Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Melt Temperature 280 - 310 °C
536 - 590 °F
Plastcom SLOVAMID 66 T 30 Polyamide 66, 30% Mineral Filled
FeaturesPA 66 with the content of 30% chemically modified mineral filler. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cove..
Melt Temperature 280 - 310 °C
536 - 590 °F
Idemitsu Kosan Xarec® EA 543 SPS, 40% Glass Filled
Melt Temperature 280 - 310 °C
536 - 590 °F
Idemitsu Kosan Xarec® N WA 7020 SPS, 20% Glass Filled
Crystalline Polymer Blend, Glass Filled, Impact Modified. Used in Automotive Electronics applications.
Melt Temperature 280 - 310 °C
536 - 590 °F
Idemitsu Kosan Xarec® WA 550 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled. Used in Automotive and Industrial applications
Melt Temperature 275 - 310 °C
527 - 590 °F
Start Point: 285°C
Kingfa PA66-G30 30% Glass Fiber Reinforced PA66
Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t..
Melt Temperature 290 - 310 °C
554 - 590 °F
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced
Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle..
Melt Temperature 290 - 310 °C
554 - 590 °F
LATI Latilub 80-10T G/40 PPS, 40% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Melt Temperature 280 - 310 °C
536 - 590 °F
Solvay Specialty Polymers Kalix® 2855 Polyamide, High Performance (HPPA), Glass Fiber
Kalix® 2855 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is formulated to provide maximum strength, stiffness, impact resistance, and p..
Melt Temperature 300 - 310 °C
572 - 590 °F
Samyang Trirex® 3030IR Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Melt Temperature 290 - 310 °C
554 - 590 °F
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66
Information provided by A. Schulman.
Melt Temperature 290 - 310 °C
554 - 590 °F
A. Schulman SCHULAMID® 66 GB40 40% Glass Bead Reinforced Nylon 66
Information provided by A. Schulman.
Melt Temperature 290 - 310 °C
554 - 590 °F
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Melt Temperature 290 - 310 °C
554 - 590 °F
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Melt Temperature 290 - 310 °C
554 - 590 °F
A. Schulman Aqualoy® 645 Glass Fiber Reinforced Hydrolysis Resistant Nylon 66
Information provided by A. Schulman.
Melt Temperature 290 - 310 °C
554 - 590 °F
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66
Information provided by A. Schulman.
Melt Temperature 290 - 310 °C
554 - 590 °F
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Melt Temperature 290 - 310 °C
554 - 590 °F
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Melt Temperature 290 - 310 °C
554 - 590 °F
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66
Information provided by A. Schulman.
Melt Temperature 290 - 310 °C
554 - 590 °F
A. Schulman SCHULAMID® 66 MK4015H 40% Glass Fiber/Mineral Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Melt Temperature 290 - 310 °C
554 - 590 °F
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Melt Temperature 280 - 310 °C
536 - 590 °F
E-Polymers TEKAPPO® J930 30% Glass Fiber Reinforced M-PPO
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a..
Melt Temperature 280 - 310 °C
536 - 590 °F
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Melt Temperature 260 - 310 °C
500 - 590 °F
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Melt Temperature 260 - 310 °C
500 - 590 °F
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..