Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+12 ohm-cm
>= 1.00e+12 ohm-cm
50% RH; IEC 60093
Murtfeldt Murylon® B Nylon 6
Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical prope..
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Rogers Corporation Poron® 4701-40-15 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
Electrical Resistivity >= 1.00e+12 ohm-cm
>= 1.00e+12 ohm-cm
ASTM D257
Quantum Composites QC-8800 63% Glass Fiber Vinyl Ester SMC
QC-8800 is a vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested for ap..
Electrical Resistivity 1.00e+12 - 3.00e+14 ohm-cm
1.00e+12 - 3.00e+14 ohm-cm
Average value: 1.27e+14 ohm-cm Grade Count:15
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Electrical Resistivity 1.00e+12 - 1.50e+16 ohm-cm
1.00e+12 - 1.50e+16 ohm-cm
Average value: 6.25e+15 ohm-cm Grade Count:4
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E..
Electrical Resistivity 1.00e+12 - 1.00e+16 ohm-cm
1.00e+12 - 1.00e+16 ohm-cm
Average value: 2.63e+15 ohm-cm Grade Count:14
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Plenco 202 Black General Purpose Woodflour Filled Phenolic Molding Compound  (discontinued **)
Plaslok 202 is a two-stage, woodflour-filled phenolic molding compound formulated to provide improved impact and fatigue strength, good dimensional stability and excellent molded finish for automoti..
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Plaslok 202 Black General Purpose Woodflour Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 202 is a two-stage, woodflour-filled ..
Electrical Resistivity 1.00e+12 - 1.00e+14 ohm-cm
1.00e+12 - 1.00e+14 ohm-cm
Average value: 5.27e+13 ohm-cm Grade Count:4
Overview of materials for Nylon 12, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Plaslok 506 Black Heat Resistant Mineral Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 506 is a two-stage, mineral-filled ph..
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Sumitomo Bakelite Durez® 156 Phenolic, Compression Grade
Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL..
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
Sapco Silicon Nitride, Si3N4
Information provided by Sapco.
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade
Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft..
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
Goodfellow Potassium Aluminosilicate (Muscovite Mica)
Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin..
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
Arkema Group Rilsan® AZM 50 NOIR T6LD Nylon 12, 50% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-090,GF50Rigid grade with glass fiber (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid..
Electrical Resistivity 1.00e+12 - 1.00e+15 ohm-cm
1.00e+12 - 1.00e+15 ohm-cm
Average value: 3.52e+14 ohm-cm Grade Count:19
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..
Electrical Resistivity 1.00e+12 - 1.00e+16 ohm-cm
1.00e+12 - 1.00e+16 ohm-cm
Average value: 6.38e+15 ohm-cm Grade Count:8
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Copyright © lookpolymers.com All Rights Reserved