| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 277 - 304 °C | 531 - 579 °F | |
|
PolyOne LubriOne™ NN-000/10T Polyamide 66 (Nylon 66)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Melt Temperature | 277 - 304 °C | 531 - 579 °F | |
|
PolyOne LubriOne™ NN-000/20T Polyamide 66 (Nylon 66)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Melt Temperature | 282 - 304 °C | 540 - 579 °F | |
|
PolyOne Stat-Tech™ PC-15CF/000 Black Polycarbonate (PC)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
|
|||
| Melt Temperature | 277 - 304 °C | 530 - 580 °F | |
|
Polymer Resources NY66-EX1 High Viscosity Nylon 66
Nylon 66, High Viscosity (RV 220 to 260)Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as ..
|
|||
| Melt Temperature | 285 - 304 °C | 545 - 580 °F | |
|
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced
Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
|
|||
| Melt Temperature | 288 - 304 °C | 550 - 580 °F | |
|
Polymer Resources NY66-IM1-G13 Nylon 66, 13% Glass Reinforced, Toughened
Nylon 66, 13% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g..
|
|||
| Melt Temperature | 288 - 304 °C | 550 - 580 °F | |
|
Polymer Resources NY66-M25G15 Nylon 66, 25% Mineral, 15% Glass Reinforced
Nylon 66, 25% Mineral, 15% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon gr..
|
|||
| Melt Temperature | 288 - 304 °C | 550 - 580 °F | |
|
Polymer Resources NY66-M25G15-[color]-H Nylon 66, 25% Mineral, 15% Glass Reinforced, Heat Stabilized
Nylon 66, 25% Mineral, 15% Glass Reinforced, Lubricated and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, te..
|
|||
| Melt Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant
Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec..
|
|||
| Melt Temperature | 288 - 304 °C | 550 - 580 °F | |
|
Polymer Resources NY6-M25G15 Nylon 6, 25% Mineral, 15% Glass Reinforced
Nylon 6, 25% Mineral, 15% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon gra..
|
|||
| Melt Temperature | 282 - 304 °C | 540 - 580 °F | |
|
PTS Tristar® PC-10FRNH-V 12 MFI Non-Bromine Non-Chlorine Flame Retardant UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
|
LTL Color Compounds ColorFast® NY2GF130 Nylon 66, 13% Glass-Filled
13% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc.
|
|||
| Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
|
LTL Color Compounds ColorFast® NY2GF131 Nylon 66, 13% Glass-Filled, Impact Modified
13% glass-filled impact modified nylon 6,6All information provided by LTL Color Compounders, Inc.
|
|||
| Melt Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Wellman Wellamid® 220-N Unfilled Nylon 66, Not Lubricated, Nucleated, or Heat Stabilized
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
|
|||
| Melt Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Wellman Wellamid® 22LHI3 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
|
|||
| Melt Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Wellman Wellamid® 22LH-N Unfilled Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
|
|||
| Melt Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Wellman Wellamid® 22LN2-N Unfilled Nylon 66, Lubricated & Nucleated
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
|
|||
| Melt Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Wellman Wellamid® GB1430-N 33% Glass Bubble Filled, Low Density Nylon 66
Description: Glass Bubble Filled, Low Density Nylon 66Information provided by Wellman.
|
|||
| Melt Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Wellman Wellamid® GFT13-66 XE-N 13% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
|
|||
| Melt Temperature | 277 - 304 °C | 530 - 580 °F | |
|
Wellman Wellamid® GS40-66 22L-N 40% Glass Sphere Filled Nylon 66, Lubricated
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
|
|||
| Melt Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Wellman Wellamid® XT1482-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
|
|||
| Melt Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Ravago Manufacturing Americas Hylon® N1043L Nylon 6/6 (Cond)
(discontinued **)
Information provided by Ravago.
|
|||
| Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
|
Polymer Resources PPX/NY G30 Modified PPO, 30% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
|
LTL Color Compounds ColorFast® NY1GF130 Nylon 6, 13% Glass-Filled
13% glass-filled nylon 6All information provided by LTL Color Compounders, Inc.
|
|||