| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
|
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE)
Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene..
|
|||
| Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
|
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE)
Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o..
|
|||
| Melt Temperature | 204 - 260 °C | 399 - 500 °F | Air purge at equilibrium conditions |
|
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade
High heat resistance, Sparking water-white clarity, Good chemical resistance, High modulus, for superior shear and torque resistanceApplications: Light pipes and lighting, High heat microwave packag..
|
|||
| Melt Temperature | 204 - 260 °C | 399 - 500 °F | air purge at equilibrium conditions |
|
NOVA Chemicals DYLARK® 378 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
|
|||
| Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
|
PolyOne Edgetek® AT-1000 Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| Melt Temperature | 204 - 210 °C | 399 - 410 °F | |
|
PolyOne Geon™ HTX M6230 Polyvinyl Chloride Alloy (PVC Alloy)
Information provided by PolyOne
|
|||
| Melt Temperature | 204 - 238 °C | 399 - 460 °F | |
|
Ineos Nova Zylar® 533 Clear Impact Modified UV Stabilized Acrylic Copolymer
(discontinued **)
Features: High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationExcellent indoor light stabilityHigh elongation and ductilityApplications: Appliance..
|
|||
| Melt Temperature | 204 - 221 °C | 399 - 430 °F | |
|
Dow Pellethane® 2102-90AR Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **)
PELLETHANE® 2102-90AR elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced mold release, low compression set, a..
|
|||
| Melt Temperature | 204 °C | 399 °F | |
|
Chevron Phillips 2151 High Impact, Liner Grade Film Resin
(discontinued **)
Resin Type: HomopolymerCharacteristics: High Impact Strength, Medium Slip, High Antiblock, Low Blocking and Good Openability, Good ProcessabilityApplications:Trash bags and other linersProcessing Co..
|
|||
| Melt Temperature | 204 °C | 399 °F | |
|
Chevron Phillips 5036 LDPE High Clarity, Impact Film Resin
(discontinued **)
Resin Type: Homopolymer; for General Purpose PackagingCharacteristics: Excellent Clarity, Good Impact Strength, High Slip, No Antiblock, Low Coefficient of Friction, Excellent ProcessabilityApplicat..
|
|||
| Melt Temperature | 204 °C | 399 °F | |
|
Chevron Phillips MarFlex® 5355 LDPE Industrial Clarity, General Purpose Film Resin
(discontinued **)
Resin Type: HomopolymerCharacteristics: Suited for High Speed Converting, Good Impact Strength, Excellent Processability, Good Sealability, Good OpenabilityApplications:Institutional Packaging, Food..
|
|||
| Melt Temperature | 204 °C | 399 °F | |
|
Chevron Phillips 5554-H LDPE High Clarity, Medium Impact Film Resin
(discontinued **)
Resin Type: HomopolymerCharacteristics: Excellent Clarity, Good Impact Strength, Excellent Processability, Low Coefficient of Friction, Good SealabilityApplications:Bread Bag, Dry Goods Packaging, P..
|
|||
| Melt Temperature | 204 - 232 °C | 399 - 450 °F | Stock |
|
PolyOne Stat-Tech™ AS-7SS/000 ABS - 7% Stainless Steel Fiber
(discontinued **)
Data provided by PolyOne.
|
|||
| Melt Temperature | 204 °C | 399 °F | |
|
Eastman 5269 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin
(discontinued **)
Resin Type: CopolymerCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flow for Injection Blow Molding Applications, Good Par..
|
|||
| Melt Temperature | 204 - 260 °C | 399 - 500 °F | air purge at equilibrium conditions |
|
NOVA Chemicals DYLARK® 238 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
|
|||
| Melt Temperature | 204 - 260 °C | 399 - 500 °F | air purge at equilibrium conditions |
|
NOVA Chemicals DYLARK® 250 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
|
|||
| Melt Temperature | 204 - 315 °C | 399 - 599 °F | |
|
NOVA Chemicals Novapol® TR-0535-U Hexene MDPE Rotational Molding Resin
(discontinued **)
Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer.
|
|||
| Melt Temperature | <= 204 °C | <= 399 °F | |
|
Kleerdex Kydex® P54 Acrylic/PVC Extrusion Compound
(discontinued **)
High impact profile extrusion compoundApplications: Extruded profiles requiring high impact, good chemical resistance, weatherability, and excellent flammability resistance.Features: P54 is extremel..
|
|||
| Melt Temperature | 204 - 315 °C | 399 - 599 °F | Varies with the mold shape and construction. Oven will also affect process time. |
|
NOVA Chemicals Sclair® TD-7915-UG Hexene MDPE Rotational Molding Resin
(discontinued **)
Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera..
|
|||
| Melt Temperature | 204 - 250 °C | 399 - 482 °F | |
|
Total PPH 3866 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics, Multifilament Yarns, and Extrusion Coating
Process Stability TOTAL Petrochemicals Polypropylene 3866 features excellent processability and gas fade resistance.FDA. 3866 complies with all applicable FDA regulations for food contact applicat..
|
|||
| Melt Temperature | 204 - 250 °C | 399 - 482 °F | |
|
Total PPR 7860 Controlled Rheology Grade Propylene Copolymer for Spunbond Nonwoven Fabrics, Multifilament Yarns and Extrusion Coating
TOTAL Petrochemicals Polypropylene 7860 is a propylene copolymer grade with narrow molecular weight distribution.Process Stability. 7860 features excellent processability and gas fade resistance.F..
|
|||
| Melt Temperature | 204 - 221 °C | 399 - 430 °F | Molding |
|
Lubrizol Estane® 2103-90A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20..
|
|||
| Melt Temperature | 204 °C | 399 °F | |
|
DuPont™ Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 1601 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
|
|||
| Melt Temperature | 204 °C | 399 °F | |
|
DuPont™ Surlyn® 1601-2 Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 1601-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s..
|
|||
| Melt Temperature | 204 °C | 399 °F | Extrusion |
|
ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
|
|||
| Melt Temperature | 204 - 315 °C | 399 - 599 °F | Varies with the mold shape and construction. Oven will also affect process time. |
|
NOVA Chemicals Sclair® TD-7915-U Hexene MDPE Rotational Molding Resin
(discontinued **)
Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera..
|
|||
| Melt Temperature | 204 °C | 399 °F | |
|
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber
(discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
|
|||
| Melt Temperature | 204 - 221 °C | 399 - 430 °F | Molding |
|
Lubrizol Estane® 2102-55D Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Load-bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product line from Dow in..
|
|||
| Melt Temperature | 204 - 221 °C | 399 - 430 °F | |
|
Dow PELLETHANE® 2355-55DE Polyurethane Elastomer, Polyester Polyadipate Based
(discontinued **)
Description: PELLETHANE® 2355-55DE polyester polyadipate based polyurethane elastomer has excellent oil and chemical resistance. Applications include: Film, Sheet, Tubing, Recreation and sporting e..
|
|||
| Melt Temperature | 204 - 238 °C | 399 - 460 °F | |
|
Ineos Nova Zylar® 94-580-A High Performance Styrenic, Acrylic Copolymer
(discontinued **)
Excellent heat distortion temperature, High clarity, strength and toughness, Enhanced mold releaseApplications: Industrial covers and housings, Paper towel dispenser covers, Appliance partsInjection..
|
|||