| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 293 - 327 °C | 559 - 621 °F | |
|
PolyOne Edgetek® PC-15CF-15GF/000 Polycarbonate (PC)
Information provided by PolyOne
|
|||
| Melt Temperature | 299 - 327 °C | 570 - 621 °F | Excellent Processability |
|
Chevron Phillips 1025 Extrusion Coating Resin
(discontinued **)
Resin Type: Speed Resin, Base Resin Type - Chevron PE1017Characteristics: Excellent Processability at 570-620°F (300-325°C) Melt, Good Adhesion at Low Coating Weights and High Speed Lines, Low COF..
|
|||
| Melt Temperature | 299 - 327 °C | 570 - 621 °F | Excellent Processability |
|
Chevron Phillips 1028 Extrusion Coating Resin
(discontinued **)
Resin Type: High Speed Slip ResinCharacteristics: Excellent Processability at 570-620°F (300-325°C) Melt, Good Adhesion at Low Coating Weights and High Speed Lines, Low COF uses, FDA Approved for ..
|
|||
| Melt Temperature | 254 - 327 °C | 489 - 621 °F | Average value: 296 °C Grade Count:36 |
|
Overview of materials for Polycarbonate, Carbon + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu..
|
|||
| Melt Temperature | 274 - 327 °C | 525 - 621 °F | Average value: 301 °C Grade Count:8 |
|
Overview of materials for Polycarbonate, Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr..
|
|||
| Melt Temperature | 299 - 327 °C | 570 - 621 °F | |
|
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, ..
|
|||
| Melt Temperature | 299 - 327 °C | 570 - 621 °F | |
|
Styron EMERGEâ„¢ 4510-6 Polycarbonate
EMERGEâ„¢ PC 4510-6 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Informa..
|
|||
| Melt Temperature | 299 - 327 °C | 570 - 621 °F | |
|
Styron EMERGEâ„¢ 4530-6 Polycarbonate
EMERGEâ„¢ PC 4510-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co..
|
|||
| Melt Temperature | 299 - 327 °C | 570 - 621 °F | |
|
Styron EMERGEâ„¢ 4800-7 Polycarbonate
EMERGEâ„¢ 4800-7 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polycar..
|
|||
| Melt Temperature | 315 - 327 °C | 599 - 621 °F | Extrusion Coating Processability |
|
Dow 4012 Low Density Polyethylene (LDPE)
Polyethylene 4012 is used for a variety of applications such as condiment packaging, dry and moist foods packaging, sugar pouches, lidding stock and medical packaging.Information provided by Dow
|
|||
| Melt Temperature | 293 - 327 °C | 559 - 621 °F | Stock |
|
PolyOne Lubri-Tech™ MP-20GF/15T Modified PPO - 20% Glass Fiber - 15% PTFE
(discontinued **)
Data provided by PolyOne.
|
|||