Polymer Property : Melt Temperature = 235 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Melt Temperature 235 °C
455 °F
Multibase TPSiV™ 1180-50D Thermoplastic Silicone Vulcanizate
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced..
Melt Temperature 235 - 260 °C
455 - 500 °F
Injection Molding
DuPont Performance Polymers Crastin® SK612SF NC010 PBT  (Unverified Data**)
Crastin® SK612SF is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc..
Melt Temperature 235 - 260 °C
455 - 500 °F
Injection Molding
DuPont Performance Polymers Crastin® SK615SF NC010 PBT  (Unverified Data**)
Crastin® SK615SF is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc..
Melt Temperature 235 - 250 °C
455 - 482 °F
Extrusion
DuPont Performance Polymers Hytrel® 7246HS BK320 TPC-ET  (Unverified Data**)
Hytrel® 7246HS BK320 is a high modulus, heat stabilized, black grade with nominal hardness of 72D.Information provided by DuPont
Melt Temperature 235 - 260 °C
455 - 500 °F
Start Point: 245°C
Kingfa JH710 G10D Flame Retardant & 10% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:Exact mechanism partsElectrical and elect..
Melt Temperature 235 - 255 °C
455 - 491 °F
Start Point: 250°C
Kingfa PBT-G30 30% Glass Fiber Reinforced PBT
Features:Good size stabilityHigh mechanical propertiesHigh heat resistanceExcellent balance propertiesApplications:Injection moldingApplication partsAuto handleDoor latchE & E partsInformation Provi..
Melt Temperature 235 - 245 °C
455 - 473 °F
Injection Molding
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant
Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b..
Melt Temperature 235 - 265 °C
455 - 509 °F
Injection Molding
LG Chemical LUPOY GN5001RFT PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical..
Melt Temperature 235 - 265 °C
455 - 509 °F
Injection Molding
LG Chemical LUPOY GN5008HF PC/ABS, Halogen Free Flame Retardant, High Impact
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: E&E (OA, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid..
Melt Temperature 235 - 265 °C
455 - 509 °F
Injection Molding
LG Chemical LUPOY GP5106F PC/ABS+GF10%, Flame Retardance
Description: Injection Molding, PC/ABS+GF10%, Flame RetardanceApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical
Melt Temperature 235 - 265 °C
455 - 509 °F
Injection Molding
LG Chemical LUPOY GP5206F PC/ABS+GF20%, Flame Retardance
Description: Injection Molding, PC/ABS+GF20%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG..
Melt Temperature 235 - 265 °C
455 - 509 °F
Injection Molding
LG Chemical LUPOY ER5001RFA PC/ABS, Halogen Free, Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Melt Temperature 235 - 255 °C
455 - 491 °F
EBM
Eastman Tritan TX1800 Copolyester
Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGoo..
Melt Temperature <= 235 °C
<= 455 °F
CoExtrusion with EVA Processing
DuPont™ Bynel® 30E783 Anhydride Modified Ethylene Vinyl Acetate
BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melt Temperature 235 - 260 °C
455 - 500 °F
Injection Molding
DuPont Performance Polymers Crastin® SK612SF BK591 PBT
Crastin® SK612SF BK591 is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast ..
Melt Temperature 235 - 275 °C
455 - 527 °F
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, DAM
Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced ..
Melt Temperature 235 - 260 °C
455 - 500 °F
Start Point: 250°C
Kingfa JE2-R2G30 Glass Fiber Reinforced ABS/PBT Alloy
Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a..