Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 527 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Melt Temperature 275 - 290 °C
527 - 554 °F
Do not melt above 300°C
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66
Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a..
Melt Temperature 275 - 290 °C
527 - 554 °F
Do not melt above 290°C
Nilit Nilamid A G10 FR PH1 50% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous)
Description: Nilamid A G10 FR PH1 was developed specifically for highly loaded, structural applications in the electrical industry. It combines extremely high mechanical performance with flame retar..
Melt Temperature 275 - 300 °C
527 - 572 °F
Do not melt above 300°C
Nilit Nilamid A3 H G6 General Purpose 30% Glass Reinforced PA66
Description: Nilamid A3 H G6 is a general purpose 30% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi..
Melt Temperature 275 - 290 °C
527 - 554 °F
Do not melt above 300°C
Nilit Nilamid A3 H ZB High Impact PA66
Description: Nilamid A3 H ZB is high impact NYLON 66. The product maintains excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas ..
Melt Temperature 275 - 310 °C
527 - 590 °F
Start Point: 285°C
Kingfa PA66-C111 Toughened PA66
Features:High impactLow tendency to wrapExcellent balance propertiesApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Melt Temperature 275 - 310 °C
527 - 590 °F
Start Point: 285°C
Kingfa PA66-G15 15% Glass Fiber Reinforced PA66
Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t..
Melt Temperature 275 - 300 °C
527 - 572 °F
Lavergne VYPET VNT 335 PET 35% Glass - Mineral Reinforced
Vypet VNT 335 is a 35% glass/mineral reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional stabilityT..
Melt Temperature 275 - 300 °C
527 - 572 °F
Lavergne VYPET VNT 930 PET 30% Glass Reinforced
Vypet VNT 930 is a 30% fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional stabilityTypi..
Melt Temperature 275 - 310 °C
527 - 590 °F
Start Point: 285°C
Kingfa PA66-G30 30% Glass Fiber Reinforced PA66
Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t..
Melt Temperature 275 - 300 °C
527 - 572 °F
LATI Latamid 66 H2 G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Melt Temperature 275 - 300 °C
527 - 572 °F
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced
Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Melt Temperature 275 - 300 °C
527 - 572 °F
LATI Latilub 66-01M G/30 PA66, 30% Glass Fiber Reinforced, Molybdenum disulphide Filled
Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Melt Temperature 275 - 300 °C
527 - 572 °F
LATI Latilub 66-10T K/10 PA66, 10% Carbon Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
Melt Temperature 275 - 320 °C
527 - 608 °F
LATI Latilub 87/28-12T G/20 PC, 20% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polycarbonate (PC). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria ..
Melt Temperature 275 - 300 °C
527 - 572 °F
LATI Latishield 66-10A H2 CETG/400 PA66, Steel/Glass Fiber Reinforced, Mineral Filled, Heat Stabilized
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
Melt Temperature 275 - 300 °C
527 - 572 °F
Lavergne VYPET VNT 615 PET 15% Glass Reinforced
Vypet VNT 615 is a 15% fiberglass reinforced PET injection molding compound designed for structural applications.Features: Easy, fast processing; Excellent strength and stiffness; Excellent dimensio..
Melt Temperature 275 - 290 °C
527 - 554 °F
Solvay Specialty Polymers Omnix® 4050 Polyamide, High Performance (HPPA) (Conditioned)
Omnix® 4050 is a 50% glass-fiber reinforced, high-performance polyamide (HPPA). It is particularly suited for replacing die-cast metal in a variety of mechanical applications and components used ..
Melt Temperature 275 - 290 °C
527 - 554 °F
Solvay Specialty Polymers Omnix® 4050 Polyamide, High Performance (HPPA) (Dry)
Omnix® 4050 is a 50% glass-fiber reinforced, high-performance polyamide (HPPA). It is particularly suited for replacing die-cast metal in a variety of mechanical applications and components used ..
Melt Temperature 275 - 295 °C
527 - 563 °F
DAM; Injection Molding
DuPont Performance Polymers Zytel® FN714 NC010A Nylon 66
Zytel® FN714 NC010A is an impact modified, very flexible, plasticizer free polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers
Melt Temperature 275 - 295 °C
527 - 563 °F
DAM; Injection Molding
DuPont Performance Polymers Zytel® FN718 NC010A Nylon 66
Zytel® FN718 NC010A is a flexible, plasticizer free modified polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers
Melt Temperature 275 - 295 °C
527 - 563 °F
DAM
DuPont Performance Polymers Zytel® PLUS PLSFR95G15DH2 BK269 Nylon  (Unverified Data**)
Zytel® PLSFR95G15DH2 BK269 is 15% glass reinforced, flame retardant black PA using SHIELD Technology, only from DuPont, exceptional resistance in hot air & hot engine oil.Information provided by Du..
Melt Temperature 275 - 285 °C
527 - 545 °F
Eurostar Staramide RFB53U PA66, 50% Glass Bead/Fiber Filled, Injection Molded
RFB53U is a Glass Bead/ Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 1525 VK Z4)Information provided by Eurostar.
Melt Temperature 275 °C
527 °F
Injection molding
BASF Petra® 140 45% Glass Filled PET
Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Ex..
Melt Temperature 275 °C
527 °F
Injection molding
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry)
Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla..
Melt Temperature 275 °C
527 °F
Injection molding
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and ..
Melt Temperature 275 °C
527 °F
Injection molding
BASF Ultramid® 8260 40% Mineral Filled PA6 (Dry)
Ultramid 8260 is a 40% mineral reinforced PA6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low..
Melt Temperature 275 °C
527 °F
Injection molding
BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Conditioned)
Ultramid 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced PA6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined wi..
Melt Temperature 275 °C
527 °F
Injection molding
BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Dry)
Ultramid 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced PA6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined wi..
Melt Temperature 275 °C
527 °F
Injection molding
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)
Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin..
Melt Temperature 275 - 300 °C
527 - 572 °F
LATI Latilub 66-20T G/40 PA66, 40% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri..
Copyright © lookpolymers.com All Rights Reserved