| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00e+15 - 1.00e+16 ohm-cm | 1.00e+15 - 1.00e+16 ohm-cm | |
|
3M Dyneon™ Aflas® FA-150L PTFE Fluoroelastomer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium..
|
|||
| Electrical Resistivity | 0.0100 - 1.00e+16 ohm-cm | 0.0100 - 1.00e+16 ohm-cm | Average value: 2.76e+15 ohm-cm Grade Count:79 |
|
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..
|
|||
| Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 1.81e+15 ohm-cm Grade Count:19 |
|
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
|
|||
| Electrical Resistivity | 10000 - 1.00e+16 ohm-cm | 10000 - 1.00e+16 ohm-cm | Average value: 4.21e+15 ohm-cm Grade Count:6 |
|
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and ..
|
|||
| Electrical Resistivity | 10000 - 1.00e+16 ohm-cm | 10000 - 1.00e+16 ohm-cm | Average value: 1.10e+15 ohm-cm Grade Count:33 |
|
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
|
|||
| Electrical Resistivity | 1.00e+9 - 1.00e+16 ohm-cm | 1.00e+9 - 1.00e+16 ohm-cm | Average value: 2.60e+15 ohm-cm Grade Count:5 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu..
|
|||
| Electrical Resistivity | 1.00e+15 - 1.00e+16 ohm-cm | 1.00e+15 - 1.00e+16 ohm-cm | Average value: 7.75e+15 ohm-cm Grade Count:4 |
|
Overview of materials for ABS/Polyester Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 6.91e+15 ohm-cm Grade Count:8 |
|
Overview of materials for Polycarbonate, Aramid Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v..
|
|||
| Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 1.95e+15 ohm-cm Grade Count:11 |
|
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
|
|||
| Electrical Resistivity | 1.00e+12 - 1.00e+16 ohm-cm | 1.00e+12 - 1.00e+16 ohm-cm | Average value: 2.33e+15 ohm-cm Grade Count:6 |
|
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
|
|||
| Electrical Resistivity | 400 - 1.00e+16 ohm-cm | 400 - 1.00e+16 ohm-cm | Average value: 1.31e+15 ohm-cm Grade Count:29 |
|
Overview of materials for Epoxy, High Temperature
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val..
|
|||
| Electrical Resistivity | 1.00e+15 - 1.00e+16 ohm-cm | 1.00e+15 - 1.00e+16 ohm-cm | Average value: 2.90e+15 ohm-cm Grade Count:10 |
|
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
|
|||
| Electrical Resistivity | 0.0500 - 1.00e+16 ohm-cm | 0.0500 - 1.00e+16 ohm-cm | Average value: 8.93e+14 ohm-cm Grade Count:7 |
|
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
|
|||
| Electrical Resistivity | 1.00e+9 - 1.00e+16 ohm-cm | 1.00e+9 - 1.00e+16 ohm-cm | Average value: 8.66e+14 ohm-cm Grade Count:24 |
|
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
|
|||
| Electrical Resistivity | 1.00e+9 - 1.00e+16 ohm-cm | 1.00e+9 - 1.00e+16 ohm-cm | Average value: 4.47e+14 ohm-cm Grade Count:24 |
|
Overview of materials for Nylon 66, 60% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. ..
|
|||
| Electrical Resistivity | 10.0 - 1.00e+16 ohm-cm | 10.0 - 1.00e+16 ohm-cm | Average value: 2.73e+14 ohm-cm Grade Count:75 |
|
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
|
|||
| Electrical Resistivity | 1.00 - 1.00e+16 ohm-cm | 1.00 - 1.00e+16 ohm-cm | Average value: 2.46e+14 ohm-cm Grade Count:270 |
|
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
|
|||
| Electrical Resistivity |
1.00e+11
-
1.00e+16
ohm-cm <br>@Temperature 20.0 - 500 °C
|
1.00e+11
-
1.00e+16
ohm-cm <br>@Temperature 68.0 - 932 °F
|
|
|
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal
Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | |
|
Kraton® D1102 (SBS) Linear Block Copolymer
(SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact ..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | |
|
Kraton® D4141 (SBS) Linear Block Copolymer
(SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact ..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | |
|
Kraton® D1101 (SBS) Linear Block Copolymer
(SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact ..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | |
|
Kraton® D1112P (SIS) Linear Block Copolymer
(SIS) styrene-isoprene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact q..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 2.51e+15 ohm-cm Grade Count:20 |
|
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 1.56e+15 ohm-cm Grade Count:17 |
|
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 5.88e+15 ohm-cm Grade Count:19 |
|
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
|
|||
| Electrical Resistivity | 1.00e+12 - 1.00e+16 ohm-cm | 1.00e+12 - 1.00e+16 ohm-cm | Average value: 6.38e+15 ohm-cm Grade Count:8 |
|
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 7.08e+15 ohm-cm Grade Count:16 |
|
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
|
|||
| Electrical Resistivity | 3.00e+13 - 1.00e+16 ohm-cm | 3.00e+13 - 1.00e+16 ohm-cm | Average value: 3.00e+15 ohm-cm Grade Count:12 |
|
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..
|
|||
| Electrical Resistivity |
1.00e+15
-
1.00e+16
ohm-cm <br>@Temperature 200 - 200 °C
|
1.00e+15
-
1.00e+16
ohm-cm <br>@Temperature 392 - 392 °F
|
Average value: 4.00e+15 ohm-cm Grade Count:3 |
|
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..
|
|||
| Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 2.58e+15 ohm-cm Grade Count:4 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu..
|
|||