| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 179 °C | 355 °F | |
|
Teknor Apex APEX® 124 Polyvinyl Chloride, Flexible
Notes: 80°C Jacket; RoHS Compliant Features: Good UV Resistance; Sunlight Resistant (720 hours) Uses: Flexible Cord Jacketing; Irrigation Cable Jacketing; Military Cable Jacketing; Wire and Cable..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Teknor Apex APEX® 154 Polyvinyl Chloride, Flexible
Notes: 80°C Jacket; RoHS Compliant Uses: Military Cable Jacketing; Non-flexible JacketingForms: Pellets Wire Types: Molded Components Agency Ratings: MIL C-915-C Additional Information: Temperatu..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Teknor Apex APEX® 155 Polyvinyl Chloride, Flexible
Notes: 80°C Jacket; RoHS CompliantFeatures: Sunlight Resistant (720 hours); Good UV Resistance Uses: Building Wire Jacketing; Wire and Cable Applications Agency Ratings: UL QMTT2 .E73402Forms: Pe..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Teknor Apex APEX® 162 Polyvinyl Chloride, Flexible
Notes: 80°C Jacket; RoHS Compliant Uses: Armored Cable; Flexible JacketingForms: Pellets Agency Ratings: MIL C-915-C; MIL C-2194-D Additional Information: Shipboard Cables, armored Temperature R..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Teknor Apex APEX® 164 Polyvinyl Chloride, Flexible
Notes: 60°C Jacket; RoHS Compliant Features: Flame Retardant; Low Temperature Flexibility; Moisture ResistantUses: Flexible Cord Jacketing Forms: Pellets Wire Types: SJTW; STW Processing Method: ..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Teknor Apex APEX® 3200-80 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Teknor Apex APEX® 3301-80 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Teknor Apex APEX® 3302-80 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Teknor Apex APEX® 3310-80 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Teknor Apex APEX® 3310-80NT Polyvinyl Chloride, Flexible
Features: DEHP Plasticizer; Ethylene Oxide Sterilizable Uses: Food Service Applications; Medical/Healthcare Applications; Tubing Processing Forms: Extrusion Forms: PelletsInformation Provided by Tek..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Teknor Apex APEX® 3311-80 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
|
|||
| Melt Temperature | 179 °C | 355 °F | Processing Temperature |
|
Teknor Apex APEX® 4103 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Teknor Apex APEX® 4124 Polyvinyl Chloride, Flexible
Notes: 75°C Jacket; RoHS Compliant Features: Good UV Resistance; Sunlight Resistant (720 hours) Uses: Appliance Wire Jacketing; Irrigation Cable Jacketing Forms: Pellets Wire Types: UL Style 2464..
|
|||
| Melt Temperature | 179 °C | 355 °F | Processing Temperature |
|
Teknor Apex APEX® 536 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
|
|||
| Melt Temperature | 179 °C | 355 °F | Processing Temperature |
|
Teknor Apex APEX® 6500-80 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
|
|||
| Melt Temperature | 179 °C | 355 °F | Processing Temperature |
|
Teknor Apex APEX® 7500-80 Polyvinyl Chloride, Flexible
Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Teknor Apex APEX® 90-A472R-80-NT Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-ClearForms-PelletsProcessing Method-..
|
|||
| Melt Temperature | 179 °C | 355 °F | Processing Temperature |
|
Teknor Apex APEX® 1003 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Teknor Apex APEX® 830 Polyvinyl Chloride, Flexible
Notes: 105°C Jacket; RoHS Compliant Features: Low Temperature Flexibility; High Heat Resistance; Oil Resistance Uses: Cable Jacketing Forms: Pellets Wire Types: SJT; ST; SVT; SRDT Processing Meth..
|
|||
| Melt Temperature | 179 - 216 °C | 355 - 420 °F | |
|
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
|
|||
| Melt Temperature | 179 - 216 °C | 355 - 420 °F | Extrusion |
|
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Axiall 11470 Wire & Cable Flexible PVC
Highly flame retardant clear compound. Recommended as jacket in PVC/PVC VW-1 constructions.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Axiall 11863 Wire & Cable Flexible PVC
Clear, UV resistant speaker wire.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Axiall 14771 Wire & Cable Flexible PVC
General purpose jacketing compound with good low temperature properties. Recommended for a maximum service temperature of 75°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpor..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Axiall 6850 Moldings & Extrusions Flexible PVC
Low gravity compound for extrusion and molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Axiall 8751 Moldings & Extrusions Flexible PVC
Clear, UV stabilized extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Axiall 8801 Moldings & Extrusions Flexible PVC
General purpose clear extrusion compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Axiall 8808 Moldings & Extrusions Flexible PVC
105°C rated flexible polyvinyl chloride compound formulated for UL94 V-2 in all colors. The compound is formulated for sunlight resistance.Information provided by Georgia GulfGeorgia Gulf became A..
|
|||
| Melt Temperature | 179 °C | 355 °F | |
|
Axiall 8850 Moldings & Extrusions Flexible PVC
General purpose extrusion.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Melt Temperature | 179 - 216 °C | 355 - 420 °F | Extrusion |
|
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance ..
|
|||