| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 20.0 - 285 °C | 68.0 - 545 °F | Average value: 236 °C Grade Count:18 |
|
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
|
|||
| Melt Temperature | 232 - 285 °C | 450 - 545 °F | Average value: 263 °C Grade Count:8 |
|
Overview of materials for Nylon 612 with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app..
|
|||
| Melt Temperature | 255 - 285 °C | 491 - 545 °F | Start Point: 265°C |
|
Kingfa PA6-G50 50% Glass Fiber Reinforced PA6
Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t..
|
|||
| Melt Temperature | 255 - 285 °C | 491 - 545 °F | Injection Molding |
|
LG Chemical LUMID LW4403A(W) PA66+GF/MF40%, Low Warpage
Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Melt Temperature | 265 - 285 °C | 509 - 545 °F | |
|
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber
PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS.
|
|||
| Melt Temperature | 255 - 285 °C | 491 - 545 °F | Start Point: 265°C |
|
Kingfa CPA-6 Toughened PA6
Features:High impactLow tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Melt Temperature | 250 - 285 °C | 482 - 545 °F | Start Point: 275°C |
|
Kingfa PC-WT01 Weather Resistance PC
Features:Excellent balance propertiesGood weather resistanceHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElec..
|
|||
| Melt Temperature | 245 - 285 °C | 473 - 545 °F | |
|
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Melt Temperature | 245 - 285 °C | 473 - 545 °F | |
|
Toyobo GLAMIDE® NB-1700 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Melt Temperature | 235 - 285 °C | 455 - 545 °F | Extrusion Coating |
|
DuPont™ Appeel® 20D855 Ethylene Acrylate
DuPont™ Appeel 20D855 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe..
|
|||
| Melt Temperature | 185 - 285 °C | 365 - 545 °F | |
|
DuPont™ Surlyn® 9320 Zinc Ionomer
Surlyn® 9320 is a zinc ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 9320 thermoplastic resin ..
|
|||
| Melt Temperature | 270 - 285 °C | 518 - 545 °F | |
|
Eurostar Starflam AF430B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR430B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 270 - 285 °C | 518 - 545 °F | |
|
Eurostar Starflam AFR450B PA66, 25% Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR450B is a Flame Retardant, 25% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 275 - 285 °C | 527 - 545 °F | |
|
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded
AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su..
|
|||
| Melt Temperature | 185 - 285 °C | 365 - 545 °F | Extrusion Coating |
|
DuPont™ Surlyn® 6320 Magnesium Ionomer
Surlyn® 6320 is a magnesium ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 6320 thermoplastic r..
|
|||
| Melt Temperature | 270 - 285 °C | 518 - 545 °F | |
|
Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 240 - 285 °C | 464 - 545 °F | |
|
BASF Ultramid® BG50XFI PA6 (Conditioned)
Description: Ultramid BG50XFI is an impact modified, injection molding type 6 nylon graft copolymer with superior impact resistance and flow especially for thinner walled parts and long flow lengths..
|
|||
| Melt Temperature | 255 - 285 °C | 491 - 545 °F | Injection Molding |
|
LG Chemical LUMID LW4009A(W) PA6+GF/MF40%, Low Warpage
Feature: Injection Molding, PA6+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical
|
|||