Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 460 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 238 - 271 °C
460 - 520 °F
Molding
PolyOne Lubri-Tech™ PS-30GF/02S Polybutylene Terephthalate (PBT), Glass Filled, PTFE/Silicone Lubricated  (dis
Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 238 - 260 °C
460 - 500 °F
Stock
PolyOne Lubri-Tech™ PS-000/20T Polyester (PBT) - 20% PTFE Lubricated  (discontinued **)
Data provided by PolyOne.
Melt Temperature 238 °C
460 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 7% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Melt Temperature 238 °C
460 °F
Injection
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 10% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Melt Temperature 238 - 260 °C
460 - 500 °F
Molding
PolyOne Edgetek® NL-08GF-02CF/000 Nylon 6/12, Glass/Carbon Fiber Filled  (discontinued **)
Description/Features:Glass/Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 238 - 274 °C
460 - 525 °F
Styron EMERGEâ„¢ 7700 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Overview: EMERGEâ„¢ PC/ABS 7700 Advanced Resin is an ignition-resistant PC/ABS blend that contains no chlorine for bromine additives. It has superior processability for injection molding applicat..
Melt Temperature 238 - 271 °C
460 - 520 °F
Melt temperatures above 530°F are not recommended, and may result in color shifts and or thermal instability.
Diamond Polymers ABS/PC 9901
Description: Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Melt Temperature 238 - 260 °C
460 - 500 °F
Clariant Renol PA211G13 Nylon 6, 13% Glass Fiber
Data provided by Clariant Masterbatches
Melt Temperature 238 - 260 °C
460 - 500 °F
Clariant Renol PA213G13 Nylon 6, 13% Glass Fiber, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Melt Temperature 238 - 260 °C
460 - 500 °F
Clariant Renol PA213G36S Nylon 6, 36% Glass Fiber, Heat Stabilized, Silicone Lubricated
Data provided by Clariant Masterbatches
Melt Temperature 238 - 260 °C
460 - 500 °F
Clariant Renol PA233G13HT Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Highly Toughened
Data provided by Clariant Masterbatches
Melt Temperature 238 - 271 °C
460 - 520 °F
Melt temperatures above 530°F are not recommended, and may result in color shifts and or thermal instability.
Diamond Polymers ABS/PC 8901
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Melt Temperature 238 - 260 °C
460 - 500 °F
Polymer Resources PC/TP-GP3 PC Polyester, High Impact, Superior Chemical Resistance  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Temperature 238 - 280 °C
460 - 536 °F
Average value: 258 °C Grade Count:30
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..
Melt Temperature 238 - 280 °C
460 - 536 °F
Average value: 257 °C Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu..
Copyright © lookpolymers.com All Rights Reserved