| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 282 - 310 °C | 540 - 590 °F | |
|
PolyOne Stat-Tech™ NN-30CF/000 Black Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
|
|||
| Melt Temperature | 282 - 304 °C | 540 - 579 °F | |
|
PolyOne Stat-Tech™ PC-15CF/000 Black Polycarbonate (PC)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
|
|||
| Melt Temperature | 282 - 310 °C | 540 - 590 °F | |
|
PolyOne Trilliant™ HC HC6600-0010 ESD Black Polyamide 66 (Nylon 66)
Information provided by PolyOne
|
|||
| Melt Temperature | 282 - 321 °C | 540 - 610 °F | |
|
Oxford Polymers Oxtron PPS-XT-40GF PPS, 40% Glass Reinforced
Product Description: Glass Fiber (40% Reinforced), Polyphenylene sulfide injection molding grade based alloy. Processing and Delivery Form: Pellets and Injection MoldingAppearance: Natural off-whit..
|
|||
| Melt Temperature | 282 - 321 °C | 540 - 610 °F | |
|
Oxford Polymers PPS/66-505-40GF-BK PPS/PA66, 40% Glass Fiber Reinforced
Product Description: Glass Fiber (40% Reinforced), Polyphenylene sulfide injection molding grade based alloy with Nylon 66 Processing and Delivery Form: Pellets and Injection MoldingAppearance: Bla..
|
|||
| Melt Temperature | 282 - 310 °C | 540 - 590 °F | |
|
Polymer Resources PC-FR3-D-[color]-3 Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
|
|||
| Melt Temperature | 282 - 316 °C | 540 - 600 °F | |
|
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Melt Temperature | 282 - 316 °C | 540 - 600 °F | |
|
Polymer Resources PC-IM1 Polycarbonate, Impact Modified, Low Flow
Polycarbonate, Impact Modified, Low FlowProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided ..
|
|||
| Melt Temperature | 282 - 310 °C | 540 - 590 °F | |
|
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
|
|||
| Melt Temperature | 282 - 310 °C | 540 - 590 °F | |
|
Polymer Resources PPX-GP2 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
|
Ravago Manufacturing Americas Hylon® N1033STL Nylon 6/6 (DAM)
Information provided by Ravago.
|
|||
| Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
|
Ravago Manufacturing Americas Hylon® N1040MHL Nylon 6/6 (DAM)
Information provided by Ravago.
|
|||
| Melt Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Ravago Manufacturing Americas Hylon® N1043HL Nylon 6/6 (Cond)
Information provided by Ravago.
|
|||
| Melt Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Ravago Manufacturing Americas Hylon® N1043HL Nylon 6/6 (DAM)
Information provided by Ravago.
|
|||
| Melt Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Ravago Manufacturing Americas Hylon® N1043L Nylon 6/6 (DAM)
Information provided by Ravago.
|
|||
| Melt Temperature | 282 - 304 °C | 540 - 580 °F | |
|
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
|
PolyOne Edgetek® NN-20CF/000 BLACK Polyamide 66 (Nylon 66)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
|
PolyOne Edgetek® NN-50GF/000 Polyamide 66 (Nylon 66)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| Melt Temperature | 282 - 304 °C | 540 - 580 °F | |
|
PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
|
Ravago Manufacturing Americas Hylon® N1013L Nylon 6/6 (Cond)
(discontinued **)
Information provided by Ravago.
|
|||
| Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
|
Ravago Manufacturing Americas Hylon® N1033TL Nylon 6/6 (Cond)
(discontinued **)
Information provided by Ravago.
|
|||
| Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
|
Ravago Manufacturing Americas Hylon® N1035HHR Nylon 6/6, 35% Fiberglass (DAM)
(discontinued **)
Information provided by Ravago.
|
|||
| Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
|
Ravago Manufacturing Americas Hylon® N1040MGL Nylon 6/6 (DAM)
(discontinued **)
Information provided by Ravago.
|
|||
| Melt Temperature | 282 - 343 °C | 540 - 650 °F | Average value: 315 °C Grade Count:32 |
|
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum..
|
|||
| Melt Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Wellman EcoLon® 2000-BK1 37% Post Consumer Compound Nylon 66
Description: Post Consumer Compound Nylon 66Information provided by Wellman.
|
|||
| Melt Temperature | 282 - 293 °C | 540 - 560 °F | |
|
Wellman EcoLon® MRGF1518-BK Mineral/Glass Fiber Reinforced Nylon 66, Lubricated, Heat Stabilized, PCR
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Melt Temperature | 282 - 293 °C | 540 - 560 °F | |
|
Wellman Wellamid® MRGF3822-BK 38% Mineral/10% Glass Fiber Reinforced Nylon 66, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Melt Temperature | 282 - 316 °C | 540 - 600 °F | Molding |
|
PolyOne Lubri-Tech™ MP-20GF/05T Modified Polyphenylene Oxide (mPPO), Glass Filled, PTFE Lubricated
(discontin
Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||