| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
|
Plastcom SLOVAMID 6 GF 20 PA6, 20% glass beads
FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti..
|
|||
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
|
Plastcom SLOVAMID 6 GF 30 FRA 3 PA6, 30% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 850°C,..
|
|||
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
|
Plastcom SLOVAMID 6 GF 5 FRA 5 Polyamide 6, 5% Glass Fiber, Halogen Flame Retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 5% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C, ..
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Plastcom SLOVAMID® 6 GF 35 LS PA6 reinforced with glass fiber, UV stabilized
PA 6 for injection molding, reinforced with 35% glass fiber, UV stabilized, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools..
|
|||
| Melt Temperature | 260 - 270 °C | 500 - 518 °F | |
|
Polyplastic Armamid® PA GF50-1 Nylon 6, 50% Glass Fiber
High stiffnessInformation provided by PolyPlastic Group.
|
|||
| Melt Temperature | 260 - 270 °C | 500 - 518 °F | |
|
DuPont Performance Polymers Crastin® SK609 BK851 PBT
(Unverified Data**)
Crastin® SK609 BK851 is a 50% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
|
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre, 20% glass beads
FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre and 20% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri..
|
|||
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
|
Plastcom SLOVAMID 6 GF 15 MI/2 PA6, 15% glass fibre, improved strength
FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..
|
|||
| Melt Temperature | 260 - 270 °C | 500 - 518 °F | Cast Film |
|
Honeywell Aegis™ H205QP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H205QP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500. It possesses the combination..
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
|
LG Chemical LUMID GP1200A(W) PA6, Medium Viscosity
Feature: Injection Molding, PA6, Medium ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical
|
|||
| Melt Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
|
LG Chemical Lupox® TE5000HZ PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Door Handle)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical
|
|||
| Melt Temperature | 230 - 270 °C | 446 - 518 °F | ISO 294 |
|
Styrolution Novodur® 4140PG ABS
Novodur Ultra 4140PG is a PC modified plating grade combining high heat resistance and excellent impact strength with the unique surface properties of a Novodur ABS material.Information provided by ..
|
|||
| Melt Temperature | 230 - 270 °C | 446 - 518 °F | ISO 294 |
|
Styrolution Novodur® HH-112 ABS
Novodur HH-112 is a high heat injection molding grade. It provides good heat resistance combined with enhanced stiffness.Information provided by Styrolution
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
|
Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Conditioned)
Description: Terblend® N NG-02 EF is a glass fiber reinforced UV stabilized ABS/PA blend with excellent dimensional stability and high impact strength. The enhanced flowability enables excellent ..
|
|||
| Melt Temperature | 255 - 270 °C | 491 - 518 °F | |
|
Toyobo VYLOPET® EMC333 Injection Molding Polyester Resin, Hydrolysis Resistant
Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo.
|
|||
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
|
Eastman Drystar 0601 Copolyester, Injection Molded
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
|
|||
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
|
Covestro Makroblend® KU 2-7912 MBS151 Polycarbonate + PBT, Impact Grade
(PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedAs of 1 September 2015, Bayer MaterialScience was separated..
|
|||
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
|
CP-Polymer-Technik Wellamid® 6000 GS 40 HWCP 40% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Eurostar Staramide BG10HU PA6, 50% Glass Fiber Filled, UV and Heat Stabilized, Injection Molded
Staramide BG10HU is an UV and Heat Stabilized, 50% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded
Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Eurostar Staramide PF006S PA6, 30% Glass Fiber Filled, Injection Molded
Staramide PF006S is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Eurostar Staramide PFB42EU PA6, Glass Fiber/Bead Filled, Injection Molded
Starflam PFB42EU is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
|
Eurostar Starflam PF0023E PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PF0023E is a Mineral Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
|
Covestro Makroblend® KU 2-7912 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedPreprocessingMax. Water content
|
|||
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
|
Plastcom SLOVAMID 6 T 30 Polyamide 6, 30% Micronized Talc
FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin..
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Eurostar Staramide BG4 PA6, 20% Glass Filled, Injection Molded
BG4 is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||