| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 232 - 271 °C | 450 - 520 °F | |
|
PolyOne Gravi-Tech™ GRV-PB-069-BMX Natural Polyether Block Amide (PEBA-Ether)
Information provided by PolyOne
|
|||
| Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
|
PolyOne Versaflex™ OM 6258-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6258-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
|
|||
| Melt Temperature | 254 - 271 °C | 489 - 520 °F | ASTM D789 |
|
Niche Polymer PA66GM38BK Nylon 66, 38% Glass/Mineral Fiber Filled
Information provided by Niche Polymer
|
|||
| Melt Temperature | 232 - 271 °C | 450 - 520 °F | |
|
PTS Trimid® N6-200L Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Temperature | 243 - 271 °C | 470 - 520 °F | |
|
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (Cond)
Information provided by Ravago.
|
|||
| Melt Temperature | 243 - 271 °C | 470 - 520 °F | |
|
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (DAM)
Information provided by Ravago.
|
|||
| Melt Temperature | 249 - 271 °C | 480 - 520 °F | Molding |
|
PolyOne Lubri-Tech™ PS-15GB/10T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont
Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Melt Temperature | 232 - 271 °C | 450 - 520 °F | Molding |
|
PolyOne Lubri-Tech™ PS-30CF/10T 2S Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced, PTFE/Silicone Lubricated
Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Melt Temperature | 238 - 271 °C | 460 - 520 °F | Molding |
|
PolyOne Lubri-Tech™ PS-30GF/02S Polybutylene Terephthalate (PBT), Glass Filled, PTFE/Silicone Lubricated
(dis
Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Polymer Resources NY6-M40 Nylon 6, 40% Mineral Filled
Nylon 6, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested ..
|
|||
| Melt Temperature | 232 - 271 °C | 450 - 520 °F | Air purge at equilibrium conditions |
|
NOVA Chemicals Dylark® 510XT Glass Reinforced Engineering Resin
Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri..
|
|||
| Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
|
MRC Polymers NAXALOYâ„¢ 780 PC+PBT Polyester Blend
Good chemical resistance, impact and heat resistance.Information provided by MRC Polymers Inc.
|
|||
| Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Eastman Eastar DN114 Copolyester, Natural
Applications:LightingProduct Description: Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage. DN1..
|
|||
| Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Eastman Eastar MN211 Copolyester, Natural
Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. MN211 contains a mold release.Application..
|
|||
| Melt Temperature | 221 - 271 °C | 430 - 520 °F | Melt temperatures above 530°F are not recommended, and may result in color shifts and or thermal instability. |
|
Diamond Polymers ASA S310
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Impact and ModulusInformation provided by Diamond Polymers, Inc.
|
|||
| Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
|
Clariant 6008 L Nylon 6, High Impact, Injection Molding
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 243 - 271 °C | 470 - 520 °F | |
|
Clariant PA612G30 Nylon 612, 30% Glass Fiber, Impact Modified