| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 302 - 329 °C | 575 - 625 °F | |
|
Polymer Resources PC-G10-IM Polycarbonate, 10% Glass Reinforced, Impact Modified
Polycarbonate, 10% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
|
|||
| Melt Temperature | 302 - 329 °C | 575 - 625 °F | |
|
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
|
|||
| Melt Temperature | 316 - 329 °C | 600 - 625 °F | Molding |
|
PolyOne Therma-Tech™ SFC-5000 TC Polyphenylene Sulfide (PPS)
(discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
|
|||
| Melt Temperature | 321 - 329 °C | 610 - 624 °F | |
|
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet..
|
|||
| Melt Temperature | 302 - 329 °C | 575 - 625 °F | |
|
Westlake EC483 Low Density Polyethylene
WESTLAKE low-density polyethylene EC483 is recommended for use in the boardstock coating industry. This resin has low neck-in, good heat sealing properties, and good drawdown characteristics.Applica..
|
|||
| Melt Temperature | 302 - 329 °C | 575 - 625 °F | |
|
Clariant Renol PPA1100G50 Polyphthalamide, 50% Glass Fiber
Data provided by Clariant Masterbatches
|
|||