| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 370 - 390 °C | 698 - 734 °F | |
|
LATI LARPEEK 10 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
|
|||
| Melt Temperature | 360 - 390 °C | 680 - 734 °F | |
|
LATI Larpeek 10 PEEK
Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;..
|
|||
| Melt Temperature | 360 - 390 °C | 680 - 734 °F | |
|
LATI Larpeek 50 PEEK
Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;..
|
|||
| Melt Temperature | 350 - 390 °C | 662 - 734 °F | |
|
LATI Lapex R G/10 PPSU, 10% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
|
|||
| Melt Temperature | 350 - 390 °C | 662 - 734 °F | |
|
LATI Lapex R G/20 PPSU, 20% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
|
|||
| Melt Temperature | 350 - 390 °C | 662 - 734 °F | |
|
LATI Latilub 85-10T G/30 PES, 30% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyether Sulfone (PES). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
|
|||
| Melt Temperature | 350 - 390 °C | 662 - 734 °F | |
|
LATI Latiohm 85-06 PD01 G/15 PES, 15% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyether Sulfone (PES). Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
|
|||
| Melt Temperature | 360 - 390 °C | 680 - 734 °F | |
|
LATI Latiohm 88/10-06 CNT PEEK
Semiconductive/dissipative product based on Polyetheretherketone (PEEK). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
|
|||
| Melt Temperature | 365 - 390 °C | 689 - 734 °F | |
|
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. ..
|
|||
| Melt Temperature | 365 - 390 °C | 689 - 734 °F | |
|
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical streng..
|
|||
| Melt Temperature | 365 - 390 °C | 689 - 734 °F | |
|
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava..
|
|||
| Melt Temperature | 350 - 390 °C | 662 - 734 °F | Injection molding |
|
BASF Ultrason S 2010 G4 20% Glass Filled PSU
Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.
|
|||
| Melt Temperature | 330 - 390 °C | 626 - 734 °F | Injection molding |
|
BASF Ultrason S 2010 PSU
Ultrason S 2010 is an unreinforced, medium viscosity standard injection molding PSU grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..
|
|||
| Melt Temperature | 350 - 390 °C | 662 - 734 °F | Injection molding/extrusion |
|
BASF Ultrason® E 2010 C6 30% Carbon Filled
Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu..
|
|||
| Melt Temperature | 350 - 390 °C | 662 - 734 °F | Injection molding/extrusion |
|
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
Information provided by BASF
|
|||
| Melt Temperature | 340 - 390 °C | 644 - 734 °F | Injection molding/extrusion |
|
BASF Ultrason® E 2010 MR SW 10111 PESU
Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF
|
|||
| Melt Temperature | 350 - 390 °C | 662 - 734 °F | Injection molding/extrusion |
|
BASF Ultrason® E 3010 MR UN PESU
Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat..
|
|||
| Melt Temperature | 340 - 390 °C | 644 - 734 °F | Injection molding |
|
BASF Ultrason E 1010 PES
Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability.
|
|||
| Melt Temperature | 350 - 390 °C | 662 - 734 °F | Injection molding |
|
BASF Ultrason E 2010 G4 20% Glass Filled PES
Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.
|
|||
| Melt Temperature | 340 - 390 °C | 644 - 734 °F | Injection molding/extrusion |
|
BASF Ultrason® E 2010 HC PESU
Information provided by BASF
|
|||
| Melt Temperature | 340 - 390 °C | 644 - 734 °F | Injection molding/extrusion |
|
BASF Ultrason® E 2010 SW Q31 10088 PESU
Information provided by BASF
|
|||
| Melt Temperature | 350 - 390 °C | 662 - 734 °F | Injection molding/extrusion |
|
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, ..
|
|||
| Melt Temperature | 330 - 390 °C | 626 - 734 °F | Injection molding/extrusion |
|
BASF Ultrason® S 3010 MR UN PSU
Description: Unreinforced, higher viscosity injection molding and extrusion grade, tougher, with improved chemical resistance and demolding optimized. Abbreviated designation according to ISO 1043-1..
|
|||
| Melt Temperature | 365 - 390 °C | 689 - 734 °F | |
|
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
(Unverified Data**)
AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The ..
|
|||
| Melt Temperature | 343 - 390 °C | 650 - 734 °F | Average value: 362 °C Grade Count:24 |
|
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
|
|||
| Melt Temperature | 330 - 390 °C | 626 - 734 °F | |
|
BASF Ultrason S 6010 PSU
Ultrason S 6010 is an unreinforced, high molecular weight injection-molding and extrusion grade with excellent chemical resistance (stress crack resistance) and good solubility in typical solvents (..
|
|||
| Melt Temperature | 360 - 390 °C | 680 - 734 °F | |
|
LATI Latilub 88/50-20T PEEK, PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter..
|
|||
| Melt Temperature | 365 - 390 °C | 689 - 734 °F | |
|
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
(Unverified Data**)
AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir..
|
|||
| Melt Temperature | 360 - 390 °C | 680 - 734 °F | |
|
LATI Latilub 88/10-10T Y/10 PEEK, 10% Aramid Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..
|
|||
| Melt Temperature | 360 - 390 °C | 680 - 734 °F | |
|
LATI Latilub 88/50-30GRT PEEK, Graphite/PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
|
|||