| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | ASTM D257 |
|
PolyOne Stat-Tech™ AS-1000 AS Acrylonitrile Butadiene Styrene (ABS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
|
PolyOne Stat-Tech™ PI-05CF/000R Black Polyether Imide (PEI)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
|
|||
| Surface Resistance | 1.00e+9 - 1.00e+12 ohm | 1.00e+9 - 1.00e+12 ohm | At 8-20% Dosing; ISO IEC 61340-5-1 |
|
Premix Thermoplastics PRE-ELEC® ESD 4000 Polyolefin Compatible Dissipative Masterbatch, IDP Additive
PRE-ELEC® ESD 4000 is a polyolefin compatible dissipative masterbatch developed for PELD and PE-HD film, sheet, blow and injection moulded products. The active substance is an IDP (inherently dissi..
|
|||
| Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | ISO IEC 61340-5-1 |
|
Premix Thermoplastics PRE-ELEC® ESD 5360 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5360 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val..
|
|||
| Surface Resistance | 5.00e+8 - 1.00e+12 ohm | 5.00e+8 - 1.00e+12 ohm | Average value: 2.78e+11 ohm Grade Count:4 |
|
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
|
|||
| Surface Resistance | 1.00 - 1.00e+12 ohm | 1.00 - 1.00e+12 ohm | Average value: 1.44e+10 ohm Grade Count:92 |
|
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
|
Techmer ES Electrablend® ABS CF5 5% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 5% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66
LNP* STAT-LOY* 9X03508 is a compound based on PPO+PA66 resin containing Proprietary Filler(s). Added features of this material include: Antistatic, Flame Retardant, High Impact.
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-LOY 9X07438 ASA+PC
LNP* STAT-LOY* 9X07438 is a compound based on Polycarbonate/ASA containing Proprietary Filler(s). Added features of this grade include: Antistatic, Colorable, Weatherable.
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D 257 |
|
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS
LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t..
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS
LNP* STAT-LOY* AF3009 is a compound based on ABS resin containing 10% Glass Fiber. Added features of this material include: Antistatic, Flame Retardant.
|
|||
| Surface Resistance | 1.00e+9 - 1.00e+12 ohm | 1.00e+9 - 1.00e+12 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-LOY AF3029U ABS (Europe-Africa-Middle East)
LNP* STAT-LOY* AF3029U is a compound based on Acrylonitrile Butadiene resin containing Glass Fiber, Flame Retardant, Propietary filler. Added features include: Antistatic, UV-Stabilized.
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-LOY KX05015 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Stat-Loy* KX05015 is a compound based on Acetal Copolymer resin containing Antistat. Added features include permanent Anti-Static.
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS
LNP* STAT-LOY* N30009 is a compound based on PC+ABS Blend resin. Added features of this material include: Antistat, Flame Retardant.
|
|||
| Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
|
Techmer ES Statiblend® 02036 Polypropylene
Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveInformation provided by TP Composites, Inc.
|
|||
| Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
|
Techmer ES Statiblend® 02056 BKN Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9109116Information provided by TP Composites, Inc.
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
|
Techmer ES Statiblend® PA6 GF20 AS BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Antistatic, Heat Stabilizer and LubricantFeatures: Antistatic, Heat Stabilizer and Lubricate..
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
|
Techmer ES Statiblend® PA6/6 GF20 AS BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Lubricant, Antistatic and Heat StabilizerFeatures: Antistatic, Heat Stabilized and Lubricate..
|
|||
| Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
|
SABIC Innovative Plastics NORYL NC208 PPE+HIPS (Asia Pacific) |
|||
| Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-LOY KX01002 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Stat-Loy* KX01002 is a compound based on Acetal Copolymer resin containing Antistat. Added features include: Permanent Anti-Static.
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-LOY NX03583 PC+ABS
LNP STAT-LOY* NX03583 is a compound based on PC+ABS Blend resin. Added features of this material include: Antistat, Flame Retardant.
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-LOY P3000U PA 6 (Europe-Africa-Middle East)
LNP* Stat-loy* P3000U is a compound based on PA 6 resin. Added features include; Antistatic, UV - Stabilized.
|
|||
| Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | IS 3396-1979 |
|
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded
Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit..
|
|||
| Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | IS 3396-1979 |
|
Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railwa..
|
|||
| Surface Resistance | 4000 - 1.00e+12 ohm | 4000 - 1.00e+12 ohm | Average value: 1.17e+11 ohm Grade Count:9 |
|
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
|
|||
| Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D 257 |
|
SABIC Innovative Plastics Valox® VC108 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | ASTM D257 |
|
Supreme Petrochem SP 6630 Antistatic Polystyrene
Characteristics Easy flow Excellent transparency Processing Extrusion Applications For glossy cap layer on HIPS To prevent dust patterns on thermoformed products Material Status: Commercial : Acti..
|
|||
| Surface Resistance | 10.0 - 1.00e+12 ohm | 10.0 - 1.00e+12 ohm | Average value: 3.89e+10 ohm Grade Count:26 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..
|
|||