| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 2.50e+13 ohm-cm | 2.50e+13 ohm-cm | Initial Insulation Resistance (50% Relative Humidity) |
|
Cytec Conathane® CC-1155 (Conap) Polyurethane Two-component Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
|
|||
| Electrical Resistivity | 2.50e+13 ohm-cm | 2.50e+13 ohm-cm | Initial Insulation Resistance (50% Relative Humidity) |
|
Cytec Conathane® CC-1155-35 (Conap) Polyurethane Two-component Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
|
|||
| Electrical Resistivity | 2.50e+13 ohm-cm | 2.50e+13 ohm-cm | Initial Insulation Resistance (50% Relative Humidity) |
|
Cytec Conathane® CC-1194 (Conap) Polyurethane Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
|
|||
| Electrical Resistivity | 2.50e+13 ohm-cm | 2.50e+13 ohm-cm | Initial Insulation Resistance (50% Relative Humidity) |
|
Cytec Conathane® CC-1195 (Conap) Polyurethane Two-component Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
|
|||
| Electrical Resistivity | 2.50e+13 ohm-cm | 2.50e+13 ohm-cm | Initial Insulation Resistance (50% Relative Humidity) |
|
Cytec Conathane® CE-1164 (Conap) Polyurethane Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
|
|||
| Electrical Resistivity | 2.50e+13 ohm-cm | 2.50e+13 ohm-cm | Initial Insulation Resistance (50% Relative Humidity) |
|
Cytec Conathane® CE-1163 (Conap) Polyurethane Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
|
|||