Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 221 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Melt Temperature 221 - 249 °C
430 - 480 °F
Molding
PolyOne Edgetek® AS-13CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 221 - 243 °C
430 - 470 °F
Molding
PolyOne Edgetek® AS-20CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 221 - 249 °C
430 - 480 °F
Molding
PolyOne Edgetek® AS-20GF-05GB/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedGlass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 221 - 243 °C
430 - 470 °F
Molding
PolyOne Edgetek® AS-30GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 221 - 249 °C
430 - 480 °F
Stock
PolyOne Edgetek® AS- 08CF / 000 ABS - 8% Carbon Fiber Reinforced With ESD Properties  (discontinued **)
Data provided by PolyOne.
Melt Temperature 221 - 249 °C
430 - 480 °F
Stock
PolyOne Stat-Tech™ AS-15CP/000 ABS - 15% Carbon Powder  (discontinued **)
Data provided by PolyOne.
Melt Temperature 221 - 243 °C
430 - 469 °F
Lubrizol Isoplast® 2530 Engineering Thermoplastic Polyurethane Resin for Medical Applications
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Melt Temperature 221 - 229 °C
430 - 445 °F
Processing Temperature
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
Melt Temperature 221 - 229 °C
430 - 445 °F
Processing Temperature
Teknor Apex Telcar® TL-8431 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing;..
Melt Temperature 221 - 271 °C
430 - 520 °F
Melt temperatures above 530°F are not recommended, and may result in color shifts and or thermal instability.
Diamond Polymers ASA M-523
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Melt Temperature 221 - 271 °C
430 - 520 °F
Melt temperatures above 530°F are not recommended, and may result in color shifts and or thermal instability.
Diamond Polymers ASA TW-18B2
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc.
Melt Temperature 221 - 271 °C
430 - 520 °F
Melt temperatures above 530°F are not recommended, and may result in color shifts and or thermal instability.
Diamond Polymers ASA TW-23V
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Melt Temperature 221 °C
430 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B901 (UV Inhibitor Added), 13% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Melt Temperature 221 °C
430 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 13% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Melt Temperature 221 - 243 °C
430 - 469 °F
Ineos Nova Zyntar® 707 High Performance Flame Retardant Polystyrene  (discontinued **)
Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo..
Melt Temperature 221 °C
430 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 13% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..