| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Plastcom SLOVAMID 66 CF 20 Polyamide 66, 20% Carbon Fiber
FeaturesChemically reinforced with 20% carbon fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. ..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Plastcom SLOVAMID 66 GF 10 PA66, 10% glass fibre
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
|
|||
| Melt Temperature | 275 - 300 °C | 527 - 572 °F | Do not melt above 300°C |
|
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It ..
|
|||
| Melt Temperature | 275 - 300 °C | 527 - 572 °F | Do not melt above 300°C |
|
Nilit Nilamid A3 H7 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H7 G6 is a 30% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | DAM |
|
DuPont Performance Polymers Zytel® 74G33W NC010 Nylon 66
(Unverified Data**)
Zytel® 74G33W NC010 is a 33% glass reinforced nylon 66 and nylon 6 co-melt resin with improved weatherability.Information provided by DuPont Performance Polymers
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | DAM |
|
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66
(Unverified Data**)
Zytel® FE270038 is a 40% glass fiber/mineral reinforced, heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.Information provided by DuPont Performan..
|
|||
| Melt Temperature | 260 - 300 °C | 500 - 572 °F | |
|
LG Chemical LUPOY GP-5200 General Purpose PC/ABS Alloy, 10% Polymer Alloy, High Strength
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | ISO 294 |
|
Gromax BFG45-B100N1 Nylon 6 46% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | ISO 294 |
|
Gromax BFG45-B100N1 Nylon 6 46% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | ISO 294 |
|
Gromax BFG50-BN00N1 Nylon 6 60% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | Recommended |
|
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers
PA 66, 15% glass fibers, injection molding, heat-ageing stabilized
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
LG Chemical LUPOY GN-2006F Halogen Free Modified PC, Unreinforced, Weather Resistant, Flame Retardant, Green
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
LG Chemical LUPOY GP-1006F General Purpose Modified PC, Unreinforced, Weather Resistant, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Melt Temperature | 275 - 300 °C | 527 - 572 °F | |
|
LATI Latilub 66-01M G/30 PA66, 30% Glass Fiber Reinforced, Molybdenum disulphide Filled
Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
|
|||
| Melt Temperature | 270 - 300 °C | 518 - 572 °F | |
|
LATI Latilub 66-20ST PA66, Silicone/PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). Silicone / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
|
|||
| Melt Temperature | 265 - 300 °C | 509 - 572 °F | |
|
LATI Latilub 87/24UV-20T PC, PTFE Filled
Self-lubricating product based on Polycarbonate (PC). UV stabilized. PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri..
|
|||
| Melt Temperature | 265 - 300 °C | 509 - 572 °F | |
|
LATI Latiohm 87/28-07 CNT PC
Semiconductive/dissipative product based on Polycarbonate (PC). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
|
|||
| Melt Temperature | 275 - 300 °C | 527 - 572 °F | |
|
Lavergne VYPET VNT 615 PET 15% Glass Reinforced
Vypet VNT 615 is a 15% fiberglass reinforced PET injection molding compound designed for structural applications.Features: Easy, fast processing; Excellent strength and stiffness; Excellent dimensio..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET
Information provided by A. Schulman.
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Melt Temperature | 270 - 300 °C | 518 - 572 °F | |
|
E-Polymers TEKANATE® G7013 General Purpose Easy Molding Polycarbonate
Modified Poly Carbonate: TEKANATE is a modified PC by improving polycarbonate resins with features of halogen-free flammability, transparency, impact resistance and reinforced fiberglass. It shows ..
|
|||
| Melt Temperature | 260 - 300 °C | 500 - 572 °F | |
|
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Dry, 60% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Melt Temperature | 285 - 300 °C | 545 - 572 °F | |
|
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM
Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go..
|
|||
| Melt Temperature | 260 - 300 °C | 500 - 572 °F | |
|
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | DAM |
|
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**)
Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers
|
|||
| Melt Temperature | 240 - 300 °C | 464 - 572 °F | |
|
Premix Thermoplastics PRE-ELEC® PA 1411 Conductive Thermoplastic Compound
PRE-ELEC® PA 1411 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. PRE-ELEC® PA 1411 has a very low electrical resistivity. P..
|
|||
| Melt Temperature | 275 - 300 °C | 527 - 572 °F | |
|
LATI Latamid 66 H2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
|
|||
| Melt Temperature | 160 - 300 °C | 320 - 572 °F | Average value: 219 °C Grade Count:53 |
|
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..
|
|||
| Melt Temperature | 275 - 300 °C | 527 - 572 °F | |
|
LATI Latilub 66-20T G/40 PA66, 40% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri..
|
|||