| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | IEC 60093 |
|
Murtfeldt Muralen® plus + AB Polyethylene, Antibacterial
Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of..
|
|||
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | IEC 60093 |
|
Murtfeldt Murinit® SP Polyphenylene Sulfide
Thanks to the low fiber content and integrated solid lubricant, Murinit® SP offers an excellent combination of good slide and wear behavior, high strength, and dimensional stability – even at high..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
|
Murtfeldt Murinyl® Polyvinylidinefluoride
As a fluorinated plastic, Murinyl® is exceptionally resistant to chemicals, hydrolysis, and sterilization. Its properties change very little at high service temperatures and after long-term exposur..
|
|||
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | dry; IEC 60093 |
|
Murtfeldt Murylon® 6 Cast Nylon 6
Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia..
|
|||
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | dry; IEC 60093 |
|
Murtfeldt Murylon® A GF Nylon 66, Glass Reinforced
Murylon® A’s impressive characteristics are enhanced with admixed glass fibers. This results in a clear improvement in cold flow behavior and dimensional stability, enabling higher static pressure..
|
|||
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | dry; IEC 60093 |
|
Murtfeldt Murylat® Polyethylene Terephthalate
Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 1.46e+15 ohm-cm Grade Count:33 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
|
|||
| Electrical Resistivity | 1.00e+14 - 5.90e+16 ohm-cm | 1.00e+14 - 5.90e+16 ohm-cm | Average value: 2.23e+16 ohm-cm Grade Count:13 |
|
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
|
3M Dyneon™ TF 2071 PTFE Paste Extrusion Powder
(discontinued **)
Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1600. Average particle size 500 µm. Used for tubing, wire/cable insulation, 'spaghetti tubing' production.Dyneon offers a..
|
|||
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | |
|
MarkeTech AN 160 Aluminum Nitride Ceramic Substrate, 99% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ..
|
|||
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | ASTM D1829 |
|
CoorsTek AD-85 Alumina (nom. 85% Al2O3)
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
|
|||
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | ASTM D1829 |
|
CoorsTek AD-94 Alumina (nom. 94% Al2O3)
Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
|
Arkema Group Rilsan® BECN W3 TL Nylon 11, Sheathing Grade (Conditioned)
Designation ISO 1874-PA11,KFHL,12-010Rigid grade for sheathing wires and cables. Available color: natural. Light and heat stabilized. Flame retardant agent.Fire-resistant. High abrasion resistance. ..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
|
BASF Novolen® 3248 TC Polypropylene
Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF.
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
|
Ashley Polymers Ashlene® 527LD Nylon 66
A very high impact, slightly lubricated nylon resin.Data provided by the manufacturer
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
|
Ashley Polymers Ashlene® 527LDS-B2 Nylon 66
A high impact lubricated nylon resin containing well dispersed carbon black for maximum resistance to weathering.Data provided by the manufacturer
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
|
Ashley Polymers Ashlene® 980LS Nylon 612
A general purpose 612 nylon for injection molding, lubricated and heat stabilized. These resins are noted for their low moisture absorption and excellent dimensional stability.Data provided by the ..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
|
CENTROPLAST CENTROMID 6 G Polyamide 6 Cast
This material has good machinability and can be bonded or welded. Its applications include sliding bearings, hammerheads, and toothed gears.Information provided by CENTROPLAST Engineering Plastics ..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | Volume; GB1410 |
|
Beijing Evergrow Resources Oilon
Information provided by Beijing Evergrow Resources.
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
|
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Conditioned)
Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. Mold-release agent...
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
|
CENTROPLAST CENTROLEN PP-H Polypropylene homopolymer
This plastic is a low density, easily machined material that can be welded and has good chemical resistance. Applications include filter housings, chemical pump components and apparatus engineering..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
|
CENTROPLAST CENTROMID 6 E FG Polyamide 6 extruded, Food Grade
This tough and impact resistant material has good chemical resistance and can be bonded and welded. Information provided by CENTROPLAST Engineering Plastics GMBH
|
|||
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | Intensity = 10 mA after 2 min @ 23°C; ASTM D 257; DIN 53483 |
|
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **)
Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ISO data |
|
BASF Capron® GR630 HS 30% Glass-Filled Nylon 66 (Dry)
(discontinued **)
Capron GR630 HS is a heat stabilized, 30% glass fiber reinforced polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This ba..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 4.73e+15 ohm-cm Grade Count:7 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
|
CENTROPLAST CENTROLEN PP GF 30 Polypropylene 30% glass fiber
This material is a low density, easily machined plastic that has high impact resistance and dimensional stability. Applications include air filter housings, fan blades, and fittings with high loads...
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 9.65e+14 ohm-cm Grade Count:13 |
|
Overview of materials for Polyphthalamide (PPA), Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a..
|
|||