| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | <= 1.00e+12 ohm-cm | <= 1.00e+12 ohm-cm | IEC 60093 |
|
Murtfeldt Original Material ”S”® plus + FP Polyethylene
Original Material ”S”® plus+ FP [FS] is a technical plastic that completely meets the requirements of the food sector for the detectability of plastic foreign bodies in foods. “FP” stands for “..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
|
Plenco 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **)
Plaslok 201 is a two-stage, woodflour and mineral-filled phenolic molding compound formulated to have an excellent balance of molded properties. The material provides good electrical insulation val..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
|
Plenco 202 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **)
Plaslok 202 is a two-stage, woodflour-filled phenolic molding compound formulated to provide improved impact and fatigue strength, good dimensional stability and excellent molded finish for automoti..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
|
Plenco 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **)
Plaslok 5000 is the replacement material for the former Union Carbide BMM-5000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding performance and preheating cha..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
|
Plenco 5303 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **)
Plaslok 5303 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in appliance, automotive and electrical applications. It can be molded by compression, transfer or i..
|
|||
| Electrical Resistivity | 1.00e+12 - 1.00e+14 ohm-cm | 1.00e+12 - 1.00e+14 ohm-cm | Average value: 5.05e+13 ohm-cm Grade Count:6 |
|
Overview of materials for Nylon 63, 35% Glass-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
|
Plaslok 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 201 is a two-stage, woodflour and min..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
|
Plaslok 202 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 202 is a two-stage, woodflour-filled ..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | |
|
GBC Grade 92 Alumina
Data provided by the manufacturer, GBC Materials Corporation.
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
|
Sumitomo Bakelite Durez® 22257 Phenolic, Compression Grade
Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. ..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
|
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade
Durez 29502 B brown phenolic is a two stage, glass and mineral filled, special purpose molding material with improved mechanical and heat resistant properties. It is formulated for close tolerance ..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | |
|
Sapco Silicon Nitride, Si3N4
Information provided by Sapco.
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
|
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade
Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
|
Sumitomo Bakelite Durez® 25378 Phenolic, Injection Grade
Durez 25378 Black Phenolic is a two stage heat resistant/electrical grade molding material having an excellent molded finish, low shrinkage and good heat resistance. Durez 25378 has exceptional UL ..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
|
Sumitomo Bakelite Sumikon® PM-9640 Glass Filled Phenolic
Two stage glass fiber filled black phenolic. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance. PM-9640 is widely used in ..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | |
|
Goodfellow Potassium Aluminosilicate (Muscovite Mica)
Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | |
|
Arkema Group Rilsan® AMN P20 TLD Nylon 12, Flexible, Injection Grade (Conditioned)
Designation ISO 1874-PA12-P,MHLR,14-005Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and ..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
|
Chang Chun Plastic Longlite PM T359J General Purpose Phenolic Molding Compound
ASTM Grades per ASTM D700 are 3, 14.Information provided by Dowell Trading Company Ltd.
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | |
|
Arkema Group Rilsan® AZM 50 NOIR T6LD Nylon 12, 50% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-090,GF50Rigid grade with glass fiber (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid..
|
|||
| Electrical Resistivity | >= 1.00e+12 ohm-cm | >= 1.00e+12 ohm-cm | DIN 53482/VDE 0303 |
|
BASF Elastollan® 1174D Polyether Type Polyurethane Elastomer
Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exh..
|
|||
| Electrical Resistivity | 1.00e+12 - 1.00e+15 ohm-cm | 1.00e+12 - 1.00e+15 ohm-cm | Average value: 3.52e+14 ohm-cm Grade Count:19 |
|
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..
|
|||
| Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
|
Plaslok 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 5000 is the replacement material for ..
|
|||
| Electrical Resistivity | 1.00e+12 - 1.00e+16 ohm-cm | 1.00e+12 - 1.00e+16 ohm-cm | Average value: 3.34e+15 ohm-cm Grade Count:3 |
|
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..
|
|||