| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
|
PolyOne OnFlex™ BIO 5180D-E0014 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab..
|
|||
| Melt Temperature | 225 - 235 °C | 437 - 455 °F | |
|
NOVA Chemicals Sclair® 14B3 Butene LMDPE Film Resin
(discontinued **)
Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer.
|
|||
| Melt Temperature | 225 - 320 °C | 437 - 608 °F | Average value: 288 °C Grade Count:5 |
|
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
|
|||
| Melt Temperature | 225 °C | 437 °F | LCL-PR29 |
|
Intercontinental Polymers HoPBT 303 HoPBT Polymer Type - Clear, Polyester Pellets
Applications: Engineering Resin Information provided by Intercontinental Polymers.
|
|||
| Melt Temperature | 225 °C | 437 °F | LCL-PR29 |
|
Intercontinental Polymers HoPBT 545 HoPBT Polymer Type - Clear, Polyester Pellets
Applications: Engineering Resin Information provided by Intercontinental Polymers.
|
|||
| Melt Temperature | 225 °C | 437 °F | |
|
Iran Petrochemical (PCC) LL0209 SR Linear Low Density Polyethylene
LL 0209 is a LLDPE copolymer with butene as comonomer which contains anti-oxidant, Slip and antiblock additives. It gives film of high slip which is easily separable. It is recommended for general ..
|
|||
| Melt Temperature | 225 °C | 437 °F | |
|
Iran Petrochemical (PCC) LL0220AA Linear Low Density Polyethylene
LL 0220 AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. This grade is suitable for the production of blown film for light duty applications and for the production of ca..
|
|||
| Melt Temperature | 225 °C | 437 °F | |
|
SIDPEC EGYPTENE® LL 0209 KJ LLDPE Film
Applications:Refuse sacksProduce bags, carrier bagsFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o..
|
|||
| Melt Temperature | 225 °C | 437 °F | |
|
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film
Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l...
|
|||
| Melt Temperature | 225 - 260 °C | 437 - 500 °F | |
|
Eastman Ecdel PCCE 9966 Copolyester Ether Elastomer
ISO data as provided by the manufacturer, Eastman Chemical
|
|||
| Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
|
Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded
Starpylen HW 30K ECR-BK is a reinforced Polypropylene with a low carbon footprint spherical filler, Injection Molding Resin (also known as HW30KECR)Information provided by Eurostar.
|
|||
| Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
|
Eurostar Starpylen HZ 50E3 PP, Injection Molded
PRELIMINARY-Starpylen HZ 50E3 is a High Specific Gravity Polypropylene (density 1.5), Injection Molding Resin (also known as HZ50E3)Information provided by Eurostar.
|
|||
| Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
|
Eurostar Starpylen MF007AS PP, Glass Fiber Filled, Injection Molded
Starpylen MF007AS is a Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
|
Eurostar Starpylen MF008S PP, 40% Glass Fiber Filled, Injection Molded
Starpylen MF008S is a 40% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
|
Eurostar Starpylen MFB44S PP, Glass Bead/Glass Fiber Filled
Starpylen MFB44S is a Glass Beads, Glass Fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WS 2020VK S37.7)Information provided by Eurostar.
|
|||
| Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
|
Eurostar Starpylen MH0200A HDPE, Injection Molding
Starpylen MH0200A is a High Density Polypropylene Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
|
Eurostar Starpylen MK001AS PP, Mineral Filled, Injection Molding
Starpylen MK001AS is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
|
Eurostar Starpylen MX06050 PP, 30% Glass Filled, Injection Molded
Starpylen MX06050 is a 30% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
|
BASF Ultramid® HFX 33 PA6 (Dry)
Description: Ultramid HFX 33 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en..
|
|||
| Melt Temperature | 225 - 280 °C | 437 - 536 °F | |
|
Beijing Ranger Chem PBT 403 G-M50 Heat Resistant and Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
|
Beijing Ranger Chem PBT 403 M-G30 HF Halogen Free Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
|
Beijing Ranger Chem PBT-201-G0 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
|
Beijing Ranger Chem PBT-201-G10 202 Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
|
Beijing Ranger Chem PBT-201-G10 272 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
|
Beijing Ranger Chem PBT-201-G20 272 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
|
Beijing Ranger Chem PBT-201-G30 202 Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Melt Temperature | 225 - 250 °C | 437 - 482 °F | Injection-molding |
|
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled PBT
Description: Is a PBT, easy-flowing injection-molding grades with 15% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers, cove..
|
|||
| Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
|
Beijing Ranger Chem PBT-MFC-G30 FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
|
Beijing Ranger Chem PBT 403 M-G0 Heat Resistant and Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||