| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | 50% RH; IEC 60093 |
|
Murtfeldt Murytal® C Acetal Copolymer
Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+17 ohm-cm | 1.00e+14 - 1.00e+17 ohm-cm | Average value: 5.03e+16 ohm-cm Grade Count:16 |
|
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor..
|
|||
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | Intensity = 10 mA after 2 min @ 23°C; ASTM D 257; DIN 53483 |
|
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound
(discontinued **)
Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
|
3M Dyneon™ TF 2072 PTFE Paste Extrusion Powder
(discontinued **)
Type I PTFE. Free flowing powder. Minimum reduction ratio is 50; Max is 3000. Average particle size 500 µm. Used for wire/cable insulation, 'spaghetti tubing' production.Dyneon offers a family ..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | Average value: 2.06e+14 ohm-cm Grade Count:17 |
|
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v..
|
|||
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | ASTM D1829 |
|
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
|
|||
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | ASTM D1829 |
|
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
|
Arkema Group Rilsan® AMN G8 TLD Nylon 12, Graphite Filled (Conditioned)
Designation ISO 1874-PA12,MHLS,14-010,CD05Rigid grade with graphite filler for injection molding. Available colors: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
|
Arkema Group Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Conditioned)
Designation ISO 1874-PA12,MHLR,16-010Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.High impact strength. Easy filling of the mold due to ..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
|
Arkema Group Rilsan® BMN D Nylon 11 (Conditioned)
Designation ISO 1874-PA11,MR,12-010Rigid grade for injection molding. Available colors: black, blue, natural, orange, white. Mold release agent.High mechanical properties. Easy filling of the mold d..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
|
CENTROPLAST BC NF Organic Thermoplastic, 15% Natural Fiber
CENTROPLAST BC NF 15 is made of CO2-neutral, sustainable raw-materials with 15% natural fiber.CENTROPLAST has the characteristics of thermoplastics while being 100% recyclable and completely biodegr..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
|
CENTROPLAST CENTRO HPM Polysulfone
This plastic has good hydrolysis, chemical and radiation resistance, and can operate at high temperatures. It is used in food processing industry, pumps and valves, and medical equipment.Informatio..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
|
CENTROPLAST CENTROPEEK Polyetheretherketone
This plastic has high temperature resistance, good chemical resistance, and good mechanical characteristics. Its has good sliding friction properties and is suitable for use with foodstuffs or medi..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
|
Ceradyne Ceralloy® 1370-1E Aluminum Nitride
Features:standard grade Applications:semiconductor componentsInformation provided by Ceradyne Company
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
|
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Conditioned)
Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. Mold-release agent...
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | Volume; GB1410 |
|
Beijing Evergrow Resources Enylon®
Information provided by Beijing Evergrow Resources.
|
|||
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | Intensity = 10 mA after 2 min @ 23°C; ASTM D 257; DIN 53483 |
|
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **)
Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO..
|
|||
| Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | Intensity = 10 mA after 2 min @ 23°C; ASTM D 257; DIN 53483 |
|
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **)
Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 1.52e+15 ohm-cm Grade Count:64 |
|
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 5.88e+15 ohm-cm Grade Count:19 |
|
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 8.35e+15 ohm-cm Grade Count:6 |
|
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | Average value: 7.60e+14 ohm-cm Grade Count:15 |
|
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
|
|||
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
|
Ceradyne Ceralloy® 147-1E Silicon Nitride
Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradynes ..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 2.58e+15 ohm-cm Grade Count:4 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu..
|
|||