Polymer Property : Melt Temperature = 534 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Melt Temperature 279 °C
534 °F
Chem Polymer Chemlon 109-18 G Nylon 66, 18% Glass Fiber Reinforced
A highly toughened 18% glass fiber reinforced nylon 66 developed for applications requiring stiffness, creep resistance and impact resistance.Data provided by the manufacturer, Chem Polymer.
Melt Temperature 279 °C
534 °F
Chem Polymer Chemlon 109-33 G Nylon 66, 33% Glass Fiber Reinforced
A highly toughened 33% glass fiber reinforced nylon 66 developed for applications requiring stiffness, creep resistance and impact resistance.Data provided by the manufacturer, Chem Polymer.
Melt Temperature 279 °C
534 °F
Chem Polymer Chemlon 113 G Nylon 66, 13% Glass Fiber Reinforced
A 13% glass fiber reinforced nylon 66 offering improved creep resistance, stiffness, tensile strength and dimensional stability over unmodified nylon 66 materials.Data provided by the manufacturer, ..
Melt Temperature 279 °C
534 °F
Chem Polymer Chemlon 115 G Nylon 66, 15% Glass Fiber Reinforced
A 15% glass fiber reinforced nylon 66 offering improved creep resistance, stiffness, tensile strength and dimensional stability over unmodified nylon 66 materials. This product offers slight improv..
Melt Temperature 279 °C
534 °F
Chem Polymer Chemlon 104-13 G Nylon 66, 13% Glass Fiber Reinforced
A toughened, 13% glass fiber reinforced nylon 66 exhibiting improved toughness and ductility, especially dry as molded.Data provided by the manufacturer, Chem Polymer.