| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
|
PolyOne Gravi-Tech™ GRV-NY-085-W-NAT Polyamide 6 (Nylon 6)
Information provided by PolyOne
|
|||
| Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
|
PlastiComp Complet® LGF40 - PA6 Nylon 6, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
|
|||
| Melt Temperature | 271 - 299 °C | 520 - 570 °F | |
|
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled
PC/ABS Alloy, General Purpose, 10% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi..
|
|||
| Melt Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant
Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec..
|
|||
| Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
|
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate
Information provided by Ravago.
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
PTS Trimid® N66-100L Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
PTS Trimid® N66-G13L 13% Glass Fiber Reinforced Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
PTS Trimid® N66-G33HL 33% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
PTS Trimid® N66-G43L 43% Glass Fiber Reinforced Lubricated Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
|
PlastiComp Complet® LCF40 - PA6 Nylon 6, 40% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Ravago Manufacturing Americas Hylon® N1000EHL Nylon 6/6 (Cond)
(discontinued **)
Information provided by Ravago
|
|||
| Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
|
Ravago Manufacturing Americas Hylon® N1025HLFR Nylon 6/6, 25% Fiberglass, Heat Stabilized, Lubricated, Flame retardant (Cond)
Information provided by Ravago.
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled
Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc.
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
MRC Polymers NAXELLâ„¢ PC210MR General Purpose Polycarbonate, Medium MFR, with Release
Medium melt without impact modificationMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedGenerally for black and gray colors onlyFR package ..
|
|||
| Melt Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Wellman Wellamid® 22L-N Unfilled Nylon 66, Lubricated
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
|
|||
| Melt Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Wellman Wellamid® 22LN2-N Unfilled Nylon 66, Lubricated & Nucleated
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Wellman Wellamid® MR340 42H-N 34% Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Melt Temperature | 271 - 299 °C | 520 - 570 °F | |
|
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Melt Temperature | 271 - 299 °C | 520 - 570 °F | |
|
Clariant Renol PA111G50 Nylon 66, 50% Glass Fiber
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Clariant Renol PC010-L FR Polycarbonate, Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 271 - 299 °C | 520 - 570 °F | |
|
Clariant Renol R66G13HSL Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Economy
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Clariant Renol 6642 2% Moly Nylon 66, Extrusion Grade, 2% Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Clariant Renol PA121 Nylon 66, Impact Modified
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 271 °C | 520 °F | |
|
Chem Polymer Chemlon 100 W Nylon 66, MoS2 Filled
A molybdenum disulfide modified nylon 66 exhibiting superior tensile strength and wear resistance, greater dimensional stability and higher heat resistance than general purpose nylon 66.Data provide..
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 559 °F | Stock |
|
PolyOne Edgetek® NI-30CF/000 Nylon 6/10 - 30% Carbon Fiber Reinforced
(discontinued **)
Data provided by PolyOne.
|
|||
| Melt Temperature | 271 - 410 °C | 520 - 770 °F | Average value: 352 °C Grade Count:9 |
|
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..
|
|||