| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+9 - 1.00e+10 ohm | 1.00e+9 - 1.00e+10 ohm | ISO IEC 61340-5-1 |
|
Premix Thermoplastics PRE-ELEC® ESD 5300 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5300 is a static dissipative thermoplastic compound based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance valu..
|
|||
| Surface Resistance | 1.00e+9 - 1.00e+10 ohm | 1.00e+9 - 1.00e+10 ohm | At 20-25% Dosing; ISO IEC 61340-5-1 |
|
Premix Thermoplastics PRE-ELEC® ESD 6010 Dissipative Masterbatch, IDP Additive
PRE-ELEC® ESD 6010 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro..
|
|||
| Surface Resistance | 1.00e+9 - 1.00e+10 ohm | 1.00e+9 - 1.00e+10 ohm | At 20-25% Dosing; ISO IEC 61340-5-1 |
|
Premix Thermoplastics PRE-ELEC® ESD 6020 Dissipative Masterbatch, IDP Additive
PRE-ELEC® ESD 6020 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro..
|
|||
| Surface Resistance | 10.0 - 1.00e+10 ohm | 10.0 - 1.00e+10 ohm | Average value: 8.30e+8 ohm Grade Count:24 |
|
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
|
|||
| Surface Resistance | 1.00 - 1.00e+10 ohm | 1.00 - 1.00e+10 ohm | Average value: 4.17e+8 ohm Grade Count:28 |
|
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
|
|||
| Surface Resistance | 100 - 1.00e+10 ohm | 100 - 1.00e+10 ohm | Average value: 1.68e+7 ohm Grade Count:13 |
|
Overview of materials for Nylon 612, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+10 ohm | 1.00e+6 - 1.00e+10 ohm | ASTM D 257 |
|
SABIC Innovative Plastics LNP Stat-kon DX07323 PC+ABS
LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, ..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+10 ohm | 1.00e+6 - 1.00e+10 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Asia Pacific)
LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, ..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+10 ohm | 1.00e+6 - 1.00e+10 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Europe-Africa-Middle East)
LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, ..
|
|||
| Surface Resistance | 1.00e+8 - 1.00e+10 ohm | 1.00e+8 - 1.00e+10 ohm | ASTM D 257 |
|
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS (Asia Pacific)
LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t..
|
|||
| Surface Resistance | 1.00e+8 - 1.00e+10 ohm | 1.00e+8 - 1.00e+10 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-LOY KX09024 ACETAL COPOLYMER (Europe-Africa-Middle East)
LNP* Statloy* KX09024 is a compound based on Polyacetal with reduced Resistivity. Added features include: Antistatic Properties
|
|||
| Surface Resistance | 1.00e+9 - 1.00e+10 ohm | 1.00e+9 - 1.00e+10 ohm | ASTM D257 |
|
Supreme Petrochem SP 6520 Permanent Antistatic Polystyrene
Characteristics No sloughing Fully colorable Meets MIL-PRF-81705D static decay specification Functions even in low humidity levels Processing Injection molding Extrusion & Forming Applications C..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+10 ohm | 1.00e+6 - 1.00e+10 ohm | |
|
Pyrotek Pyromat TS-045 Electrical Insulating Board
Pyromat TS-045 is a black laminate, press molded from high-temperature thermoset resin and reinforced with glass filament mat. Its composition ensures excellent chemically resistance and antistatic..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+10 ohm | 1.00e+6 - 1.00e+10 ohm | ASTM D257 |
|
PolyOne Stat-Tech™ RA-06CF-07GF/000 EM Polyarylsulfone - 7% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications - Flow Enhanced Grade
Data provided by PolyOne.
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+10 ohm | 1.00e+6 - 1.00e+10 ohm | ASTM D257 |
|
PolyOne Stat-Tech™ RA-06CF-09GF/000 Polyarylsulfone - 9% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications
&a
Data provided by PolyOne.
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+10 ohm | 1.00e+6 - 1.00e+10 ohm | ASTM D257 |
|
PolyOne Stat-Tech™ RA-06CF-09GF/000 EM Polyarylsulfone - ESD Applications - Flow Enhanced Grade
(discontinued
Data provided by PolyOne.
|
|||
| Surface Resistance | 100 - 1.00e+10 ohm | 100 - 1.00e+10 ohm | Average value: 5.56e+8 ohm Grade Count:13 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu..
|
|||