| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+15 - 1.00e+16 ohm | 1.00e+15 - 1.00e+16 ohm | ASTM D257 |
|
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific)
Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame..
|
|||
| Surface Resistance | 10000 - 1.00e+16 ohm | 10000 - 1.00e+16 ohm | Average value: 5.36e+14 ohm Grade Count:41 |
|
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
|
|||
| Surface Resistance | 10.0 - 1.00e+16 ohm | 10.0 - 1.00e+16 ohm | Average value: 3.03e+15 ohm Grade Count:184 |
|
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
|
|||
| Surface Resistance | 1000 - 1.00e+16 ohm | 1000 - 1.00e+16 ohm | Average value: 2.33e+15 ohm Grade Count:13 |
|
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
|
|||
| Surface Resistance | 1.00e+14 - 1.00e+16 ohm | 1.00e+14 - 1.00e+16 ohm | Average value: 1.00e+15 ohm Grade Count:19 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
|
|||
| Surface Resistance | 1.00e+14 - 1.00e+16 ohm | 1.00e+14 - 1.00e+16 ohm | Average value: 6.70e+15 ohm Grade Count:3 |
|
Overview of materials for ABS/Polyester Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat..
|
|||
| Surface Resistance | 1.00e+15 - 1.00e+16 ohm | 1.00e+15 - 1.00e+16 ohm | ASTM D 257 |
|
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific)
Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di..
|
|||
| Surface Resistance | 10000 - 1.00e+16 ohm | 10000 - 1.00e+16 ohm | Average value: 3.92e+15 ohm Grade Count:26 |
|
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
|
|||
| Surface Resistance | 1.00e+15 - 1.00e+16 ohm | 1.00e+15 - 1.00e+16 ohm | Average value: 4.67e+15 ohm Grade Count:27 |
|
Overview of materials for Polycarbonate, High Heat
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro..
|
|||
| Surface Resistance | 1.00e+9 - 1.00e+16 ohm | 1.00e+9 - 1.00e+16 ohm | Average value: 2.84e+15 ohm Grade Count:19 |
|
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
|
|||
| Surface Resistance | 2000 - 1.00e+16 ohm | 2000 - 1.00e+16 ohm | Average value: 8.84e+14 ohm Grade Count:35 |
|
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
|
|||
| Surface Resistance | 1.00e+12 - 1.00e+16 ohm | 1.00e+12 - 1.00e+16 ohm | Average value: 1.66e+15 ohm Grade Count:10 |
|
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
|
|||
| Surface Resistance | 1.00e+15 - 1.00e+16 ohm | 1.00e+15 - 1.00e+16 ohm | Average value: 4.56e+15 ohm Grade Count:5 |
|
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
|
|||
| Surface Resistance | 3000 - 1.00e+16 ohm | 3000 - 1.00e+16 ohm | Average value: 4.88e+15 ohm Grade Count:24 |
|
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 7.47e+14 ohm Grade Count:31 |
|
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 1.45e+15 ohm Grade Count:23 |
|
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 3.60e+14 ohm Grade Count:36 |
|
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
|
|||
| Surface Resistance | 1.00 - 1.00e+16 ohm | 1.00 - 1.00e+16 ohm | Average value: 8.14e+14 ohm Grade Count:69 |
|
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
|
|||
| Surface Resistance | 1.00 - 1.00e+16 ohm | 1.00 - 1.00e+16 ohm | Average value: 9.40e+14 ohm Grade Count:113 |
|
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
|
|||
| Surface Resistance | 1.00e+13 - 1.00e+16 ohm | 1.00e+13 - 1.00e+16 ohm | ASTM D257 |
|
Supreme Petrochem SP 6530 Antistatic Polystyrene
Characteristics Prevents dust patterns due to static charges Eliminates need of coatings Fully colorable Processing Injection molding Extrusion & Forming Applications Meter housings Foodservice ..
|
|||
| Surface Resistance | 1.00e+14 - 1.00e+16 ohm | 1.00e+14 - 1.00e+16 ohm | ASTM D257 |
|
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing
Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po..
|
|||
| Surface Resistance | 1.00e+14 - 1.00e+16 ohm | 1.00e+14 - 1.00e+16 ohm | ASTM D257 |
|
Daelim H&L Plavis-N DF Unfilled Aromatic Polyimide Bearing
Direct Formed. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS polyimi..
|
|||
| Surface Resistance |
1.00e+15
-
1.00e+16
ohm <br>@Temperature 23.0 °C
|
1.00e+15
-
1.00e+16
ohm <br>@Temperature 73.4 °F
|
ASTM D257 |
|
DuPont Performance Polymers VESPEL TP-8054 Polyimide
DuPont Vespel TP-8054 parts are specified for high-temperature applications requiring a balance of mechanical and thermal properties. TP-8054 parts are produced from unreinforced thermoplastic polyi..
|
|||
| Surface Resistance |
1.00e+15
-
1.00e+16
ohm <br>@Temperature 23.0 °C
|
1.00e+15
-
1.00e+16
ohm <br>@Temperature 73.4 °F
|
ASTM D257 |
|
DuPont Performance Polymers VESPEL TP-8161 Polyimide
DuPont Vespel TP-8161 parts are specified for high-temperature applications. TP-8161 parts offer a unique balance of mechanical and thermal properties for superior performance in aggressive environm..
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 5.72e+14 ohm Grade Count:40 |
|
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
|
|||
| Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 8.03e+14 ohm Grade Count:15 |
|
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
|
|||
| Surface Resistance | 1.00e+14 - 1.00e+16 ohm | 1.00e+14 - 1.00e+16 ohm | Average value: 5.05e+15 ohm Grade Count:4 |
|
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
|
|||
| Surface Resistance | 100 - 1.00e+16 ohm | 100 - 1.00e+16 ohm | Average value: 2.52e+15 ohm Grade Count:4 |
|
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
|
|||
| Surface Resistance | 1000 - 1.00e+16 ohm | 1000 - 1.00e+16 ohm | Average value: 2.31e+15 ohm Grade Count:45 |
|
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
|
|||
| Surface Resistance | 260 - 1.00e+16 ohm | 260 - 1.00e+16 ohm | Average value: 2.08e+15 ohm Grade Count:30 |
|
Overview of materials for Acetal Copolymer, Impact Modified