| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 250 - 280 °C | 482 - 536 °F | |
|
Plastcom SLOVAMID 6 GF 30 006/1M PA6 reinforced with 30% glass fibre
Features: PA 6 for injection moulding, chemically strengthened with 30% of milled glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and cons..
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
|
Plastcom SLOVAMID® 6/66 FRC 3 TS PA6/66 flame retarded, heat stabilized
PA 6 + PA 66 alloy for injection molding, reinforced with 30 % glass fiber, flame retarded with non halogen flame retardant, heat stabilized. Main features: flammability in accordance with UL 94 5 a..
|
|||
| Melt Temperature | 250 - 280 °C | 482 - 536 °F | |
|
Plastcom SLOVASTER® B GF 50 PBT, 50% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 50% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
|
Polykemi AB POLYblend 65V PC/ABS-Blend, Flame Retardant
Information provided by Polykemi AB
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | Do not melt above 300°C |
|
Nilit Nilamid B3 H ZC Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
|
PolyOne Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66)
These products contain flame retardants which are activated by longer residence times in the cylinder and then can decompose. At interruption of the moulding cycle (approx. >5 min) it is recommended..
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | Do not melt above 300°C |
|
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu..
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | Average value: 260 °C Grade Count:21 |
|
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
|
|||
| Melt Temperature | 180 - 280 °C | 356 - 536 °F | Molding |
|
Ineos Styrenics Avantra® 585K Rubber Modified Polystyrene
Avantra® 585K is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical impact strength. Although Avantra® 585K can be processed by any method applicable..
|
|||
| Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
|
Gromax BFM30-EL04B2 Nylon 6 30% Mineral Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
|
Gromax BFM40-DL04N1 Nylon 6 40% Mineral Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
|
Lanxess Pocan® A 3121 901510 PBT+ASA, 20% Glass Fiber
PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS.
|
|||
| Melt Temperature | 270 - 280 °C | 518 - 536 °F | |
|
LATI Latamid 66 B G/20-V PA 66, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. High fluidity. Glass fibers. Flame retardant, non classifiable, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific;..
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
|
Styron EMERGEâ„¢ 7560 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ PC/ABS 7560 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the..
|
|||
| Melt Temperature | 250 - 280 °C | 482 - 536 °F | |
|
Toyobo GLAMIDE® T-402FR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
|
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
|
Covestro Makroblend® DP 7665 Polycarbonate + PET, Mineral Filled Impact Grade
Developmental productISO 7792-1-PC/PET,MHPR,-030,MD20(PC+PET)-blendsimpact modifiedInjection molding grade 20 % mineral filledPreprocessingMax. Water content
|
|||
| Melt Temperature | 250 - 280 °C | 482 - 536 °F | |
|
CP-Polymer-Technik Wellamid® 6000 GV 25 HWUVCP 25% Glass Fiber Nylon 6, UV Stabilized, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Melt Temperature | 250 - 280 °C | 482 - 536 °F | |
|
CP-Polymer-Technik Wellamid® 6000 GV 35 HWCP 35% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
|
CP-Polymer-Technik Wellamid® 6600/506 HWCP Nylon 66, Impact Modified, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
|
CP-Polymer-Technik Wellamid® 6600/508 HWUVCP Nylon 66, Impact Modified, UV Stabilized, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Melt Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Eurostar Star L PA66 30Y D51 PA66, Carbon Fiber Filled, Injection Molded
Star L PA66 30Y D51 is a PTFE Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Eurostar Star L PA66 D91 PA66, Aramid Fiber Filled, Injection Molded
Star L PA66 D91 is a PTFE lubricated, Aramid Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Eurostar Staramide RX06027 PA66, 30% Glass Filled, Injection Molded
Staramide RX06027 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S34/8)Information provided by Eurostar.
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
|
Eurostar Staramide ALY540A PA66, Glass/Mineral Fiber Reinforced, Injection Molding
Staramide ALY540A is a Glass Fiber Reinforced, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 250 - 280 °C | 482 - 536 °F | Injection-molding |
|
BASF Ultradur® S 4090 GX 14% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab..
|
|||
| Melt Temperature | 225 - 280 °C | 437 - 536 °F | |
|
Beijing Ranger Chem PBT 403 G-M50 Heat Resistant and Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | DAM; Injection Molding |
|
DuPont Performance Polymers Zytel® FG7301 NC010 Nylon 6
(Unverified Data**)
Zytel® FG7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications. It has been developed for consideration into applications such as parts for the food industry.In..
|
|||
| Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
|
Gromax CFG33-RN13N1 Nylon 6 33% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
|
|||