| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 271 - 293 °C | 520 - 559 °F | |
|
PolyOne Nymax™ GF 924 33 UV Black 108 Polyamide 66 (Nylon 66)
Property data for molded test bars: Dry as MoldedInformation provided by PolyOne
|
|||
| Melt Temperature | 277 - 293 °C | 530 - 560 °F | |
|
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized
General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade..
|
|||
| Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
|
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release
Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced
Information provided by Ravago.
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Ravago Manufacturing Americas Hylon® N1000HL Nylon 6/6
Available in North America Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and Lubricated RoHS Compliant Auto Specifications: FORD WSK-M4D648-A Color: Black Form: Pellets Processi..
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Ravago Manufacturing Americas Hylon® N1000NL2 Nylon 6/6 (Cond)
Information provided by Ravago.
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
PTS Trimid® N66-G13HL 13% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
PTS Trimid® N66-G43L 43% Glass Fiber Reinforced Lubricated Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Temperature | 277 - 293 °C | 530 - 560 °F | |
|
Polymer Resources NY66-IM2 Impact Modified Nylon 66
Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are ..
|
|||
| Melt Temperature | 277 - 293 °C | 530 - 560 °F | |
|
Polymer Resources NY66-MD2 Nylon 66, 2% MoS2
Nylon 66, 2% Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
|
|||
| Melt Temperature | 277 - 293 °C | 530 - 560 °F | |
|
PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Ravago Manufacturing Americas Hylon® N1000NL2 Nylon 6/6 (DAM)
Information provided by Ravago.
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Ravago Manufacturing Americas Hylon® N1000EHL Nylon 6/6 (DAM)
(discontinued **)
Information provided by Ravago.
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Ravago Manufacturing Americas Hylon® N1000NL Nylon 6/6 (Cond)
(discontinued **)
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Melt Temperature | 277 - 293 °C | 530 - 560 °F | |
|
Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6
(discontinued **)
Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat StabilizedRoHS CompliantAuto Specifications: GM GMP.PA66.074 Color: BlackF..
|
|||
| Melt Temperature | 277 - 293 °C | 530 - 560 °F | |
|
Ravago Manufacturing Americas Hylon® N1000TL Nylon 6/6 (Cond)
(discontinued **)
Information provided by Ravago
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | Molding |
|
PolyOne Edgetek® NL-43GF/000 Nylon 6/12, Glass Filled
(discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
MRC Polymers NAXELLâ„¢ PC210MR General Purpose Polycarbonate, Medium MFR, with Release
Medium melt without impact modificationMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedGenerally for black and gray colors onlyFR package ..
|
|||
| Melt Temperature | 277 - 293 °C | 530 - 560 °F | |
|
Samyang Trirex® PC-3025U 12 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Temperature | 277 - 293 °C | 531 - 559 °F | |
|
Styron EMERGEâ„¢ 4530-15 Polycarbonate
EMERGEâ„¢ PC 4530-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co..
|
|||
| Melt Temperature | 227 - 293 °C | 440 - 560 °F | |
|
Wellman Wellamid® 42LH XE-N Unfilled Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc.
|
|||
| Melt Temperature | 277 - 293 °C | 531 - 559 °F | |
|
Eastman Eastar MN058 Copolyester
Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN058 Copolyester is a medical gra..
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Clariant Renol PA111 Nylon 66, General Purpose
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
|
Clariant Renol PA133G33 Nylon 66, 33% Glass Fiber, Highly Impact Modified
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Clariant Renol PA2SP0024 Nylon 6, Flame Retardant, Static Dissipative
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Clariant Renol PA121 Nylon 66, Impact Modified
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Clariant Renol 66G33-L Nylon 66, 33% Glass Fiber Reinforced, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 271 - 293 °C | 520 - 559 °F | Stock |
|
PolyOne Edgetek® NI-40CF/000 Nylon 6/10 - 40% Carbon Fiber Reinforced
(discontinued **)
Data provided by PolyOne.
|
|||