 is an ethylene vinyl acetate copolymer with 18.5% VA. It contains no slip or antiblock and is designed for blown and cast films requiring excellent optics and low heat seal ..
|
|||
| Melt Temperature | 204 - 216 °C | 400 - 420 °F | |
|
Westlake Hifor Clear SC74580 Linear Low Density Polyethylene
WESTLAKE Hifor Clear Polyethylene SC74580 polymer is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. It doe..
|
|||
| Melt Temperature | 204 - 216 °C | 400 - 420 °F | |
|
Westlake Hifor LT74119 Linear Low Density Polyethylene
WESTLAKE HIFOR Polyethylene LT74119 is a high strength linear low density polyethylene containing medium slip and high antiblock and it contains processing aid. It is designed for blown film applic..
|
|||
| Melt Temperature | 204 - 216 °C | 400 - 420 °F | |
|
Westlake LF2050 Hexene Linear Low Density Polyethylene
Westlake LF2050 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s..
|
|||
| Melt Temperature | 204 - 250 °C | 399 - 482 °F | Extrusion |
|
Total PPH 3762 Polypropylene, Extrusion Grade
Homopolymer fiber grade for staple fiber and multifilament yarnsFading Resistance - FINA 3762 is formulated to resist gas fading while maintaining excellent processing stability up to 250oC.Process ..
|
|||
| Melt Temperature | 204 - 250 °C | 399 - 482 °F | |
|
Total PPH 3764 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics and Multifilament Yarns
Process Stability TOTAL Petrochemicals Polypropylene 3764 features excellent processability and gas fade resistance.FDA. 3764 complies with all applicable FDA regulations for food contact applicat..
|
|||
| Melt Temperature | 204 - 254 °C | 400 - 490 °F | |
|
Ecomass® 1080TU96 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b..
|
|||
| Melt Temperature | 204 - 254 °C | 400 - 490 °F | |
|
Ecomass® 1080ZD95 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b..
|
|||
| Melt Temperature | 204 - 221 °C | 400 - 430 °F | |
|
Ecomass® 4703ZD90 Tungsten Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polym..
|
|||
| Melt Temperature | 204 - 221 °C | 400 - 430 °F | |
|
Ecomass® 4703ZD95 Tungsten Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technical Po..
|
|||
| Melt Temperature | 204 °C | 400 °F | |
|
ExxonMobil Paxon™ BA50-100 Blow Molding Resin
Product Description: BA50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: ..
|
|||
| Melt Temperature | 204 °C | 400 °F | |
|
ExxonMobil Paxon™ BC50-100 Sheet Extrusion and Blow Molding Resin
(discontinued **)
BC50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Information provided by ExxonMobil ..
|
|||
| Melt Temperature | 204 °C | 399 °F | |
|
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber
(discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
|
|||
| Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
|
Ineos Nova 817 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
High flow crystal polystyrene, Custom colorsApplications: Injection molding, Designed for use in high speed, Thin section applications and complex parts designs where custom coloring is a requiremen..
|
|||
| Melt Temperature | 204 - 238 °C | 399 - 460 °F | |
|
PolyOne Stat-Tech™ PP-CP1/000 HF6 Black Polypropylene Impact Copolymer (PP Impact Copolymer)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
|
|||