| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 230 - 240 °C | 446 - 464 °F | |
|
Polyplastic Armlen® PP MF 30-3IM Polypropylene, 30% Mineral Filled
UV resistant, impact modified, heat stabilizedInformation provided by PolyPlastic Group.
|
|||
| Melt Temperature | 225 - 240 °C | 437 - 464 °F | |
|
Eastman Tenite 371A-10 Cellulose Acetate Propionate
(discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
|
Kingfa MAC-451 PC/ABS Alloy
Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingHousehold applianceAutomobile interior/exterior trim partsTel..
|
|||
| Melt Temperature | 210 - 240 °C | 410 - 464 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1063D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Melt Temperature | 200 - 240 °C | 392 - 464 °F | Injection Molding |
|
LG Chemical KEYFLEX TO1192A Olefin Type TPE
Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7, 1333-86-4 and 9002-88-4Information provided by LG Chemical
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
|
LG Chemical LG704W ABS, Low Gloss, Heat Resistance
Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chem..
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
|
LG Chemical LG749W ABS, Low Gloss, Heat Resistance
Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by..
|
|||
| Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
|
LG Chemical LUPOL TE-5202U Thermoplastic Elastomer Alloy, 20% Polymer Alloy, High Impact, High Modulus
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
|
|||
| Melt Temperature | 210 - 240 °C | 410 - 464 °F | Extrusion |
|
Ineos Styrenics Avantra® 585K Q402 Rubber Modified Polystyrene
Avantra® 585K Q402 is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical toughness. Although Avantra® 585K Q402 can be processed by any method applic..
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | Injection molding |
|
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
|
LG Chemical XR401B ABS, High Flow, Heat Resistance
Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p..
|
|||
| Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
|
LG Chemical LUPOL TE-5006K Thermoplastic Elastomer Alloy, Weather Resistant
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem
|
|||
| Melt Temperature | 210 - 240 °C | 410 - 464 °F | Injection Molding |
|
LG Chemical SG175NS ABS, Super Surface Gloss, General Anti-Static
Feature: Injection Molding, Super Surface Gloss, General Anti-StaticApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
|
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica..
|
|||
| Melt Temperature | 210 - 240 °C | 410 - 464 °F | Flat film |
|
Styrolution Polystyrol 168 N GR 2 PS
Description: Polystyrol 168 N is a high molecular, heat grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact..
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
|
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Temperature | 170 - 240 °C | 338 - 464 °F | Flat film extrusion |
|
Styrolution Styroflex® 2G 66 SBC
Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o..
|
|||
| Melt Temperature | 200 - 240 °C | 392 - 464 °F | Flat film |
|
Styrolution Polystyrol 165 H GR 21 PS
Description: Polystyrol 165 H is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.Applications: In blends with high impact Polystyrene or Styrolux; thermo..
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
|
Tisan TISLAMID® 6 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
|
Tisan TISLAMID® 6 30% Glass Bead Reinforced Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Melt Temperature | 205 - 240 °C | 401 - 464 °F | |
|
Eastman Eastar CN015 Copolyester, High Flow Grade with Mold Release
Applications:CompactsCosmetic jar capsCosmetic jarsCosmetics/personal care packagingFragrance capsFragrance packagingLip gloss containersLipstick containersPersonal care bottlesKey Attributes:Abilit..
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
|
Covestro Desmopan® DP 9662DU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPrepro..
|
|||
| Melt Temperature | 230 - 240 °C | 446 - 464 °F | DAM; Extrusion |
|
DuPont Performance Polymers Zytel® FE310001 NC010 Nylon 612
Zytel® FE310001 NC010 is a high viscosity polyamide 612 resin that is suitable for extrusion applications, such as monofilaments and tubing.Information provided by DuPont Performance Polymers
|
|||
| Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
|
Clariant Renol ABNN732017 Nylon 6 with anchored silicone
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
|
Bapolene® 122F Polyethylene, Film Grade
Bapolene LL122F is a general purpose LLDPE for blown film extrusion applications. This resin offers excellent tensile and toughness properties. Contains medium levels of slip/antiblock additives. ..
|
|||
| Melt Temperature | 230 - 240 °C | 446 - 464 °F | DAM; Extrusion |
|
DuPont Performance Polymers Zytel® FG7301 NC010 Nylon 6
(Unverified Data**)
Zytel® FG7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications. It has been developed for consideration into applications such as parts for the food industry.In..
|
|||
| Melt Temperature | 230 - 240 °C | 446 - 464 °F | |
|
LATI Later 4-V0 PBT, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide freeAvailability: Africa & Middle East; Asia Pacific; Europe; L..
|
|||
| Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
|
LG Chemical LUPOL GP-2201F General Purpose Polypropylene, 20% Glass Fiber Reinforced, Flame Retardant
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
|
|||