| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 235 - 245 °C | 455 - 473 °F | |
|
Polyplastic Armamid® PA 6-1FR Nylon 6, Flame Retardant
Halogen and phosphor freeInformation provided by PolyPlastic Group.
|
|||
| Melt Temperature | 205 - 245 °C | 401 - 473 °F | |
|
Huntsman Rexell® V8801 Cast Film Extrusion LLDPE
(discontinued **)
Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and..
|
|||
| Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
|
Kingfa FRHIPS-117 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica..
|
|||
| Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
|
Kingfa FRHIPS-702 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing..
|
|||
| Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
|
Kingfa FRHIPS-980 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance properties, Non-DPOExcellent heat stability & electrical propertyColor tailor-made for clientApplications:Injection moldingGas assistant mold..
|
|||
| Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
|
Kingfa HP-126 Modified ABS
Features:UL94 HB @ 1.6-3.0mmHigh impact resistanceHigh flowApplications:LCD cabinetLarge thin-wall partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Melt Temperature | 215 - 245 °C | 419 - 473 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 3047D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Melt Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
|
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance
Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical
|
|||
| Melt Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
|
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose
Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical
|
|||
| Melt Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
|
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose
Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical
|
|||
| Melt Temperature | 235 - 245 °C | 455 - 473 °F | |
|
LG Chemical Lupox® SV-1120 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
|
|||
| Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
|
Kingfa FRHIPS-8002 Flame Retardant Polystyrene
Features:UL 94 V-2 @ 1.0mm, V-2 @ 3.2mmExcellent balancing properties, Non-DPOExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElec..
|
|||
| Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
|
Kingfa FRHIPS-930 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6mm, 5VA @ 2.6mmNon-DPO, high UV stabilityExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingPrinter, photocopier, fax machineElec..
|
|||
| Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
|
Kingfa FRHIPSV-0 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingTV or aud..
|
|||
| Melt Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
|
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose
Feature: Injection Molding, ABS+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical
|
|||
| Melt Temperature | 230 - 245 °C | 446 - 473 °F | |
|
LATI Latilub 75/4-20T PBT, PTFE Filled
Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria ..
|
|||
| Melt Temperature | 220 - 245 °C | 428 - 473 °F | |
|
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin
ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li..
|
|||
| Melt Temperature | 210 - 245 °C | 410 - 473 °F | Extrusion |
|
Total XSene® 4206 B High Density Polyethylene - Steel Pipe Coating
HDPE 4206 B is a high performance black compound primarily intended for steel pipe coating applications.Key characteristics areSuperior mechanical properties under stress cracking as well as under i..
|
|||
| Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
|
BASF Ultramid® HFX 35 PA6 (Dry)
Description: Ultramid HFX 35 is a polyamide specialty extrusion resin combining high flexibility, outstanding chemical resistance and enhanced heat stability.Applications: Ultramid HFX 35 is recomme..
|
|||
| Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
|
Beijing Ranger Chem PBT 403 M-G10 HF Halogen Free Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
|
Beijing Ranger Chem PBT-201-G10 202 Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
|
Beijing Ranger Chem PBT-201-G10 272 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
|
Beijing Ranger Chem PBT-MFC-G0 FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
|
Beijing Ranger Chem PBT-201-G10 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Melt Temperature | 205 - 245 °C | 401 - 473 °F | |
|
Huntsman Rexell® L8102 Cast Film Extrusion LLDPE
(discontinued **)
Linear-low density copolymer with high slip and medium antiblock, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.A..
|
|||
| Melt Temperature | 205 - 245 °C | 401 - 473 °F | |
|
Huntsman Rexell® L8408 Cast Film Extrusion LLDPE
(discontinued **)
Linear-low density copolymer, high quality blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength optics, and very low gel levels.Applications: Seali..
|
|||
| Melt Temperature | 205 - 245 °C | 401 - 473 °F | |
|
Huntsman Rexell® V8403 Cast Film Extrusion LLDPE
(discontinued **)
Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and..
|
|||
| Melt Temperature | 230 - 245 °C | 446 - 473 °F | |
|
LATI Later 4 PBT
Polybutylene Terephthalate (PBT). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
|
|||
| Melt Temperature | 230 - 245 °C | 446 - 473 °F | |
|
LATI Later 4E61 PBT