| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 200 - 235 °C | 392 - 455 °F | |
|
SABIC F04660 High Density Polyethylene for Blown Film Applications
Product Description: F04660 is a homopolymer HDPE film grade with excellent processability and high stiffness. It has good moisture barrier properties and can be blended with LDPE and LLDPE to imp..
|
|||
| Melt Temperature | 179 - 235 °C | 354 - 455 °F | |
|
PolyOne Dynaflex™ G2730 Thermoplastic Elastomer (TPE)
Dynaflex™ G2730 is a soft, easy processing compound. - Excellent Weatherability - High Resilience - Soft, Rubbery FeelColor concentrates with polypropylene, ethylene vinyl acetate, or low density p..
|
|||
| Melt Temperature | 225 - 235 °C | 437 - 455 °F | Blow Molding |
|
DuPont Performance Polymers Hytrel® HTR8730 BK320 TPC-ET
(Unverified Data**)
Hytrel® HTR8730 BK320 is a high viscosity thermoplastic polyester elastomer designed for blow molding. It has excellent mechanical properties at elevated temperatures and very good resistance to mo..
|
|||
| Melt Temperature | 225 - 235 °C | 437 - 455 °F | Extrusion |
|
DuPont Performance Polymers Hytrel® HTR8730 BK320 TPC-ET
(Unverified Data**)
Hytrel® HTR8730 BK320 is a high viscosity thermoplastic polyester elastomer designed for blow molding. It has excellent mechanical properties at elevated temperatures and very good resistance to mo..
|
|||
| Melt Temperature | 165 - 235 °C | 329 - 455 °F | |
|
M. Holland Company MAGMA® LM372-A LLDPE
(discontinued **)
Features: High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessProcessing Method: Injection MoldingInformation provided by M. Holland.
|
|||
| Melt Temperature | 205 - 235 °C | 401 - 455 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 3038D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Melt Temperature | 205 - 235 °C | 401 - 455 °F | Extrusion Molding |
|
LG Chemical KEYFLEX BT 3038D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Melt Temperature | 220 - 235 °C | 428 - 455 °F | Recommended for Injection |
|
Kolon DIAMAT® EG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
|
|||
| Melt Temperature | 220 - 235 °C | 428 - 455 °F | Recommended for Injection |
|
Kolon DIAMAT® EH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
|
|||
| Melt Temperature | 220 - 235 °C | 428 - 455 °F | Recommended for Injection |
|
Kolon DIAMAT® EM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
|
|||
| Melt Temperature | 220 - 235 °C | 428 - 455 °F | Recommended for Injection |
|
Kolon DIAMAT® GP
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
|
|||
| Melt Temperature | 220 - 235 °C | 428 - 455 °F | Recommended for Injection |
|
Kolon DIAMAT® IM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
|
|||
| Melt Temperature | 220 - 235 °C | 428 - 455 °F | |
|
Lavergne VYTEEN ABS 2904 Acrylonitrile Butadiene Styrene
Vyteen ABS 2904 is a black recycled ABS high impact flow terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Excellent resilience -Good proc..
|
|||
| Melt Temperature | 225 - 235 °C | 437 - 455 °F | |
|
Borealis Borcoat™ BB700E-7032 Polypropylene Compound for Steel Pipe Coating Applications
Borcoat BB700E-7032 is a grey colored high impact polypropylene. This product is especially designed for direct extrusion of syntactic PP with high thermal insulations capacity and high compression..
|
|||
| Melt Temperature | 225 - 235 °C | 437 - 455 °F | |
|
Covestro Desmopan® 481 Polyurethane
injection molding gradefree from plasticizersgrease and oil-resistantlow compression sethigh elasticitygood heat resistanceEasy releaseApplicationRoller coatingSealsmembranesAutomotive engineeringPr..
|
|||
| Melt Temperature | 215 - 235 °C | 419 - 455 °F | |
|
Covestro Desmopan® DP 3660DU Polyurethane
Extrusion- and injection molding gradetransparent up to 6 mm wall thicknesshydrolysis-stabilisedwith special UV stabilizerswith release agentgood wear resistanceApplicationSports shoe solesHosesnon-..
|
|||
| Melt Temperature | 210 - 235 °C | 410 - 455 °F | Extrusion Coating |
|
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate
Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a ..
|
|||
| Melt Temperature | 185 - 235 °C | 365 - 455 °F | Cast Film/Sheet Processing |
|
DuPont™ Appeel® 72D811 Sealing Resin
DuPont™ Appeel® 72D811 resin is designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDPE, LDPE, EVA, and Ion..
|
|||
| Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
|
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail..
|
|||
| Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
|
DuPont™ Bynel® 4140 Anhydride Modified LLDPE
BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi..
|
|||
| Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
|
DuPont™ Bynel® 41E755 Anhydride Modified LLDPE
BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi..
|
|||
| Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
|
DuPont™ Bynel® 41E762 Anhydride Modified LLDPE
BYNEL® 41E762 is an anhydride-modified, linear low-density polyethylene (LLDPE) resin. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextru..
|
|||
| Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
|
DuPont™ Bynel® 41E850 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
|
|||
| Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
|
DuPont™ Bynel® 50E725 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
|
|||
| Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
|
DuPont™ Bynel® 50E739 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
|
|||
| Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
|
DuPont™ Bynel® 50E803 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
|
|||
| Melt Temperature | 160 - 235 °C | 320 - 455 °F | Extrusion Coating |
|
DuPont™ Elvaloy® AC34035 Ethylene Methyl Acrylate
Elvaloy® AC 34035 is a copolymer of ethylene and butyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® A..
|
|||
| Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
|
DuPont™ Bynel® 41E766 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
|
|||
| Melt Temperature | 180 - 235 °C | 356 - 455 °F | Injection Molding |
|
BASF Styroclear GH 58 SBC