| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 299 - 316 °C | 570 - 601 °F | |
|
PolyOne Stat-Tech™ LC-20NCF/000 V3 Natural Liquid Crystal Polymer (LCP)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
|
|||
| Melt Temperature | 299 - 310 °C | 570 - 590 °F | |
|
LNP Thermocomp® UF-1006 FR HS LEX BK8-115 Polyphthalamide, Glass Fiber Reinforcement
(discontinued **)
Features: Heat Stabilized, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L..
|
|||
| Melt Temperature | 299 - 327 °C | 570 - 621 °F | Excellent Processability |
|
Chevron Phillips 1025 Extrusion Coating Resin
(discontinued **)
Resin Type: Speed Resin, Base Resin Type - Chevron PE1017Characteristics: Excellent Processability at 570-620°F (300-325°C) Melt, Good Adhesion at Low Coating Weights and High Speed Lines, Low COF..
|
|||
| Melt Temperature | 299 - 327 °C | 570 - 621 °F | Excellent Processability |
|
Chevron Phillips 1028 Extrusion Coating Resin
(discontinued **)
Resin Type: High Speed Slip ResinCharacteristics: Excellent Processability at 570-620°F (300-325°C) Melt, Good Adhesion at Low Coating Weights and High Speed Lines, Low COF uses, FDA Approved for ..
|
|||
| Melt Temperature | 299 - 371 °C | 570 - 700 °F | Average value: 327 °C Grade Count:13 |
|
Overview of materials for Polycarbonate, High Heat
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro..
|
|||
| Melt Temperature | 299 - 330 °C | 570 - 626 °F | Average value: 308 °C Grade Count:6 |
|
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..
|
|||
| Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
|
PolyOne Lubri-Tech™ SF-25GF/13T BLACK Polyphenylene Sulfide (PPS), Glass Filled, PTFE Lubricated
(discontinue
Description/Features:Glass Fiber ReinforcedPTFE LubricatedBlackPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
|
PolyOne Lubri-Tech™ SF-25GF/13T-2S Polyphenylene Sulfide (PPS), Glass Filled, PTFE/Silicone Lubricated
(disco
Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
|
PolyOne Edgetek® SF-30GF-25MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **)
Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
|
PolyOne Edgetek® SF-35GF-15MC/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **)
Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
|
PolyOne Edgetek® SF-35GF-25MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **)
Description/Features:Glass/Mineral ReinforcedUL 94 V0 (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
|
PolyOne Edgetek® SF-40GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
|
PolyOne Edgetek® SF-40GF-10 MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **)
Description/Features:Glass/Mineral ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Melt Temperature | 299 - 332 °C | 570 - 630 °F | |
|
PolyOne Edgetek® SF-40GF-25MN1/000 PPS (Polyphenylene Sulfide), 40% Glass Fiber and 25% Mineral Filled
(disco
Information provided by PolyOne™ Corporation
|
|||
| Melt Temperature | 299 - 327 °C | 570 - 621 °F | |
|
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, ..
|
|||
| Melt Temperature | 299 - 327 °C | 570 - 621 °F | |
|
Styron EMERGEâ„¢ 4510-6 Polycarbonate
EMERGEâ„¢ PC 4510-6 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Informa..
|
|||
| Melt Temperature | 299 - 327 °C | 570 - 621 °F | |
|
Styron EMERGEâ„¢ 4530-6 Polycarbonate
EMERGEâ„¢ PC 4510-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co..
|
|||
| Melt Temperature | 299 - 327 °C | 570 - 621 °F | |
|
Styron EMERGEâ„¢ 4800-7 Polycarbonate
EMERGEâ„¢ 4800-7 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polycar..
|
|||
| Melt Temperature | 299 - 327 °C | 570 - 620 °F | |
|
Chevron Phillips MarFlex® 1023 LDPE Extrusion Coating Resin
Resin Type: Base, SpeedCharacteristics: Good adhesion at low coating weights and high line speedsLow COF usesFDA approved for food contactApplications: Can be used in the outer coextrusion layer or ..
|
|||
| Melt Temperature | 299 - 321 °C | 570 - 610 °F | |
|
Clariant Renol PPSS0007 Polyphenylene Sulfide, Glass Fiber and Mineral Filled
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 299 - 321 °C | 570 - 610 °F | |
|
Clariant Renol PPSSP0001 Polyphenylene Sulfide, Glass Fiber and Bead Filled
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 299 - 321 °C | 570 - 610 °F | |
|
Clariant Renol PPSSP0006 Polyphenylene Sulfide, Glass Fiber, PTFE Lubricated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
|
PolyOne Edgetek® SF-35GF-25MN/000 L Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **)
Description/Features:Glass/Mineral ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||