| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 255 - 270 °C | 491 - 518 °F | |
|
Parker Chomerics PREMIER™ A240-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
|
|||
| Melt Temperature | 255 - 270 °C | 491 - 518 °F | |
|
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
|
|||
| Melt Temperature | 255 - 260 °C | 491 - 500 °F | Extrusion |
|
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
|
|||
| Melt Temperature | 255 - 280 °C | 491 - 536 °F | Start Point: 260°C |
|
Kingfa JH720 G15 15% Glass Fiber Reinforced PC
Features:Excellent balance propertiesHigh mechanical propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug partsIn..
|
|||
| Melt Temperature | 255 - 285 °C | 491 - 545 °F | Start Point: 265°C |
|
Kingfa PA6-G50 50% Glass Fiber Reinforced PA6
Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t..
|
|||
| Melt Temperature | 255 - 285 °C | 491 - 545 °F | Start Point: 265°C |
|
Kingfa PA6-MG45 45% Glass & Mineral Filled PA6
Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Melt Temperature | 255 - 270 °C | 491 - 518 °F | Injection Molding |
|
LG Chemical LUMID GP2151AF PA6+GF15%, Flame Retardant
Feature: Injection Molding, PA6+GF15%, Flame RetardantApplication: ConnectorsCAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
|
|||
| Melt Temperature | 255 - 285 °C | 491 - 545 °F | Injection Molding |
|
LG Chemical LUMID LW4403A(W) PA66+GF/MF40%, Low Warpage
Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Melt Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
|
LG Chemical Lupox® SG3250M PBT+PET+MF25%
Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical
|
|||
| Melt Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
|
LG Chemical Lupox® SG5200 PBT+PET+GF20%
Description: Injection Molding, PBT+PET+GF20%, Good Surface Application: E&E (Microwave Oven Door Gasket)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical
|
|||
| Melt Temperature | 255 - 285 °C | 491 - 545 °F | Injection Molding |
|
LG Chemical LUPOY GN1006FT PC, Halogen Free, Flame Retardant
Description: Injection Molding, PC, Halogen Free Flame Retardant, Good FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
|
|||
| Melt Temperature | 255 - 285 °C | 491 - 545 °F | Injection Molding |
|
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature
Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided..
|
|||
| Melt Temperature | 255 - 260 °C | 491 - 500 °F | Extrusion |
|
LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
|
|||
| Melt Temperature | 255 °C | 491 °F | LCL-PR29 |
|
Intercontinental Polymers HoPET 737 HoPET Polymer Type - Bright, Polyester Pellets
Applications: Filament Yarn Information provided by Intercontinental Polymers.
|
|||
| Melt Temperature | 255 °C | 491 °F | LCL-PR29 |
|
Intercontinental Polymers HoPET 774 HoPET Polymer Type - Dull, Polyester Pellets
Applications: Filament Yarn Information provided by Intercontinental Polymers.
|
|||
| Melt Temperature | 255 - 270 °C | 491 - 518 °F | |
|
Lavergne VYPET 2130 Polyester Alloy Resin, 30% Fiberglass Reinforced
Vypet 2130 is a 30% fiberglass reinforced, toughened Modified PBT injection molding compound designed for structural and electrical applications.Features: High temperature performances; Excellent di..
|
|||
| Melt Temperature | 255 - 285 °C | 491 - 545 °F | Start Point: 265°C |
|
Kingfa PA6-G30 N101 30% Glass Fiber Reinforced PA6 (general purpose)
Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t..
|
|||
| Melt Temperature | 255 - 285 °C | 491 - 545 °F | Start Point: 265°C |
|
Kingfa PA6-M25G20 20% Glass & 25% Mineral Filled PA6
Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Melt Temperature | 255 - 285 °C | 491 - 545 °F | Start Point: 265°C |
|
Kingfa PA6-T25 25% Mineral Filled PA6
Features:Low tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Melt Temperature | 255 - 275 °C | 491 - 527 °F | Start Point: 260°C |
|
Kingfa PET-RG15 Flame Retardant, 15% Glass Fiber Reinforced PET
Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & ..
|
|||
| Melt Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
|
LG Chemical Lupox® SG5500 PBT+PET+GF50%
Description: Injection Molding, PBT+PET+GF50%, Good Surface, High StiffnessApplication: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical
|
|||
| Melt Temperature | 255 °C | 491 °F | LCL-PR29 |
|
Intercontinental Polymers HoPET 728-02 HoPET Polymer Type - Clear, Polyester Pellets
Applications: Engineering ResinInformation provided by Intercontinental Polymers.
|
|||
| Melt Temperature | 255 - 260 °C | 491 - 500 °F | Extrusion |
|
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
|
|||
| Melt Temperature | 255 - 265 °C | 491 - 509 °F | |
|
Toyobo VYLOPET® EMC310 Injection Molding Polyester Resin
Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo.
|
|||
| Melt Temperature | 255 - 265 °C | 491 - 509 °F | |
|
Toyobo VYLOPET® EMC317A Injection Molding Polyester Resin, Warpageless
Applications: Iron's heat insulation plateChair framesHousingsFeatures: WarpagelessInformation provided by Toyobo.
|
|||
| Melt Temperature | 255 - 270 °C | 491 - 518 °F | |
|
Toyobo VYLOPET® EMC341 Injection Molding Polyester Resin, Hydrolysis Resistant
Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo.
|
|||
| Melt Temperature | 255 - 270 °C | 491 - 518 °F | |
|
Toyobo VYLOPET® EMC545 Injection Molding Polyester Resin, Glass Reinforced
Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo.
|
|||
| Melt Temperature | 255 - 270 °C | 491 - 518 °F | |
|
Toyobo VYLOPET® EMC532 Injection Molding Polyester Resin, Glass Reinforced
Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo.
|
|||
| Melt Temperature | 255 - 265 °C | 491 - 509 °F | |
|
Eurostar Starflam P10003 PA6, Mineral Filled, Flame Retardant, Extrusion
Starflam P10003 is a Mineral Filled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 255 °C | 491 °F | |
|
E-Polymers TEKAMID® H24WC High Toughness Heat Strength PA/ABS Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB..
|
|||